# US 2004/0080868 A1 · Electroplated magnetic thin film, method of manufacturing the same, electroplating bath and thin film magnetic head

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0080868 A1
- Document ID: US20040080868A1
- Status: Published application
- Kind: A1
- Application number: 10/376,607
- Filed: 2003-03-03
- Published: 2004-04-29
- Earliest claimed: 2002-03-06
- Assignees: TDK Corporation
- Inventors: Atsushi Yamaguchi; Tetsuya Mino; Seiji Yari; Shigeru Ichihara
- Web page: https://patentgrep.com/patent/US20040080868A1

## CPC

- G11B 5/3109: {Details (G11B5/3103 takes precedence)}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- B82Y 40/00: Manufacture or treatment of nanostructures
- G11B 5/3163: {Fabrication methods or processes specially adapted for a particular head structure, e.g. using base layers for electroplating, using functional layers for masking, using energy or particle beams for shaping the structure or modifying the properties of the basic layers}
- G11B 5/3909: {Arrangements using a magnetic tunnel junction}
- G11B 5/3967: {Composite structural arrangements of transducers, e.g. inductive write and magnetoresistive read (G11B5/3906 takes precedence)}
- H01F 10/16: containing cobalt ({H01F10/126} , H01F10/13 take precedence)
- H01F 10/324: {Exchange coupling of magnetic film pairs via a very thin non-magnetic spacer, e.g. by exchange with conduction electrons of the spacer}
- H01F 41/26: using electric currents {, e.g. electroplating}
- H01F 41/309: {electroless or electrodeposition processes from plating solution}
- G11B 2005/3996: {large or giant magnetoresistive effects [GMR], e.g. as generated in spin-valve [SV] devices}
- Y10T 428/115: Magnetic layer composition
- Y10T 428/1186: with head pole component
- Y10T 428/1193: with interlaminar component [e.g., adhesion layer, etc.]
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An electroplated magnetic thin film consisting of an electroplated film of Fe—Co alloy containing Fe by an amount of 52-86 wt % and having a highly packed fine crystal grain structure, a flat and glossy surface, a high saturation magnetic flux density not less than 2.1 T, a low coercive force of 5-10 Oe, and being particularly suitable as a pole portion of a thin film magnetic head is proposed. The electroplated magnetic thin film is deposited on a substrate by an electroplating process with a pulsatory current or direct current having a current density of 3-120 mA/cm while using an electroplating bath containing one or both of sulfate salt and hydrochloric salt serving as supply sources of Fe ions and Co ions, saccharin sodium serving as a stress relaxation agent by an amount not less than 1 g/l, boric acid as a pH buffer agent, ammonium chloride as an electrically conductivity salt, and sodium lauryl sulfate as a surfactant.

## Claims

### Claim 1

An electroplated magnetic thin film consisting of an electroplated film of Fe—Co alloy containing Fe by an amount of 52-86 wt % and having a highly packed fine crystal grain structure and a flat and glossy surface.

### Claim 2 (depends on 1)

The electroplated magnetic thin film according to claim 1, wherein said electroplated magnetic thin film has a saturation magnetic flux density not less than 2.1 T.

### Claim 3 (depends on 1)

The electroplated magnetic thin film according to claim 1, wherein said electroplated magnetic thin film contains Fe by an amount of 58-70 wt %.

### Claim 4 (depends on 3)

The electroplated magnetic thin film according to claim 3, wherein said electroplated magnetic thin film has a saturation magnetic flux density not less than 2.2 T.

### Claim 5 (depends on 1)

The electroplated magnetic thin film according to claim 1, wherein said electroplated magnetic thin film has a coercive force in an axis of difficult magnetization of 5-10 Oe.

### Claim 6 (depends on 1)

The electroplated magnetic thin film according to claim 1, wherein said electroplated magnetic thin film is formed by an electroplating using a pulsatory current.

### Claim 7

A method of manufacturing an electroplated magnetic thin film, wherein a magnetic thin film made of Fe—Co alloy containing Fe by an amount of 52-86 wt % and having a highly packed fine crystal grain structure, a flat and glossy surface and a saturation magnetic flux density not less than 2.1 T is deposited on a substrate using a pulsatory current as an electroplating current.

### Claim 8

A method of manufacturing an electroplated magnetic thin film made of Fe—Co alloy containing Fe by an amount of 52-86 wt % and having a highly packed fine crystal grain structure, a flat and glossy surface and a saturation magnetic flux density not less than 2.1 T, wherein said electroplated magnetic thin film is deposited on a substrate by an electroplating process using a pulsatory current or direct current and an electroplating bath containing one or both of sulfate salt and hydrochloric salt serving as a supply source of Fe ions and Co ions, saccharin sodium serving as a stress relaxation agent by not less than 1 g/l and at least one of a pH buffer agent, an electrically conductive salt and a surfactant.

### Claim 9 (depends on 8)

The method of manufacturing a magnetic thin film according to claim 8, wherein said electroplating bath contains boric acid as a pH buffer agent.

### Claim 10 (depends on 8)

The method of manufacturing an electroplated magnetic thin film according to claim 8, wherein said electroplating bath contains ammonium chloride as an electrically conductivity salt.

### Claim 11 (depends on 8)

The method of manufacturing an electroplated magnetic thin film according to claim 8, wherein said electroplating bath contains sodium lauryl sulfate as a surfactant.

### Claim 12 (depends on 8)

The method of manufacturing an electroplated magnetic thin film according to claim 8, wherein said pulsatory current or direct current has a current density of 3-120 mA/cm2.

### Claim 13 (depends on 12)

The method of manufacturing an electroplated magnetic thin film according to claim 12, wherein said pulsatory current or direct current has a current density of 20-120 mA/cm2 and said electroplated magnetic thin film has a coercive force in an axis of difficult magnetization of 5-10 Oe.

### Claim 14

An electroplating bath for use in manufacturing an electroplated magnetic thin film made of Fe—Co alloy containing Fe by an amount of 52-86 wt % and having a highly packed fine crystal grain structure, a flat and glossy surface and a saturation magnetic flux density not less than 2.1 T, wherein said electroplating bath contains one or both of sulfate salt and hydrochloric salt serving as supply sources of Fe ions and Co ions, saccharin sodium serving as a stress relaxation agent by not less than 1 g/l, and at least one of a pH buffer agent, an electrically conductive salt and a surfactant

### Claim 15 (depends on 14)

The electroplating bath according to claim 14, wherein said electroplating bath contains boric acid as a pH buffer agent.

### Claim 16 (depends on 14)

The electroplating bath according to claim 14, wherein said electroplating bath contains ammonium chloride as an electrically conductivity salt.

### Claim 17 (depends on 14)

The electroplating bath according to claim 14, wherein said electroplating bath contains sodium lauryl sulfate as a surfactant.

### Claim 18

A thin film magnetic head comprising:
a first magnetic thin film having a pole portion which is to be opposed to a magnetic record medium;
a second magnetic thin film having a pole portion constituting an air bearing surface together with the pole portion of the first magnetic thin film, and being magnetically coupled with the first magnetic thin film at a back gap position remote from the air bearing surface;
a write gap film made of a non-magnetic material and interposed between the pole portion of the first magnetic thin film and the pole portion of the second magnetic thin film at at least the air bearing surface;
a thin film coil having a portion arranged between said first magnetic thin film and the second magnetic thin film in an insulated and isolated manner; and
a substrate supporting said first and second magnetic thin films, write gap film and thin film coil;
wherein one or both of said first and second magnetic thin film is formed by an electroplated magnetic thin film made of Fe—Co alloy containing Fe by an amount of 52-86 wt % and having a highly packed fine crystal grain structure and a flat and glossy surface.

### Claim 19 (depends on 18)

The thin film magnetic head according to claim 18, wherein said electroplated magnetic thin film has a saturation magnetic flux density not less than 2.1 T.

### Claim 20 (depends on 18)

The thin film magnetic head according to claim 18, wherein said electroplated magnetic thin film contains Fe by an amount of 58-70 wt %.

### Claim 21 (depends on 20)

The thin film magnetic head according to claim 20, wherein said electroplated magnetic thin film has a saturation magnetic flux density not less than 2.2 T.

### Claim 22 (depends on 18)

The thin film magnetic head according to claim 18, wherein said electroplated magnetic thin film has a coercive force in an axis of difficult magnetization of 5-10 Oe.

### Claim 23 (depends on 18)

The thin film magnetic head according to claim 18, wherein said electroplated magnetic thin film is formed by an electroplating process using a pulsatory current.

### Claim 24 (depends on 18)

The thin film magnetic head according to claim 18, wherein said thin film magnetic head is formed as a combination type thin film magnetic head, in which a magnetoresistive type thin film magnetic head element for reading magnetic information out of a magnetic record medium and an inductive type thin film magnetic head element for recoding the magnetic information on the magnetic record medium, and at least the pole portion of said second magnetic thin film opposite to the magnetoresistive type thin film magnetic head element with respect to the write gap film is consisting of a sputtered thin film of Fe—Co alloy containing Fe by 52-86 wt % and an electroplated thin film of Fe—Co containing Fe by 52-86 wt % formed by an electroplating process using said sputtered thin film as seed layer, said sputtered thin film of Fe—Co alloy containing oxygen by an amount of 0.01-5.0 atomic % measured at a position which is substantially on an effective air bearing surface and is separated from a reference point by 25 nm, said reference point situating on a bisecting center line of a width of the pole portion as well as on a boundary surface between the second magnetic thin film and the write gap film.

### Claim 25 (depends on 24)

The thin film magnetic head according to claim 24, wherein said seed layer of the second magnetic thin film contains Fe by an amount of 55-75 wt %.

### Claim 26 (depends on 25)

The thin film magnetic head according to claim 25, wherein said seed layer of the second magnetic thin film contains Fe by an amount of 63-73 wt %.

### Claim 27 (depends on 24)

The thin film magnetic head according to claim 24, wherein said seed layer of the second magnetic thin film has a coercive force in an axis of difficult magnetization of 400-16000 A/m (5-200 Oe).

### Claim 28 (depends on 24)

The thin film magnetic head according to claim 24, wherein said seed layer of the second magnetic thin film has a thickness of 30-500 nm.