# US 2004/0082081 A1 · Ultra-violet treatment for a tunnel barrier layer in a tunnel junction device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082081 A1
- Document ID: US20040082081A1
- Status: Published application
- Kind: A1
- Application number: 10/282,577
- Filed: 2002-10-29
- Published: 2004-04-29
- Earliest claimed: 2002-10-29
- Inventors: Manish Sharma
- Web page: https://patentgrep.com/patent/US20040082081A1

## CPC

- G11C 11/16: using elements in which the storage effect is based on magnetic spin effect
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- B82Y 40/00: Manufacture or treatment of nanostructures
- G01R 33/093: {using multilayer structures, e.g. giant magnetoresistance sensors (thin magnetic films H01F10/00)}
- G01R 33/098: {comprising tunnel junctions, e.g. tunnel magnetoresistance sensors}
- H01F 41/307: {insulating or semiconductive spacer}
- H10N 50/01: Manufacture or treatment
- G11C: STATIC STORES (semiconductor memory devices H10B)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A method for treating a tunnel barrier layer of a tunnel junction device is disclosed. The method includes irradiating a tunnel barrier layer with ultra-violet light to activate oxygen or nitrogen atoms disposed in the barrier layer so that those atoms will react with a material of the tunnel barrier layer to form a uniformly oxidized or nitridized tunnel barrier layer having minimal or no defects therein and/or a desired breakdown voltage. The ultra violet light can irradiate an already formed tunnel barrier layer or it can irradiate the tunnel barrier layer as it is being formed. Heat can be applied before, during, or after the irradiation step to increase activation and further reduce defects. The method is applicable to any tunnel junction device including a magnetic field sensitive memory device such as a MRAM.

## Claims

### Claim 1

A method of treating a tunnel barrier layer of a tunnel junction device, comprising:
forming the tunnel barrier layer on a precursor layer of the tunnel junction device;
transforming the tunnel barrier layer into an electrically non-conductive material by a process selected from the group consisting of an oxidation process and a nitridation process; and
irradiating the tunnel barrier layer with ultra-violet light, the ultra-violet light is incident on a reactant disposed in the tunnel barrier layer, and wherein the ultra-violet light is operative to activate the reactant so that the reactant reacts with a material of the tunnel barrier layer and transforms the material into the electrically non-conductive material.

### Claim 2 (depends on 1)

The method as set forth in claim 1 and further comprising continuing the irradiating with the ultra-violet light for a predetermined time until a desired property of the tunnel barrier layer is obtained.

### Claim 3 (depends on 2)

The method as set forth in claim 2, wherein the desired property of the tunnel barrier layer is a property selected from the group consisting of a predetermined defect density in the tunnel barrier layer, a predetermined breakdown voltage of the tunnel barrier layer, a change in a crystal structure of the tunnel barrier layer, and a change in a texture of a grain orientation of tunnel barrier layer.

### Claim 4 (depends on 1)

The method as set forth in claim 1, wherein the reactant is a material selected from the group consisting of oxygen, ozone, and nitrogen.

### Claim 5 (depends on 1)

The method as set forth in claim 1, wherein the material for the tunnel barrier layer comprises a material selected from the group consisting of aluminum, magnesium, boron, and tantalum.

### Claim 6 (depends on 1)

The method as set forth in claim 1 and further comprising:
heating the tunnel barrier layer to increase an activation rate of the reactant with the material of the tunnel barrier layer, the heating occurring at a time relative to the irradiating selected from the group consisting of a time before the irradiating, a time during the irradiating, and a time after the irradiating.

### Claim 7 (depends on 1)

The method as set forth in claim 1, wherein the forming comprises a process selected from the group consisting of RF sputtering, DC sputtering, evaporation, plasma assisted deposition, chemical vapor deposition, physical vapor deposition, plasma enhanced chemical vapor deposition, molecular beam epitaxy, and metalorganic chemical vapor deposition.

### Claim 8 (depends on 1)

The method as set forth in claim 1, wherein the oxidation process is a process selected from the group consisting of plasma oxidation, natural oxidation, room temperature natural oxidation, and UV-ozone oxidation.

### Claim 9

A method of treating a tunnel barrier layer of a tunnel junction device, comprising:
forming an electrically non-conductive tunnel barrier layer on a precursor layer of the tunnel junction device; and
irradiating the tunnel barrier layer with ultra-violet light, the ultra-violet light is incident on a reactant disposed in the tunnel barrier layer, and wherein the ultra-violet light is operative to activate the reactant so that the reactant reacts with a material of the electrically non-conductive tunnel barrier layer and transforms the material into an electrically non-conductive material.

### Claim 10 (depends on 9)

The method as set forth in claim 9, wherein the forming comprises a process selected from the group consisting of a sputtering process and a reactive sputtering process.

### Claim 11 (depends on 10)

The method as set forth in claim 10, wherein a target material for the sputtering process and the reactive sputtering process is a material selected from the group consisting of an oxide material and a nitride material.

### Claim 12 (depends on 9)

The method as set forth in claim 9 and further comprising:
heating the tunnel barrier layer to increase an activation rate of the reactant with the material of the electrically non-conductive tunnel barrier layer, the heating occurring at a time relative to the irradiating selected from the group consisting of a time before the irradiating, a time during the irradiating, and a time after the irradiating.

### Claim 13 (depends on 9)

The method as set forth in claim 9, wherein the material for the tunnel barrier layer comprises a material selected from the group consisting of aluminum, magnesium, boron, and tantalum.

### Claim 14 (depends on 9)

The method as set forth in claim 9 and further comprising continuing the irradiating with the ultra-violet light for a predetermined time until a desired property of the tunnel barrier layer is obtained.

### Claim 15 (depends on 14)

The method as set forth in claim 14, wherein the desired property of the tunnel barrier layer is a property selected from the group consisting of a predetermined defect density in the tunnel barrier layer, a predetermined breakdown voltage of the tunnel barrier layer, a change in a crystal structure of the tunnel barrier layer, and a change in a texture of a grain orientation of tunnel barrier layer.

### Claim 16

A method of treating a tunnel barrier layer formed on a precursor layer of a tunnel junction device, comprising:
irradiating the tunnel barrier layer with ultra-violet light, the ultra-violet light is incident on a reactant disposed in the tunnel barrier layer, and
wherein the ultra-violet light is operative to activate the reactant so that the reactant reacts with a material of the tunnel barrier layer and transforms the material into an electrically non-conductive material.

### Claim 17 (depends on 16)

The method as set forth in claim 16 and further comprising:
heating the tunnel barrier layer to increase an activation rate of the reactant with the material of the tunnel barrier layer, the heating occurring at a time relative to the irradiating selected from the group consisting of a time before the irradiating, a time during the irradiating, and a time after the irradiating.

### Claim 18 (depends on 16)

The method as set forth in claim 16, wherein the material for the tunnel barrier layer comprises a material selected from the group consisting of aluminum, magnesium, boron, and tantalum.

### Claim 19 (depends on 16)

The method as set forth in claim 16, wherein the reactant is a material selected from the group consisting of oxygen, ozone, and nitrogen.

### Claim 20 (depends on 16)

The method as set forth in claim 16 and further comprising continuing the irradiating with the ultra-violet light for a predetermined time until a desired property of the tunnel barrier layer is obtained.

### Claim 21 (depends on 20)

The method as set forth in claim 20, wherein the desired property of the tunnel barrier layer is a property selected from the group consisting of a predetermined defect density in the tunnel barrier layer, a predetermined breakdown voltage of the tunnel barrier layer, a change in a crystal structure of the tunnel barrier layer, and a change in a texture of a grain orientation of tunnel barrier layer.