# US 2004/0082072 A1 · Method and apparatus for measurement of sulfate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082072 A1
- Document ID: US20040082072A1
- Status: Published application
- Kind: A1
- Application number: 10/611,416
- Filed: 2003-07-01
- Published: 2004-04-29
- Earliest claimed: 2001-01-02
- Assignees: President and Fellows of Harvard College
- Inventors: George Allen; David Harrison
- Web page: https://patentgrep.com/patent/US20040082072A1

## CPC

- G01N 33/0013: {by a chemical reaction (a chemical reaction taking place or a gas being eliminated in one or more analysing channels G01N33/0024)}
- G01N 31/005: {investigating the presence of an element by oxidation (G01N31/12 takes precedence)}
- G01N 33/0042: {SO2 or SO3}
- Y02A 50/20: Air quality improvement or preservation, e.g. vehicle emission control or emission reduction by using catalytic converters
- Y10T 436/156666: Sulfur containing
- Y10T 436/18: Sulfur containing
- Y10T 436/186: Sulfur dioxide
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- Y02A: TECHNOLOGIES FOR ADAPTATION TO CLIMATE CHANGE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method and apparatus for sulfate analysis in a sample are provided. A portion of the sulfate contained in the sample is converted to sulfur dioxide, and at least a portion of the sulfur dioxide can be determined. The amount of sulfur dioxide determined can be used to quantify the amount of sulfate in the sample.

## Claims

### Claim 1

A method comprising:
providing a sample comprising sulfate;
converting at least a portion of the sulfate to sulfur dioxide; and
continuously determining the sulfur dioxide.

### Claim 2 (depends on 1)

The method of claim 1 wherein the sulfate is particulate sulfate.

### Claim 3 (depends on 1)

The method of claim 1 wherein at least a portion of the sulfate is ammonium sulfate.

### Claim 4 (depends on 1)

The method of claim 1 wherein the at least a portion of the sulfate is converted to sulfur dioxide by passing the sample over a surface.

### Claim 5 (depends on 4)

The method of claim 4 wherein the surface is at an elevated temperature.

### Claim 6 (depends on 4)

The method of claim 4 wherein the surface comprises a transition metal.

### Claim 7 (depends on 6)

The method of claim 6 wherein the surface comprises stainless steel.

### Claim 8 (depends on 6)

The method of claim 6 wherein the surface comprises chromium.

### Claim 9 (depends on 8)

The method of claim 8 wherein the surface comprises chromium carbide.

### Claim 10 (depends on 8)

The method of claim 8 wherein the surface comprises a chromium salt.

### Claim 11 (depends on 1)

The method of claim 1 wherein the sulfur dioxide is determined by pulsed fluorescence detection.

### Claim 12 (depends on 1)

The method of claim 1 further comprising quantifying the amount of sulfur dioxide determined.

### Claim 13 (depends on 12)

The method of claim 12 further comprising determining the amount of sulfate converted to sulfur dioxide.

### Claim 14 (depends on 1)

The method of claim 1 wherein at least 50% of the sulfate is converted to sulfur dioxide.

### Claim 15 (depends on 14)

The method of claim 14 wherein at least 90% of the sulfate is converted to sulfur dioxide.

### Claim 16 (depends on 12)

The method of claim 12 further comprising:
removing at least a portion of any particulate matter from at least a portion of the sample to produce a background sample essentially free of particulate sulfate; and
detecting a positive or negative sulfur dioxide response in the background sample.

### Claim 17 (depends on 16)

The method of claim 16 further comprising subtracting the positive or negative response from the amount of sulfur dioxide determined.

### Claim 18 (depends on 1)

The method of claim 1 wherein the at least a portion of the sulfate is continuously converted to sulfur dioxide.

### Claim 19 (depends on 1)

The method of claim 1 wherein the sample is a fluid.

### Claim 20 (depends on 19)

The method of claim 19 wherein the fluid is air.

### Claim 21

A method comprising:
passing a sample comprising sulfate over a surface, the surface comprising a transition metal and being at an elevated temperature;
reducing at least a portion of the sulfate to sulfur dioxide; and
continuously determining at least a portion of the sulfur dioxide.

### Claim 22 (depends on 21)

The method of claim 21 wherein at least 50% of the sulfate is reduced to sulfur dioxide.

### Claim 23 (depends on 22)

The method of claim 22 wherein at least 80% of the sulfate is reduced to sulfur dioxide.

### Claim 24 (depends on 23)

The method of claim 23 wherein at least 90% of the sulfate is reduced to sulfur dioxide.

### Claim 25 (depends on 24)

The method of claim 24 wherein at least 95% of the sulfate is reduced to sulfur dioxide.

### Claim 26 (depends on 21)

The method of claim 21 wherein the temperature is greater than 500° C.

### Claim 27 (depends on 26)

The method of claim 26 wherein the temperature is greater than 800° C.

### Claim 28 (depends on 27)

The method of claim 27 wherein the temperature is greater than 1000° C.

### Claim 29 (depends on 28)

The method of claim 28 wherein the temperature is about 1100° C.

### Claim 30 (depends on 21)

The method of claim 21 wherein the sample is a fluid.

### Claim 31 (depends on 30)

The method of claim 30 wherein the fluid is air.

### Claim 32 (depends on 21)

The method of claim 21 wherein the sulfate comprises particulate matter.

### Claim 33 (depends on 21)

The method of claim 21 further comprising removing at least a portion of any sulfur dioxide that may be in the sample prior to reducing the sulfate to sulfur dioxide.

### Claim 34 (depends on 21)

The method of claim 21 comprising removing particles of a size greater than about 2.5 μm from the sample prior to passing the sample over the surface.

### Claim 35 (depends on 21)

The method of claim 21 wherein the sulfur dioxide is determined quantitatively.

### Claim 36 (depends on 21)

The method of claim 21 wherein the determining is performed with a pulsed fluorescence sulfur dioxide detector.

### Claim 37 (depends on 21)

The method of claim 21 wherein the sulfur dioxide is determined at a rate of more than one reading per hour.

### Claim 38 (depends on 37)

The method of claim 37 wherein the sulfur dioxide is determined at a rate of more than one reading per minute.

### Claim 39 (depends on 38)

The method of claim 38 wherein the sulfur dioxide is determined at a rate of more than one reading per second.

### Claim 40 (depends on 21)

The method of claim 21 wherein the sulfur dioxide is determined at a rate of about 10 times per second.

### Claim 41 (depends on 21)

The method of claim 21 wherein the surface comprises stainless steel.

### Claim 42 (depends on 21)

The method of claim 21 wherein the surface comprises a chromium alloy.

### Claim 43 (depends on 21)

The method of claim 21 wherein the surface comprises chromium carbide.

### Claim 44 (depends on 21)

The method of claim 21 wherein the surface comprises a powder.

### Claim 45 (depends on 21)

The method of claim 21 wherein the surface comprises a metallic chromium wool.

### Claim 46 (depends on 21)

The method of claim 21 wherein the surface comprises tubing.

### Claim 47

A device comprising:
a surface comprising a transition metal; and
a sulfur dioxide detector in fluid communication with the surface.

### Claim 48 (depends on 47)

The device of claim 47 wherein an air source is in fluid communication with the surface.

### Claim 49 (depends on 47)

The device of claim 47 wherein the detector is a fluorescence detector.

### Claim 50 (depends on 47)

The device of claim 47 wherein the surface comprises chromium.

### Claim 51 (depends on 47)

The device of claim 47 wherein the surface comprises at least 10%, by weight, of chromium.

### Claim 52 (depends on 50)

The device of claim 50 wherein the surface comprises a chromium salt.

### Claim 53 (depends on 47)

The device of claim 47 wherein the surface comprises chromium carbide.

### Claim 54 (depends on 47)

The device of claim 47 wherein the surface comprises a stainless steel tube.

### Claim 55 (depends on 47)

The device of claim 47 wherein the temperature of the surface is greater than about 500° C.

### Claim 56 (depends on 55)

The device of claim 55 wherein the temperature is greater than about 800° C.

### Claim 57 (depends on 56)

The device of claim 56 wherein the temperature is greater than about 900° C.

### Claim 58 (depends on 57)

The device of claim 57 wherein the temperature is greater than about 1000C.

### Claim 59 (depends on 58)

The device of claim 58 wherein the temperature is about 1100° C.

### Claim 60 (depends on 47)

The device of claim 47 wherein the surface is disposed in a quartz furnace.

### Claim 61 (depends on 55, 56, 57, 58)

The device of claim 55, 56, 57, 58, or 59 further comprising air flowing across the surface.

### Claim 62

A method comprising:
passing air comprising particulate matter across a heated surface comprising chromium, the particulate matter comprising sulfate;
reducing at least a portion of the sulfate to sulfur dioxide; and
determining sulfur dioxide.

### Claim 63 (depends on 62)

The method of claim 62 wherein the sulfur dioxide is determined via a pulse fluorescence sulfur dioxide detector.

### Claim 64 (depends on 62)

The method of claim 62 further comprising removing at least a portion of any sulfur dioxide from the air prior to passing the air across the surface.

### Claim 65 (depends on 62)

The method of claim 62 further comprising excluding particles of a size greater than about 2.5 μm prior to passing the air across the surface.

### Claim 66 (depends on 62)

The method of claim 62 further comprising pretreating the air with ammonia.

### Claim 67 (depends on 62)

The method of claim 62 further comprising correlating a concentration of sulfur dioxide determined with an amount of sulfate in the air.

### Claim 68 (depends on 62)

The method of claim 62 further comprising heating at least a portion of the surface to a temperature greater than about 500° C.

### Claim 69 (depends on 68)

The method of claim 68 wherein the temperature is greater than about 800° C.

### Claim 70 (depends on 69)

The method of claim 69 wherein the temperature is greater than about 900° C.

### Claim 71 (depends on 69)

The method of claim 69 wherein the temperature is greater than about 1000° C.

### Claim 72 (depends on 71)

The method of claim 71 wherein the temperature is about 1100° C.

### Claim 73 (depends on 62)

The method of claim 62 wherein the surface comprises stainless steel.

### Claim 74 (depends on 62)

The method of claim 62 wherein the surface comprises chromium carbide.

### Claim 75 (depends on 62)

The method of claim 62 wherein the particulate matter is classified as PM 10.

### Claim 76 (depends on 62)

The method of claim 62 wherein the particulate matter is classified as PM 2.5.

### Claim 77 (depends on 62)

The method of claim 62 wherein the air is passed continuously across the heated surface.

### Claim 78 (depends on 62)

The method of claim 62 wherein the sulfur dioxide is continuously determined.

### Claim 79 (depends on 62)

The method of claim 62 further comprising filtering at least a portion of the particulate matter from the air sample to produce a second air sample;
determining a positive or negative sulfur dioxide response in the second air sample; and
comparing the determined response in the second air sample with a response determined in the air sample.

### Claim 80

A method of measuring particulate sulfate content in a fluid sample comprising:
providing a sample comprising particulate matter;
continuously contacting the sample with means for reducing the sulfate to sulfur dioxide; and
analytically determining sulfur dioxide in the sample.

### Claim 81 (depends on 80)

The method of claim 80 wherein the means comprises a surface having a temperature greater than about 500° C.

### Claim 82 (depends on 80)

The method of claim 80 wherein the means comprises a surface comprising chromium, and the surface is at a temperature greater than about 800° C.

### Claim 83

An apparatus comprising:
means for continuously converting at least 50% of any aerosol sulfate in an air sample to sulfur dioxide; and
means for detecting sulfur dioxide in the air sample.

### Claim 84 (depends on 83)

The apparatus of claim 83 wherein the means can convert at least 80% of any aerosol sulfate in the air sample.