# US 2004/0081918 A1 · Polysilicon hard mask etch defect particle removal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0081918 A1
- Document ID: US20040081918A1
- Status: Published application
- Kind: A1
- Application number: 10/272,655
- Filed: 2002-10-17
- Published: 2004-04-29
- Earliest claimed: 2002-10-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chu-Sheng Lee; Tou-Yu Chen
- Web page: https://patentgrep.com/patent/US20040081918A1

## CPC

- H10P 50/667: {by liquid etching only}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10W 20/031: {of conductive parts of the interconnections}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The removal of defect particles that may be created during polysilicon hard mask etching, and that are embedded within the polysilicon layer, is disclosed. Oxide is first grown in the polysilicon layer exposed through the patterned hard mask layer, so that the defect particle becomes embedded within the oxide. Oxide growth may be accomplished by rapid thermal oxidation (RTO). The oxide is then exposed to an acidic solution, such as hydrofluoric (HF) acid, to remove the oxide and the embedded defect particle embedded therein.

## Claims

### Claim 1

A method for removing a defect particle created during a silicon-based hard mask etching, comprising:
forming an oxide in a silicon-based layer exposed through a patterned hard mask layer, the defect particle becoming embedded within the oxide; and,
exposing the oxide to an acidic solution to remove the oxide and the defect particle.

### Claim 2 (depends on 1)

The method of claim 1, wherein growing the oxide comprises employing a rapid thermal oxidation (RTO) process.

### Claim 3 (depends on 1)

The method of claim 1, wherein employing the RTO process comprises exposing a semiconductor wafer including the patterned hard mask layer and the silicon-based layer to a temperature of substantially 700° C. for substantially thirty seconds.

### Claim 4 (depends on 1)

The method of claim 1, wherein exposing the oxide to the acidic solution comprises exposing the oxide to a hydrofluoric (HF) acidic solution.

### Claim 5 (depends on 1)

The method of claim 1, wherein exposing the oxide to the HF acidic solution comprises dipping a semiconductor wafer including the patterned hard mask layer and the silicon-based layer into the HF acidic solution for substantially thirty seconds.

### Claim 6 (depends on 1)

The method of claim 1, wherein exposing the oxide to the HF acidic solution comprises exposing the oxide to a substantially 100:1 water:HF acid solution.

### Claim 7 (depends on 1)

The method of claim 1, further initially comprising etching the hard mask layer through a patterned photoresist layer to pattern the hard mask layer.

### Claim 8 (depends on 1)

The method of claim 1, further initially comprising patterning the photoresist layer prior to etching the hard mask layer.

### Claim 9 (depends on 1)

The method of claim 1, further initially comprising removing the photoresist layer after etching the hard mask layer.

### Claim 10 (depends on 1)

The method of claim 1, further comprising etching the silicon-based layer through the patterned hard mask layer.

### Claim 11 (depends on 1)

The method of claim 1, further comprising removing the hard mask layer.

### Claim 12 (depends on 1)

The method of claim 1, wherein the hard mask layer comprises an upper layer and a lower layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the upper layer comprises a SiO2 layer.

### Claim 14 (depends on 12)

The method of claim 12, wherein the lower layer comprises a SiON layer.

### Claim 15

A method for removing a defect particle created during silicon-based hard mask etching, comprising:
growing oxide in a polysilicon layer exposed through a patterned hard mask layer via rapid thermal oxidation (RTO), the defect particle becoming embedded within the oxide; and,
exposing the oxide to a hydrofluoric (HF) acidic solution to remove the oxide and the defect particle.

### Claim 16 (depends on 15)

The method of claim 15, wherein growing the oxide in the silicon-based layer via the RTO comprises exposing a semiconductor wafer including the patterned hard mask layer and the silicon-based layer to a temperature of substantially 700° C. for substantially thirty seconds.

### Claim 17 (depends on 15)

The method of claim 15, wherein exposing the oxide to the HF acidic solution comprises dipping a semiconductor wafer including the patterned hard mask layer and the polysilicon layer into the HF acidic solution for substantially thirty seconds.

### Claim 18 (depends on 15)

The method of claim 15, wherein exposing the oxide to the HF acidic solution comprises exposing the oxide to a substantially 100:1 water:HF acid solution.

### Claim 19 (depends on 15)

The method of claim 15, wherein the hard mask layer comprises an upper SiO2 layer and a lower SiON layer.

### Claim 20

A semiconductor device fabricated at least in part by a method comprising:
patterning a photoresist layer over a hard mask layer over a polysilicon layer;
etching the hard mask layer through the patterned photoresist layer to correspondingly pattern the hard mask layer, and resulting in one or more defect particles embedded in the polysilicon layer exposed through the patterned hard mask layer;
removing the photoresist layer;
growing oxide in the polysilicon layer exposed through the patterned hard mask layer, embedding the one or more defect particles in the oxide;
exposing the oxide to an acidic solution to remove the oxide and the one or more defect particles;
etching the polysilicon layer through the patterned hard mask layer; and
removing the hard mask layer.