# US 2004/0080049 A1 · Solder terminal and fabricating method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0080049 A1
- Document ID: US20040080049A1
- Status: Published application
- Kind: A1
- Application number: 10/279,383
- Filed: 2002-10-23
- Published: 2004-04-29
- Earliest claimed: 2002-10-23
- Assignees: CCUBE Digital Co., Ltd.
- Inventors: Jong-Heon Kim
- Web page: https://patentgrep.com/patent/US20040080049A1

## CPC

- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/019: {of bond pads}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/01255: {by using masks}
- H10W 72/01257: {by reflowing}
- H10W 72/251: {Materials}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 74/15: on active surfaces of flip-chip devices, e.g. underfills
- H10W 90/724: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 95/00: Packaging processes not covered by the other groups of this subclass
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A solder terminal and a fabrication method thereof are provided. According to one embodiment of the present invention, a solder terminal structure includes an adhesion metal layer formed on an electrode pad of a semiconductor device, a thermal diffusion barrier, a solder bonding layer, and a solder bump formed on upper portion of the solder bonding layer. With the thermal diffusion layer, the characteristic deterioration caused by the probe mark generated on the electrode pad can be prevented during a semiconductor reliability test, and at the same time, material movement between the layers of the electrode pad, the solder bonding layer and the adhesion metal layer can be reduced. Also, by having the thermal diffusion barrier act as a solder dam (a layer to confine the melted solder area to prevent the solder from being wetted), an additional deposition or etching process can be omitted.

## Claims

### Claim 1

A solder terminal structure, comprising:
a plurality of electrode pads exposed through an insulating layer on a surface of a semiconductor device chip;
an adhesion metal layer formed on the electrode pads and on the insulating layer adjacent to the electrode pad;
a thermal diffusion barrier formed on the adhesion metal layer;
a solder bonding layer formed on the thermal diffusion barrier; and
a solder bump formed on the solder bonding layer,
wherein the thermal diffusion barrier does not substantially reach with either the electrode pad or the solder bump during a solder reflow process or a high-temperature semiconductor reliability test.

### Claim 2 (depends on 1)

The structure of claim 1, wherein the thermal diffusion barrier prevents interdiffusion between the solder bonding layer and the electrode pads, and between the adhesion metal layer and the solder bonding layer at the temperature of about 50-350 C.

### Claim 3 (depends on 1)

The structure of claim 1, wherein the thermal diffusion barrier is also a wetting barrier layer such that the solder bump is not wettable during the solder reflow process or the high temperature reliability test.

### Claim 4 (depends on 1)

The structure of claim 1, wherein the adhesion metal layer comprises Al or Al alloy material.

### Claim 5 (depends on 1)

The structure of claim 1, wherein the thermal diffusion barrier comprises TiW or Ti alloy material.

### Claim 6 (depends on 1)

The structure of claim 1, wherein the solder bonding layer is comprises NiV material or Ni alloy material.

### Claim 7 (depends on 1)

The structure of claim 1, further comprising:
a NiV material or Ni alloy material layer formed on the upper portion of the solder bonding layer.

### Claim 8 (depends on 1)

The structure of claim 1, further comprising:
an oxidation barrier of Au formed on the surface of the solder bonding layer.

### Claim 9

A method for forming a solder terminal structure, the method comprising:
forming an insulating layer on a surface of a semiconductor device chip;
exposing a plurality of electrode pads separated from each other, by etching the insulating layer selectively;
forming an adhesion metal layer, a thermal diffusion barrier and a solder bonding layer in order on the exposed electrode pads and the insulating film;
coating photoresist layer on the solder bonding layer and patterning the photoresist layer by exposing and developing so that the solder bonding layer above each electrode pad is selectively exposed;
plating solder on the exposed solder bonding layer;
removing the patterned photoresist layer and etching the solder bonding layer by using the plated solder as a mask;
forming solder bumps by attaching the plated solder to the solder bonding layer; and
etching the thermal diffusion barrier and the adhesion metal layer using the solder bumps as a mask.

### Claim 10 (depends on 9)

The method of claim 9, wherein the adhesion metal layer is formed of a Al material or Al alloy material of about 100 to 5000 Å thickness.

### Claim 11 (depends on 9)

The method of claim 9, wherein the thermal diffusion barrier is formed of a TiW material or Ti alloy material of about 100 to 5000 Å thickness.

### Claim 12 (depends on 9)

The method of claim 9, wherein the solder bonding layer is formed of a NiV material or Ni alloy material of about 100 to 5000 Å thickness.

### Claim 13 (depends on 9)

The method of claim 9, further comprising:
forming a NiV material or Ni alloy material layer having a thickness of 1˜5 μm through an electrolytic or non-electrolytic plating method on the upper portion of the solder bonding layer exposed selectively by the photoresist layer.

### Claim 14 (depends on 9)

The method of claim 9, further comprising:
before plating the solder, forming an oxidation barrier of Au material on the surface of the solder bonding layer selectively exposed by the photoresist layer.

### Claim 15

A fabrication method of a solder terminal structure, the method comprising:
forming an insulating layer on a semiconductor device chip;
exposing a plurality of electrode pads separated from each other, by etching the insulating layer selectively;
forming an adhesion metal layer, a thermal diffusion barrier and a solder bonding layer in order on the exposed electrode pads and insulating film;
coating a photoresist layer on the solder bonding layer;
patterning the photoresist layer by exposing and developing so that photoresist layer remains behind only at the upper portion of the solder bonding layer selectively;
etching the solder bonding layer using the residual photoresist layer as a mask;
removing the residual photoresist layer;
forming a first mask so that the exposed solder bonding layer is exposed selectively therethrough;
coating a solder paste on the upper portion of the solder bonding layer exposed selectively by the first mask using a blade;
removing the first mask,
forming solder bumps by attaching the solder paste to the solder bonding layer; and
etching the thermal diffusion barrier and adhesion metal layer using the solder bump as a mask.

### Claim 16 (depends on 15)

The method of claim 15, wherein the first mask is formed by a stencil mask.

### Claim 17

A solder terminal structure, comprising:
a plurality of electrode pads exposed through an insulating layer on a surface of a semiconductor device chip;
an Al adhesion metal layer formed on the electrode pads and on the insulating layer adjacent the electrode pad;
a thermal diffusion barrier formed on each adhesion metal layer, the thermal diffusion layer formed of TiW or Ti alloy;
a solder bonding layer formed on the thermal diffusion barrier; and
a solder bump attached to the solder bonding layer, wherein the thermal diffusion barrier does not substantially reach with either the electrode pads or the solder bump during a solder reflow process or a high-temperature semiconductor reliability test.

### Claim 18 (depends on 16)

The structure of claim 16, wherein the solder bonding layer is formed of NiV material or Ni alloy material.

### Claim 19 (depends on 18)

The structure of claim 18, further comprising:
a NiV material or Ni alloy material layer formed on the upper portion of the solder bonding layer.

### Claim 20 (depends on 19)

The structure of claim 19, further comprising:
an oxidation barrier of Au material formed on the solder bonding layer.