# US 2004/0082099 A1 · Elimination of dendrite formation during metal/chalcogenide glass deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082099 A1
- Document ID: US20040082099A1
- Status: Published application
- Kind: A1
- Application number: 10/602,483
- Filed: 2003-06-24
- Published: 2004-04-29
- Earliest claimed: 2002-06-06
- Assignees: Micron Technology, Inc.
- Inventors: Jiutao Lin; Allen McTeer
- Web page: https://patentgrep.com/patent/US20040082099A1

## CPC

- H10N 70/8825: {Selenides, e.g. GeSe}
- C23C 14/0688: {Cermets, e.g. mixtures of metal and one or more of carbides, nitrides, oxides or borides}
- C23C 14/541: {Heating or cooling of the substrates}
- H10N 70/026: {by physical vapor deposition, e.g. sputtering}
- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10N 70/245: {the species being metal cations, e.g. programmable metallization cells}
- H10N 70/882: {Compounds of sulfur, selenium or tellurium, e.g. chalcogenides}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of forming a programmable conductor memory cell array is disclosed wherein metal and chalcogenide glass are co-sputtered to fill an array of cell vias in a prepared substrate. The prepared substrate is heated above room temperature before the metal and chalcogenide glass film is deposited, and the heating is maintained throughout the deposition. The resulting metal/chalcogenide glass film has good homogeneity, a desired ratio of components, and has a regular surface.

## Claims

### Claim 1

A method of forming a programmable conductor memory cell comprising:
sputtering metal and chalcogenide glass onto a prepared substrate; and
maintaining the prepared substrate at a temperature higher than room temperature during the sputtering.

### Claim 2 (depends on 1)

The method of claim 1, wherein sputtering metal and chalcogenide glass comprises first sputtering a chalcogenide glass element and then separately sputtering a metal layer thereover.

### Claim 3 (depends on 1)

The method of claim 1, wherein sputtering metal and chalcogenide glass comprises co-sputtering.

### Claim 4 (depends on 1)

The method of claim 1, wherein the prepared substrate comprises a top insulating layer with vias therein.

### Claim 5 (depends on 1)

The method of claim 1, wherein the programmable conductor memory cell comprises metal and chalcogenide glass containing between about 25% and 35% metal.

### Claim 6 (depends on 1)

The method of claim 1, wherein the metal is a fast diffuser.

### Claim 7 (depends on 1)

The method of claim 1, wherein the metal is silver.

### Claim 8 (depends on 1)

The method of claim 1, wherein the metal is copper.

### Claim 9 (depends on 1)

The method of claim 1, wherein the chalcogenide glass comprises components selected from the group consisting of sulfur, germanium, selenium, and tellurium.

### Claim 10 (depends on 1)

The method of claim 1, wherein the chalcogenide glass comprises germanium selenide.

### Claim 11 (depends on 1)

The method of claim 1, further comprising maintaining the prepared substrate at a temperature higher than room temperature for at least 5 minutes before sputtering the metal and chalcogenide glass.

### Claim 12 (depends on 1)

The method of claim 1, wherein maintaining the prepared substrate at a temperature higher than room temperature comprises maintaining the prepared substrate at between about 30° C. and 150° C.

### Claim 13 (depends on 1)

The method of claim 1, wherein maintaining the prepared substrate at a temperature higher than room temperature comprises maintaining the prepared substrate at between about 45° C. and 60° C.

### Claim 14

A method of co-sputtering a homogeneous metal/chalcogenide glass layer onto an irregular surface, comprising keeping the irregular surface at an elevated temperature, above room temperature, before and during the co-sputtering.

### Claim 15 (depends on 14)

The method of claim 14, wherein the metal/chalcogenide glass layer comprises silver, germanium, and selenium.