# US 2004/0081602 A1 · Recovery of platinum group metals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0081602 A1
- Document ID: US20040081602A1
- Status: Published application
- Kind: A1
- Application number: 10/280,714
- Filed: 2002-10-25
- Published: 2004-04-29
- Earliest claimed: 2002-10-25
- Assignees: South Dakota School of Mines and Technology
- Inventors: Kenneth N. Han; Peter Nam-soo Kim
- Web page: https://patentgrep.com/patent/US20040081602A1

## CPC

- C22B 11/04: {by wet processes (extraction of metal compounds by leaching in organic solutions C22B3/16; treatment or purification of solutions by liquid-liquid extraction C22B3/26)}
- C22B 1/06: Sulfating roasting
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

This invention relates to the recovery of platinum group metals and, more particularly, to the recovery of platinum group metals from various sources by roasting the source material with one or more of sulfuric acid, a sulfate and/or a bi-sulfate and with one or more halogen salt. The roasted product is put in contact with a leaching solution to dissolve at least a portion of the platinum group metals, which then may be separated and recovered.

## Claims

### Claim 1

A method of recovering a platinum group metal from a source material, comprising:
a) mixing a source material comprising a platinum group metal with at least one of sulfuric acid, a sulfate and a bi-sulfate, and with at least one halogen salt to form a roasting mixture;
b) heating the roasting mixture to a temperature in the range of approximately 300° Celsius to approximately 1,000° Celsius to form a roasted product;
c) contacting the roasted product with a leaching solution to dissolve at least a portion of the platinum group metal into the leaching solution; and
d) recovering at least a portion of the platinum group metal from the leaching solution.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sulfate is selected from the group consisting of sodium sulfate, potassium sulfate and ammonium sulfate.

### Claim 3 (depends on 1)

The method of claim 1, wherein the bi-sulfate is selected from the group consisting of sodium bi-sulfate, potassium bi-sulfate and ammonium bi-sulfate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the halogen salt is selected from the group consisting of sodium chloride, potassium chloride, ammonium chloride, sodium bromide, potassium bromide, ammonium bromide, sodium iodide, potassium iodide and ammonium iodide.

### Claim 5 (depends on 1)

The method of claim 1, wherein the roasting mixture is heated to a temperature of approximately 450° Celsius to approximately 700° Celsius.

### Claim 6 (depends on 1)

The method of claim 1, wherein the leaching solution has a pH of approximately 0.5 to approximately 7.

### Claim 7 (depends on 1)

The method of claim 1, wherein the leaching solution comprises at least one of hydrochloric acid, nitric acid, sulfuric acid, halogen salt media, and ammonium salts.

### Claim 8 (depends on 1)

The method of claim 1, further comprising adding water to the roasting mixture before heating the roasting mixture.

### Claim 9 (depends on 1)

The method of claim 1, further comprising adding water to the roasting mixture and removing at least some of the water from the roasting mixture before heating.

### Claim 10 (depends on 1)

The method of claim 1, wherein the leaching solution comprises an oxidant.

### Claim 11 (depends on 1)

The method of claim 1, wherein the leaching solution comprises at least one oxidant selected from the group consisting of chlorine, iodine and bromine.

### Claim 12

A method of separating a platinum group metal from a source material, comprising:
a) combining a source material comprising at least one platinum group metal with a solution comprising water, at least one halogen salt, and at least one of sulfuric acid, a sulfate and a bi-sulfate to form a roasting mixture;
b) heating the roasting mixture to a temperature of approximately 300° Celsius to approximately 1,000° Celsius to form a roasted product;
c) contacting the roasted product with a leaching solution having a pH of approximately 0.5 to approximately 7; and
d) separating at least a portion of the platinum group metal from the leaching solution.

### Claim 13 (depends on 12)

The method of claim 12, wherein the sulfuric acid is concentrated sulfuric acid.

### Claim 14 (depends on 12)

The method of claim 12, wherein the sulfate is selected from the group consisting of sodium sulfate, potassium sulfate and ammonium sulfate.

### Claim 15 (depends on 12)

The method of claim 12, wherein the bi-sulfate is selected from the group consisting of sodium bi-sulfate, potassium bi-sulfate and ammonium bi-sulfate.

### Claim 16 (depends on 12)

The method of claim 12, wherein the halogen salt is selected from the group consisting of sodium chloride, potassium chloride, ammonium chloride, sodium bromide, potassium bromide, ammonium bromide, sodium iodide, potassium iodide and ammonium iodide.

### Claim 17 (depends on 12)

The method of claim 12, wherein the roasting mixture is heated to a temperature of approximately 450° Celsius to approximately 700° Celsius.

### Claim 18 (depends on 24)

The method of claim 24, wherein the roasting mixture is heated to a temperature of approximately 550° Celsius.

### Claim 19 (depends on 12)

The method of claim 12, wherein the leaching solution has a pH of approximately 1.

### Claim 20 (depends on 12)

The method of claim 12, wherein the leaching solution comprises at least one of hydrochloric acid, nitric acid, sulfuric acid, halogen salt media, and ammonium salts.

### Claim 21 (depends on 12)

The method of claim 12, further comprising removing at least some of the water from the roasting mixture before heating the roasting mixture.

### Claim 22 (depends on 12)

The method of claim 12, wherein the leaching solution comprises an oxidant.

### Claim 23 (depends on 12)

The method of claim 12, wherein the leaching solution comprises at least one oxidant selected from the group consisting of chlorine, iodine and bromine.

### Claim 24

A method of recovering platinum group metals from a catalyst matrix, comprising:
a) crushing a catalyst matrix containing at least one platinum group metal;
b) mixing the crushed catalyst matrix with one or more of sulfuric acid, a sulfate and a bi-sulfate, with at least one halogen salt and with water to form a roasting mixture;
c) roasting the roasting mixture at a temperature of approximately 300° Celsius to approximately 1,000° Celsius to form a roasted product;
d) contacting the roasting product with an acidic leaching solution;
e) separating the non-dissolved solids from the leaching solution; and
f) recovering at least a portion of the platinum group metal from the leaching solution.

### Claim 25 (depends on 24)