# US 2004/0082126 A1 · Semiconductor device incorporated therein high K capacitor dielectric and method for the manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082126 A1
- Document ID: US20040082126A1
- Status: Published application
- Kind: A1
- Application number: 10/728,855
- Filed: 2003-12-08
- Published: 2004-04-29
- Earliest claimed: 1999-12-22
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: Ki-Seon Park; Byoung-Kwan Ahn
- Web page: https://patentgrep.com/patent/US20040082126A1

## CPC

- H10D 1/68: Capacitors having no potential barriers
- H10B 12/315: {with the capacitor higher than a bit line}
- H10D 1/696: {comprising multiple layers, e.g. comprising a barrier layer and a metal layer (barrier layers to prevent diffusion of hydrogen or oxygen in perovskite based capacitors H10D1/688)}
- H10D 1/716: {having vertical extensions}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69391: {the material containing aluminium, e.g. Al2O3}
- H10P 14/69397: {the material containing two or more metal elements}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device for use in a memory cell includes an active matrix provided with a semiconductor substrate, a plurality of transistors formed on the semiconductor substrate and conductive plugs electrically connected to the transistors, a number of bottom electrodes formed on top of the conductive plugs, composite films formed on the bottom electrodes and A2O3 films formed on the composite films. In the device, the composite films are made of (Ta2O5)0.92 (TiO2)0.08 by using an atomic layer deposition (ALD).

## Claims

### Claim 1

A semiconductor device for use in a memory cell, comprising:
an active matrix having a plurality of transistors on a semiconductor substrate and a plurality of conductive plugs electrically coupled to the transistors;
a bottom electrode over each conductive plug;
a composite layer over the bottom electrode; and
an aluminum oxide layer over the composite layer.

### Claim 2 (depends on 1)

The semiconductor device of claim 1, wherein the bottom electrode includes a material selected from a group consisting of poly silicon (poly-Si), W, WN, Wsix, TiN, Pt, Ru and Ir.

### Claim 3 (depends on 1)

The semiconductor device of claim 1, wherein the composite layer includes (Ta2O5)0.92(TiO2)0.08.

### Claim 4 (depends on 1)

The semiconductor device of claim 1, further comprising a TiN layer over the aluminum oxide layer and an upper electrode layer over the TiN layer.

### Claim 5

A method for manufacturing a semiconductor device for use in a memory cell, comprising the steps of:
a) preparing an active matrix having at least one transistor, a plurality of conductive plugs electrically connected to the at least one transistor and an insulating layer laterally between adjacent conductive plugs;
b) forming a conductive layer over each conductive plug to form a bottom electrode;
d) forming a (Ta2O5)x(TiO2)y composite layer over the bottom electrodes, x and y representing a respective molar fraction;
e) forming a dielectric layer over the (Ta2O5)x(TiO2)y composite layer; and
f) patterning the dielectric layer and the (Ta2O5)x(TiO2)y composite layer into a preset configuration.

### Claim 6 (depends on 5)

The method of claim 5, wherein the bottom electrode includes a material selected from a group consisting of a poly-Si, W, WN, Wsix, TiN, Pt, Ru and Ir.

### Claim 7 (depends on 5)

The method of claim 5, the step of forming a (Ta2O5)x(TiO2)y composite layer includes the steps of:
(1) alternatively introducing first and second source gases into a reaction chamber, thereby forming a Ta2O5 thin layer;
(2) alternately introducing third and fourth source gases into the reaction chamber, thereby forming a TiO2 thin layer over the Ta2O5 thin layer;
(3) repeating the steps (1) and (2), thereby obtaining stacked Ta2O5 and TiO2 thin layers; and
(4) heating the stacked thin layers at a temperature ranging from approximately 400° C. to approximately 550° C., thereby obtaining the (Ta2O5)x(TiO2)y composite layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the first source gas includes a pentaethoxytantalum ((Ta(C2H5O)5) gas, and the second source gas includes a gas selected from a group consisting of H2O, O2, N2O and alcohol (CxHyOH) gases.

### Claim 9 (depends on 7)

The method of claim 7, wherein the reaction chamber is kept at a temperature ranging from approximately 250° C. to approximately 350° C.

### Claim 10 (depends on 7)

The method of claim 7, wherein a thickness of the Ta2O5 thin layer is less than or equal 10 Å.

### Claim 11 (depends on 7)

The method of claim 7, wherein the third source gas includes TiCl4, and the fourth source gas includes a gas selected from a group consisting of H2O, O2 and N2O gases.

### Claim 12 (depends on 7)

The method of claim 7, wherein a thickness of the TiO2 thin layer is less than or equal 5 Å.

### Claim 13 (depends on 7)

The method of claim 7, wherein the (Ta2O5)x(TiO2)y composite layer has a thickness ranging from approximately 100 Å to approximately 200 Å.

### Claim 14 (depends on 7)

The method of claim 7, wherein process cycles of steps (1) and (2) are controlled in such a way that x=0.92 and y=0.08.

### Claim 15 (depends on 7)

The method of claim 7, further comprising introducing a first inert gas into the reaction chamber for 0.1-10 seconds to remove the first and second source gases which remain in the reaction chamber, after step (1).

### Claim 16 (depends on 15)

The method of claim 15, further comprising introducing a second inert gas into the reaction chamber for 0.1-10 seconds to remove the first and second source gases and the first inert gas remain in the reaction chamber, after step (2).

### Claim 17 (depends on 7)

The method of claim 7, further comprising forming a dielectric layer over the (Ta2O5)x(TiO2)y, composite layer.

### Claim 18 (depends on 17)

The method of claim 17, further comprising heat treating the (Ta2O5)x(TiO2)y composite layer and the dielectric layer in a furnace at a temperature ranging from approximately 600° C. to approximately 850° C. in the presence of N2O.

### Claim 19 (depends on 17)

The method of claim 17, further comprising forming a TiN layer over the dielectric layer.

### Claim 20 (depends on 7)

The method of claim 7, wherein the first source gas includes tantalum chloride (TaCl5), and the second source gas includes a gas selected from a group consisting of H2O, O2, N2O and CxHyOH gases.