# US 2004/0080071 A1 · Thermoplastic composite decking profile of continuous fiber reinforcement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0080071 A1
- Document ID: US20040080071A1
- Status: Published application
- Kind: A1
- Application number: 10/281,796
- Filed: 2002-10-28
- Published: 2004-04-29
- Earliest claimed: 2002-10-28
- Inventors: Byeong H. Jo; John B. Peavey
- Web page: https://patentgrep.com/patent/US20040080071A1

## CPC

- B29C 70/50: for producing articles of indefinite length, e.g. prepregs, sheet moulding compounds [SMC] or cross moulding compounds [XMC]
- B29C 48/12: Articles with an irregular circumference when viewed in cross-section, e.g. window profiles
- B29C 48/07: Flat, e.g. panels
- B29C 48/13: Articles with a cross-section varying in the longitudinal direction, e.g. corrugated pipes
- B29C 48/15: incorporating preformed parts or layers, e.g. extrusion moulding around inserts
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

The present invention relates to a process for providing a consolidated form of the commingled continuous filaments of glass fibers and polymeric fibers as reinforcement. The consolidation of the commingled fibers into composite reinforcement can be used in a continuous form or bulk molding compound pellets. The consolidation of the commingled fibers into composite reinforcement can be made in-situ during in-line extrusion of the final end product extrudate, or prepared as a tape or rod and incorporated into an off-line extrusion of final product. The bulk molding pellets are used solely or diluted with an addition of polymeric material for mono or co-extrusion or compression molding.

## Claims

### Claim 1

A process for providing a thermoplastic composite decking profile of continuous fiber reinforcement, which comprises including within said thermoplastic composite decking profile a polymer composite decking material, said polymer composite decking material comprising a commingled, continuous filament of glass fibers and polymeric fibers as reinforcement, wherein the polymeric fiber that becomes a consolidation matrix is a fiberizable polymer selected from the group consisting of polyethylene, polypropylene and polyesters.

### Claim 2 (depends on 1)

The process as recited in claim 1, wherein the consolidation of the commingled fibers into composite reinforcement is made in-situ during in-line extrusion or pultrusion of the final end product.

### Claim 3 (depends on 1)

The process as recited in claim 1, wherein the consolidation of commingled fibers into composite reinforcement is prepared as a tape or rod, and incorporated into an off-line extrusion of the final product.

### Claim 4 (depends on 1)

The process as recited in claim 1, wherein the commingled, continuous filaments of glass fibers and polymeric fibers are incorporated through a cross-die head into a polymer extrudate.

### Claim 5 (depends on 1)

The process as recited in claim 1, wherein the commingled, continuous filaments contain glass fibers dispersed uniformly in a longitudinal direction during extrusion or pultrusion.

### Claim 6 (depends on 1)

The process as recited in claim 1, wherein the commingled, continuous filaments of glass fibers and polymeric fibers include from about 40%-80% glass fiber content.

### Claim 7 (depends on 1)

The process as recited in claim 1, wherein the commingled, continuous filaments of glass fibers and polymeric fibers further include carbon fibers and/or aramid fibers.

### Claim 8 (depends on 1)

The process as recited in claim 1, wherein a bulk molding compound is made of the commingled, continuous filaments of glass fibers and polymeric fibers.

### Claim 9 (depends on 8)

The process as recited in claim 8, wherein the bulk molding compound made of the commingled, continuous filaments of glass fibers and polymeric fibers is compression molded into building products.

### Claim 10 (depends on 9)

The process as recited in claim 9, wherein the building products are selected from the group consisting of fence, rail, post and deck materials.

### Claim 11 (depends on 5)

The process as recited in claim 5, wherein the commingled, continuous filaments are added through a helical winding machine.

### Claim 12 (depends on 8)

The process as recited in claim 8, wherein the bulk molding compound includes from about 20%-80% glass fiber content, or is diluted with an addition of polymeric pellets to a glass fiber content of 10%-20% in the final product.

### Claim 13 (depends on 8)

The process as recited in claim 8, wherein the thermal expansion and contraction is controlled by the use of the bulk molding compound.