# US 2004/0080080 A1 · Reaction injection and compression molding of a golf ball

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0080080 A1
- Document ID: US20040080080A1
- Status: Published application
- Kind: A1
- Application number: 10/278,525
- Filed: 2002-10-23
- Published: 2004-04-29
- Earliest claimed: 2002-10-23
- Assignees: Acushnet Company
- Inventors: Jeffrey L. Dalton; Christopher Cavallaro
- Web page: https://patentgrep.com/patent/US20040080080A1

## CPC

- B29C 45/14073: {using means being retractable during injection}
- B29C 45/561: {Injection-compression moulding}
- B29C 67/246: {Moulding high reactive monomers or prepolymers, e.g. by reaction injection moulding [RIM], liquid injection moulding [LIM] (casting monomers B29C39/006, mixing construction B29B7/74)}
- B29C 2045/563: {Enlarging the mould cavity during injection}
- B29L 2031/545: {Football balls}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A method of molding a layer of a thermoset or thermoplastic material around a golf ball component within a mold, in which the component is positioned within a mold cavity defined by opposing mold portions of the mold, to leave a cavity space between the component and the mold portions. A reaction mixture comprising at least two reactants is injected under a hydraulic pressure into the cavity space. The pressurized reaction mixture pushes the mold portions apart from each other to a partially open position with an opening therebetween. The reaction mixture is allowed to react partially within the cavity space, and then the mold portions are compressed toward each other to the closed position. The reaction mixture further reacts to form the layer of the thermoset or thermoplastic material immediately about the component.

## Claims

### Claim 1

A method of molding a layer of a thermoset or thermoplastic material around a golf ball component within a mold, comprising:
placing the golf ball component within a mold cavity defined by opposing mold potions of the mold to leave a cavity space between the component and the mold portions;
holding the opposing mold portions together in a closed position;
providing a pre-mixed reaction mixture that comprises at least two reactants;
injecting the reaction mixture under a hydraulic pressure into the cavity space;
moving the mold portions by the hydraulic pressure apart from each other to a partially open position with an opening therebetween;
allowing the reaction mixture to react partially within the cavity space;
compressing the mold portions toward each other to the closed position; and
allowing the reaction mixture to further react to form the layer of the thermoset or thermoplastic material immediately about the component.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
holding the component with support members to be substantially concentric to the mold cavity during the injecting of the reaction mixture; and
removing the support members after a sufficient amount of the mixture has been injected to maintain the component substantially in the predetermined position.

### Claim 3 (depends on 2)

The method of claim 2, wherein the support members comprise retractable pins.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
providing a first tonnage sufficient to hold the mold portions in the closed position; and
allowing the hydraulic pressure to overcome the first tonnage and move the mold portions to the partially open position.

### Claim 5 (depends on 4)

The method of claim 4, further comprising providing a second tonnage sufficient to overcome the hydraulic pressure and compress the mold portions to the closed position, wherein the second tonnage is at least about 20 percent greater than the first tonnage.

### Claim 6 (depends on 1)

The method of claim 1, further comprising removing the hydraulic pressure to allow the compressing the mold portions.

### Claim 7 (depends on 1)

The method of claim 1, wherein the at least two reactants comprises an isocyanate and a polyol or polyamine.

### Claim 8 (depends on 1)

The method of claim 1, wherein the reaction mixture further comprises at least one additive comprising curing agents, crosslinking agents, catalysts, fillers, accelerators, processing aids, processing oils, plasticizers, foaming agents, colorants, or radical quenchers.

### Claim 9 (depends on 1)

The method of claim 1, wherein the layer has a thickness of less than about 0.03 inches.

### Claim 10 (depends on 1)

The method of claim 1, wherein the layer has a thickness of from about 0.0005 inches to about 0.02 inches.

### Claim 11 (depends on 1)

The method of claim 1, wherein the opening between the mold portions in the partially open position is at least about 0.001 inches.

### Claim 12 (depends on 1)

The method of claim 1, further comprising:
heating the reactants to a temperature between about 90° F. and about 150° F.;
mixing the reactants in a mix head through a process comprising impingement or mechanical mixing to form the reaction mixture; and
cooling the thermosetting material formed from the reaction mixture to a temperature below the freezing point of the thermosetting material after the compressing the mold portions.

### Claim 13 (depends on 1)

The method of claim 1, wherein the component has a surface area, and the layer covers from about 10% to about 100% of the surface area of the component.

### Claim 14 (depends on 1)

The method of claim 1, wherein the layer comprises a continuous spherical lattice network.

### Claim 15 (depends on 16)

The method of claim 16, wherein the spherical lattice network comprises octahedron, cubactahedron, icosahedron, or icosadodecadron.

### Claim 16 (depends on 1)

The method of claim 1, wherein the layer is a discontinuous layer comprising a plurality of discrete circular, triangular, or hexagonal elements.

### Claim 17

A method of molding a layer of a thermoset or thermoplastic material around a golf ball component within a mold, comprising:
placing the golf ball component within a mold cavity defined by opposing mold potions of the mold to leave a cavity space between the component and the mold portions substantially surrounding the component;
holding the opposing mold portions apart with an opening therebetween in a partially open position;
providing a pre-mixed reaction mixture that comprises at least two reactants;
injecting the mixture under the hydraulic pressure into the cavity space;
allowing the reaction mixture to partially react within the cavity space;
compressing the mold portions toward each other to a closed position; and
allowing the reaction mixture to further react to form the layer of the thermoset or thermoplastic material to substantially encapsulate the component.

### Claim 18 (depends on 17)

The method of claim 17, wherein the compressing of the mold portions begins after at least about 80 percent of the cavity space is injected with the reaction mixture.

### Claim 19 (depends on 17)

The method of claim 17, wherein the reaction mixture is injected into the cavity space at a plurality of locations.

### Claim 20 (depends on 17)

The method of claim 17, further comprising providing a tonnage sufficient to compress the mold portions to the closed position.

### Claim 21 (depends on 17)

The method of claim 17, wherein the at least two reactants comprises an isocyanate and a polyol or polyamine.

### Claim 22 (depends on 17)

The method of claim 17, wherein the layer has a thickness of from about 0.0005 inches to about 0.02 inches.

### Claim 23 (depends on 17)

The method of claim 17, wherein the layer is continuous or discontinuous.

### Claim 24 (depends on 17)

The method of claim 17, wherein the opening between the mold portions in the partially open position is at least about 0.001 inches.

### Claim 25

A method of molding a layer of a thermoset or thermoplastic material around a golf ball component within a mold, comprising:
placing the golf ball component on a support member within a mold cavity defined by opposing mold potions of the mold to leave a cavity space between the component and the mold portions substantially surrounding the component;
providing a pre-mixed reaction mixture that comprises at least two reactants;
injecting the mixture under the hydraulic pressure into the cavity space through an opening of at least about 0.001 inches between the mold portions in a partially open position;
filling at least about 80% of the cavity space with the mixture in the partially open position;
allowing the reaction mixture to partially react within the cavity space;
compressing the mold portions toward each other under a tonnage to a closed position; and
allowing the reaction mixture to further react to form the layer of the thermoset or thermoplastic material no greater than about 0.03 inches in thickness to substantially encapsulate the component.