# US 2004/0080271 A1 · Plasma display device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0080271 A1
- Document ID: US20040080271A1
- Status: Published application
- Kind: A1
- Application number: 10/468,727
- Filed: 2003-08-22
- Published: 2004-04-29
- Earliest claimed: 2001-10-23
- Assignees: Matsushita Electric Industrial Co., Ltd.
- Inventors: Masaki Aoki; Mitsuhiro Otani; Hiroyuki Kawamura; Kazuhiko Sugimoto; Junichi Hibino
- Web page: https://patentgrep.com/patent/US20040080271A1

## CPC

- C09K 11/77342: {Silicates}
- H01J 9/223: {by uniformly dispersing of liquid}
- H01J 2211/42: Fluorescent layers
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Disclosed is a plasma display device that provides high luminance and minimal degradation in luminance under panel operations. A blue phosphor in a phosphor layer has a crystal structure of MeMgSi2O6:Eu or Me3MgSi2O8:Eu (where, Me contains at least one of Ca, Sr, and Ba) produced with a precursor that is obtained by any one of methods: an aqueous solution synthesis method, a spray synthesis method, a hydrothermal synthesis method, and a hydrolysis method. The phosphor has an average particle diameter ranging from 0.1 to 3.0 μm.

## Claims

### Claim 1

A plasma display device having a plasma display panel in which a plurality of discharge cells having any one of one and a plurality of colors are disposed, phosphor layers having a color corresponding to the respective discharge cells are disposed, and the phosphor layers are excited by ultraviolet light to emit light, wherein the phosphor layers have a compound blue phosphor with a crystal structure of any one of MeMgSi2O6:Eu and Me3MgSi2O8:Eu (where, Me is a combination of at least one of Ca, Sr, and Ba) that are manufactured using a precursor prepared through an aqueous solution synthesis method, a phosphor particle obtained has an average particle diameter ranging from 0.1 to 3.0 μm, and has a particle diameter of at most 8 μm.

### Claim 2

A plasma display device having a plasma display panel in which a plurality of discharge cells having any one of one and a plurality of colors are disposed, phosphor layers having a color corresponding to the respective discharge cells are disposed, and the phosphor layers are excited by ultraviolet light to emit light, wherein the phosphor layers have a compound blue phosphor with a crystal structure of any one of MeMgSi2O6:Eu and Me3MgSi2O8:Eu (where, Me is a combination of at least one of Ca, Sr, and Ba) that are manufactured using a precursor prepared through a spray synthesis method, a phosphor particle obtained has an average particle diameter ranging from 0.1 to 3.0 μm, and the phosphor layer formed of the phosphor particles has a film thickness ranging from 3 to 20 μm.

### Claim 3

A plasma display device having a plasma display panel in which a plurality of discharge cells having any one of one and a plurality of colors are disposed, phosphor layers having a color corresponding to the respective discharge cells are disposed, and the phosphor layers are excited by ultraviolet light to emit light, wherein the phosphor layers have a compound blue phosphor with a crystal structure of any one of MeMgSi2O6:Eu and Me3MgSi2O8:Eu (where, Me is a combination of at least one of Ca, Sr, and Ba) that are manufactured using a precursor prepared through a hydrothermal synthesis method, a phosphor particle obtained has an average particle diameter ranging from 0.1 to 3.0 μm, and the phosphor layer formed of the phosphor particles has a film thickness ranging from 3 to 20 μm.

### Claim 4

A plasma display device having a plasma display panel in which a plurality of discharge cells having any one of one and a plurality of colors are disposed, phosphor layers having a color corresponding to the respective discharge cells are disposed, and the phosphor layers are excited by ultraviolet light to emit light, wherein the phosphor layers have a compound blue phosphor with a crystal structure of any one of MeMgSi2O6:Eu and Me3MgSi2O8:Eu (where, Me is a combination of at least one of Ca, Sr, and Ba) that are manufactured using a precursor prepared through a hydrolysis method, a phosphor particle obtained has an average particle diameter ranging from 0.1 to 3.0 μm, and the phosphor layer formed of the phosphor particles has a film thickness ranging from 3 to 20 μm.

### Claim 5

A blue phosphor excited by ultraviolet light to emit visible light, and have a crystal structure of MeMgSi2O6:Eu (where, Me is a combination of at least one of Ca, Sr, and Ba).

### Claim 6 (depends on 5)

The blue phosphor as defined in claim 5, wherein a particle of the phosphor has an average particle diameter ranging from 0.1 to 3.0 μm, and has a particle diameter of at most 8 μm.

### Claim 7 (depends on 5)

A method of manufacturing the blue phosphor as defined in claim 5, the method comprising:
a mixed solution fabricating step of preparing a mixed solution by mixing a material and an aqueous medium;
a hydrate fabricating step of preparing a hydrate by mixing the mixed solution and an aqueous base; and
a hydrothermal synthesis step of performing a hydrothermal synthesis reaction on a solution containing the hydrate and water therein at temperatures ranging from 100 to 300° C. under pressures ranging from 0.2 to 10 MPa.

### Claim 8 (depends on 5)

A method of manufacturing the blue phosphor as defined in claim 5, the method comprising:
a mixed solution fabricating step of preparing a mixed solution by mixing a material and an aqueous medium;
a precursor forming step of preparing a hydrate by mixing the mixed solution and an aqueous base in a vibrating container with an application of ultrasonic wave and O2-(O3-)bubbling;
a baking step of drying the hydrate and then baking the hydrate in an air at temperatures ranging from 800 to 1250° C.;
a baking step of baking the hydrate in a reducing atmosphere at temperatures ranging from 1000 to 1400° C.

### Claim 9 (depends on 5)

A method of manufacturing the blue phosphor as defined in claim 5, the method comprising:
a mixed solution fabricating step of mixing organic metal that contains Ca, Ba, Sr, Mg, and Eu, with an aqueous medium;
a hydrate forming step of preparing a precursor hydrate for a blue phosphor by mixing the mixed solution with an application of ultrasonic wave and O2-(O3-)bubbling;
a baking step of drying the hydrate and then baking the hydrate in an air at temperatures ranging from 800 to 1350° C.;
a baking step of baking the hydrate in a reducing atmosphere at temperatures ranging from 1000 to 1400° C.