# US 2004/0082129 A1 · Method of fabricating a semiconductor device including a tunnel oxide film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082129 A1
- Document ID: US20040082129A1
- Status: Published application
- Kind: A1
- Application number: 10/606,792
- Filed: 2003-06-27
- Published: 2004-04-29
- Earliest claimed: 2002-10-25
- Assignees: Oki Electric Industry Co., Ltd.
- Inventors: Toshio Nagata
- Web page: https://patentgrep.com/patent/US20040082129A1

## CPC

- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10D 30/6891: {characterised by the shapes, relative sizes or dispositions of the floating gate electrode}
- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6506: {Formation of intermediate materials}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of fabricating a semiconductor device includes the steps of forming a first film of silicon nitride or silicon oxynitride on a polysilicon layer, forming a second film of silicon oxide on the first film by chemical vapor deposition, and oxygen-annealing the second film to form a tunnel oxide film. The presence of the silicon nitride or silicon oxynitride film enables an annealing process with a high oxidation capability to be used without oxidizing the polysilicon layer. The leakage of unwanted current through the tunnel oxide film can thereby be reduced, improving the data retention characteristics of devices such as flash memories.

## Claims

### Claim 1

A method of fabricating a semiconductor device including a tunnel oxide film formed on a polysilicon layer, comprising:
forming a first film of silicon nitride or silicon oxynitride on the polysilicon layer;
forming a second film of silicon oxide on the first film by chemical vapor deposition; and
oxygen-annealing the second film to form the tunnel oxide film.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first film is a film of silicon nitride, and oxygen-annealing the second film comprises wet oxygen annealing for five to ten minutes.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first film is a film of silicon nitride, and oxygen-annealing the second film comprises wet oxygen annealing at 850° C. to 900° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first film is a film of silicon oxynitride.

### Claim 5 (depends on 4)

The method of claim 4, wherein the first film and the second film are formed by a continuous process.

### Claim 6 (depends on 4)

The method of claim 4, wherein oxygen-annealing the second film comprises dry oxygen annealing for 30 to 60 minutes.

### Claim 7 (depends on 4)

The method of claim 4, wherein oxygen-annealing the second film comprises dry oxygen annealing at 850° C. to 900° C.

### Claim 8 (depends on 4)

The method of claim 4, wherein oxygen-annealing the second film comprises wet oxygen annealing for 5 to 60 minutes.

### Claim 9 (depends on 4)

The method of claim 4, wherein oxygen-annealing the second film comprises wet oxygen annealing at 850° C. to 900° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein:
the polysilicon layer is formed on a silicon substrate and constitutes a first floating gate;
the semiconductor device also includes a second floating gate formed on the silicon substrate, overlapping at least an edge of the first floating gate; and
the first film, the second film, and the tunnel oxide film separate the first floating gate from the second floating gate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the first film is a film of silicon nitride, and oxygen-annealing the second film comprises wet oxygen annealing for five to ten minutes.

### Claim 12 (depends on 10)

The method of claim 10, wherein the first film is a film of silicon nitride, and oxygen-annealing the second film comprises wet oxygen annealing at 850° C. to 900° C.

### Claim 13 (depends on 10)

The method of claim 10, wherein the first film is a film of silicon oxynitride.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first film and the second film are formed by a continuous process.

### Claim 15 (depends on 13)

The method of claim 13, wherein oxygen-annealing the second film comprises dry oxygen annealing for 30 to 60 minutes.

### Claim 16 (depends on 13)

The method of claim 13, wherein oxygen-annealing the second film comprises dry oxygen annealing at 850° C. to 900° C.

### Claim 17 (depends on 13)

The method of claim 13, wherein oxygen-annealing the second film comprises wet oxygen annealing for 5 to 60 minutes.

### Claim 18 (depends on 13)

The method of claim 13, wherein oxygen-annealing the second film comprises wet oxygen annealing at 850° C. to 900° C.