# US 2004/0079964 A1 · Semiconductor element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079964 A1
- Document ID: US20040079964A1
- Status: Published application
- Kind: A1
- Application number: 10/690,290
- Filed: 2003-10-21
- Published: 2004-04-29
- Earliest claimed: 2000-12-07
- Assignees: NGK Insulators, Ltd.
- Inventors: Yuji Hori; Tomohiko Shibata; Osamu Oda; Mitsuhiro Tanaka
- Web page: https://patentgrep.com/patent/US20040079964A1

## CPC

- H10D 10/021: {of heterojunction BJTs [HBT]}
- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/061: {of FETs having Schottky gates (H10D30/015 takes precedence)}
- H10D 30/0614: {using processes wherein the final gate is made after the completion of the source and drain regions, e.g. gate-last processes using dummy gates}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2901: {Materials}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10D 62/8503: {Nitride Group III-V materials, e.g. AlN or GaN}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

An AlN film as an underlayer is epitaxially grown on a substrate having a dislocation density of 1011/cm2 or below and a crystallinity of 90 seconds or below in full width at half maximum (FWHM) of an X-ray rocking curve at (002) reflection. Then, on the AlN film an n-GaN film is epitaxially grown as a conductive layer having a dislocation density of 1010/cm2 or below and a crystallinity of 150 seconds or below in full width at half maximum (FWHM) of an X-ray rocking curve at (002) reflection, to fabricate a semiconductor element.

## Claims

### Claim 1

A semiconductor element, substantially comprising:
a substrate,
an underlayer, epitaxially grown on the substrate, made of a first semiconductor nitride including at least one element selected from the group consisting of Al, Ga and In, the dislocation density of the underlayer being set to 1011/cm2 or below, the crystallinity of the underlayer being set to 90 seconds or below in full width at half maximum of X-ray rocking curve at (002) reflection,
a first conductive layer of a first conduction type, epitaxially grown on the underlayer, made of a second semiconductor nitride including at least one element selected from the group consisting of Al, Ga and In, the dislocation of the first conductive layer being set to 1010/cm2 or below, the crystallinity of the first conductive layer being set to 150 seconds or below in full width at half maximum of X-ray rocking curve at (002) reflection,
a second conductive layer of the first conduction type, epitaxially grown on the first conductive layer, made of a third semiconductor nitride including at least one element selected from the group consisting of Al, Ga and In, the dislocation of the second conductive layer being set to 1010/cm2 or below, the crystallinity of the second conductive layer being set to 90 seconds or below in full width at half maximum of X-ray rocking curve at (002) reflection,
a third conductive layer of a second conduction type opposite to the first conduction type, epitaxially grown on the second conductive layer, made of a fourth semiconductor nitride including at least one element selected from the group consisting of Al, Ga and In, the dislocation of the third conductive layer being set to 1010/cm2 or below, the crystallinity of the third conductive layer being set to 150 seconds or below in full width at half maximum of X-ray rocking curve at (002) reflection, and
a fourth conductive layer of the first conduction type, epitaxially grown on the third conductive layer, made of a fifth semiconductor nitride including at least one element selected from the group consisting of Al, Ga and In, the dislocation of the fourth conductive layer being set to 1010/cm2 or below, the crystallinity of the fourth conductive layer being set to 150 seconds or below in full width at half maximum of X-ray rocking curve at (002) reflection.

### Claim 2 (depends on 1)

A semiconductor element as defined in claim 1, wherein the underlayer is formed at 1100° C. or over by a MOCVD method.

### Claim 3 (depends on 2)

A semiconductor element as defined in claim 2, wherein the underlayer is formed at a temperature within 1100-1250° C.

### Claim 4 (depends on 1)

A semiconductor element as defined in claim 1, wherein the substrate is made of a sapphire single crystal having a surface nitride layer on the main surface of the crystal, and the underlayer is formed on the main surface via the surface nitride layer.

### Claim 5 (depends on 1)

A semiconductor element as defined in claim 1, wherein the material composition of the first semiconductor nitride constituting the underlayer is varied continuously or stepwisely from the substrate toward the conductive layer.

### Claim 6 (depends on 1)

A semiconductor element as defined in claim 1, wherein the warp of the semiconductor element is 100 μm or below per 5 cm length.

### Claim 7

A heterojunction bipolar transistor comprising a semiconductor element, an emitter electrode, a collector electrode and a base electrode which are provided on the semiconductor element.