# US 2004/0079940 A1 · Substrate and organic electroluminescence device using the substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079940 A1
- Document ID: US20040079940A1
- Status: Published application
- Kind: A1
- Application number: 10/627,683
- Filed: 2003-07-28
- Published: 2004-04-29
- Earliest claimed: 2002-08-02
- Assignees: Samsung SDI Co., Ltd.
- Inventors: Michael Redecker; Marcus Schaedig; Michael Kubiak
- Web page: https://patentgrep.com/patent/US20040079940A1

## CPC

- H10K 59/122: Pixel-defining structures or layers, e.g. banks
- G03F 7/0035: {Multiple processes, e.g. applying a further resist layer on an already in a previously step, processed pattern or textured surface}
- G03F 7/40: Treatment after imagewise removal, e.g. baking
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A substrate and an organic electroluminescence device employing the substrate are provided. The substrate has at least one non-continuous photo-resist coating layer formed on at least one surface of a supporting substrate and the non-continuous photo-resist coating has a plurality of continuous portions. The continuous portions may have high surface energy areas and low surface energy areas. A second photo-resist coating layer is used to at least temporarily overlap the continuous portion which corresponds to the high surface energy area in order to form the low surface energy area.

## Claims

### Claim 1

A method for manufacturing a substrate, comprising:
depositing a first photo-resist coating material on a supporting substrate;
exposing the first photo-resist coating material using a mask;
developing the first photo-resist coating material to provide a first photo-resist coating layer;
treating with a first treatment the first photo-resist coating layer to adjust a surface energy of the first photo-resist coating layer;
depositing a second photo-resist coating material on at least a portion of the first photo-resist coating layer;
exposing the second photo-resist coating material;
developing the second photo-resist coating material to provide a second photo-resist coating layer, wherein at least a portion of the second photo-resist coating layer overlaps at least a portion of the first photo-resist coating layer;
treating with a second treatment at least one portion of the first photo-resist coating layer; and
removing the second photo-resist coating layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein:
the step of treating with a first treatment comprises treating the first photo-resist coating layer with at least one of an UV-ozone treatment or an oxygen-plasma treatment to provide a high surface energy; and
the step of treating with a second treatment comprises treating at least one portion of the first photo-resist coating layer to reduce a surface energy of the at least one surface.

### Claim 3 (depends on 2)

The method of claim 2, wherein the step of treating with a second treatment comprises treating the at least one portion with a plasma treatment including a fluorine-containing gas mixture.

### Claim 4 (depends on 3)

The method of claim 3, wherein the fluorine-containing gas mixture is at least one of CF4, SF6 and NF3,

### Claim 5 (depends on 1)

The method of claim 1, wherein the first photo-resist coating material is at least one of a Novolak based photo-resist, acrylic lacquer, epoxy lacquer and polyimide lacquer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the second photo-resist coating material is at least one of a Novolak based photo-resist, acrylic lacquer, epoxy lacquer and polyimide lacquer.

### Claim 7 (depends on 2)

The method of claim 2, wherein the step of treating with a second treatment at least one portion of the first photo-resist coating layer comprises treating at least one portion using a plasma treatment including a gas mixture of tetrafluoromethane and oxygen in the volume ratio 4:1 to reduce a surface energy of the at least one portion.

### Claim 8 (depends on 1)

The method of claim 1, wherein the step of removing of the second photo-resist coating layer comprises removing the second photo-resist coating layer using at least one of acetone and tetrahydrofuran acetone.

### Claim 9

A substrate having a non-continuous photo-resist coating layer, an insulating layer and a pixel defining layer formed on at least one surface of a supporting substrate, wherein the non-continuous photo-resist coating layer, insulating layer and pixel defining layer comprises a plurality of continuous portions, and the plurality of continuous portions comprise:
at least one high surface energy area; and
at least one low surface energy area, wherein at least one of a second photo-resist coating layer and a mask is used to at least temporarily overlap the continuous portion corresponding to the at least one high surface energy area in order to form the at least one low surface energy area..

### Claim 10 (depends on 9)

The substrate of claim 9, wherein the high surface energy areas have a surface energy of about 60-70 dyne/cm and the low surface energy areas have a surface energy of about 20-35 dyne/cm.

### Claim 11 (depends on 9)

The substrate of claim 9, wherein the supporting substrate is rigid.

### Claim 12 (depends on 9)

The substrate of claim 9, wherein the supporting substrate is flexible.

### Claim 13 (depends on 9)

The substrate of claim 9, wherein the supporting substrate is made of at least one of glass, plastic and silicon.

### Claim 14 (depends on 9)

The substrate of claim 9, wherein the non-continuous photo-resist coating material is at least one of a Novolak based photo-resist, acrylic lacquer, epoxy lacquer and polyimide lacquer.

### Claim 15

A method for manufacturing an organic electroluminescence device, comprising:
depositing a first photo-resist coating material on a supporting substrate;
exposing and developing the first photo-resist coating material to provide a first photo-resist coating layer;
treating with a first treatment at least one surface of the first photo-resist coating layer to adjust a surface energy of the first photo-resist coating layer;
depositing a second photo-resist coating material on at least a portion of the first photo-resist coating layer;
exposing and developing the second photo-resist coating material to provide a second photo-resist coating layer, wherein at least a portion of the second photo-resist coating layer overlaps at least a portion of the first photo-resist coating layer;
treating with a second treatment at least one portion of the first photo-resist coating layer not overlapped by the second photo-resist layer;
removing the second photo-resist coating layer; and
supplying an ink drop containing an organic layer forming material to the resultant structure to form an organic layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the organic layer forming material is at least one of a conductive polymer and a light-emitting polymer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the conductive polymer is at least one of polyethylene dioxothiophene—polystyrene sulfone acid, polyaniline and a mixture thereof.

### Claim 18 (depends on 16)

The method of claim 16, wherein a surface tension of the conductive polymer is reduced by means of at least one of a surfactant and a lower alcohol.

### Claim 19 (depends on 18)

The method of claim 18, wherein the lower alcohol is at least one of butanol and propanol.

### Claim 20 (depends on 16)

The method of claim 16, wherein the light-emitting polymer is at least one of polyphenylenvinylenes and polyfluorenes.

### Claim 21 (depends on 15)

The method of claim 15, wherein the organic layer is a light-emitting portion of the electroluminescence device.

### Claim 22 (depends on 15)

The method of claim 15, wherein:
the step of treating with a first treatment comprises:
treating the first photo-resist coating layer with at least one of an UV-ozone treatment or an oxygen-plasma treatment to provide a high surface energy, and
the step of treating with a second treatment comprises:
treating at least one portion of the first photo-resist coating layer to reduce a surface energy of the at least one portion.

### Claim 23 (depends on 15)

The method of claim 15, wherein the step of treating with a second treatment comprises treating the at least one portion with a plasma treatment including a fluorine-containing gas mixture.

### Claim 24 (depends on 23)

The method of claim 23, wherein the fluorine-containing gas mixture is at least one of CF4, SF6 and NF3,

### Claim 25 (depends on 15)

The method of claim 15, wherein the first photo-resist coating material is at least one of a Novolak based photo-resist, acrylic lacquer, epoxy lacquer and polyimide lacquer.

### Claim 26 (depends on 15)

The method of claim 15, wherein the second photo-resist coating material is at least one of a Novolak based photo-resist, acrylic lacquer, epoxy lacquer and polyimide lacquer.

### Claim 27 (depends on 15)

The method of claim 15, wherein the step of treating with a second treatment at least one portion of the first photo-resist coating layer comprises treating the at least one portion using a plasma treatment including a gas mixture of tetrafluoromethane and oxygen in the volume ratio 4:1 to reduce a surface energy of the at least one portion.

### Claim 28 (depends on 15)

The method of claim 15, wherein the step of removing the second photo-resist coating layer comprises removing the second photo-resist coating layer using at least one of acetone and tetrahydrofuran.

### Claim 29 (depends on 15)

The method of claim 15, wherein the organic layer is formed by at least one of imprinting a conductive polymer and imprinting a solution of a light-emitting polymer using inkjet printing.

### Claim 30 (depends on 15)

An organic electroluminescence device manufactured by the method according to claim 15.

### Claim 31

An organic electroluminescence device, comprising:
a pixel define layer (PDL), wherein the PDL defines at least one area of the organic electroluminescence device with a high surface energy and at least one area of the organic electroluminescence device with a low surface energy.

### Claim 32 (depends on 31)

The organic electroluminescence device according to claim 31, wherein a surface energy of an area of the organic electroluminescence device where the PDL is not formed is either high or low.

### Claim 33 (depends on 31)

The organic electroluminescence device according to claim 31, wherein at least one layer is provided on the PDL, and a surface of the layer includes at least one area with a high surface energy and at least one area with a low surface energy.

### Claim 33 (depends on 31)

The organic electroluminescence device according to claim 31, wherein the PDL is a photo-resist coating layer.

### Claim 34

A method for manufacturing a substrate, comprising:
depositing at least one of a first insulating layer and a first pixel defining layer on a supporting substrate; and
treating at least a first portion of at least one of the first insulating layer and the first pixel defining layer; and
treating a second portion of the first portion of at least one of the first insulating layer and the first pixel defining layer.

### Claim 35 (depends on 34)

The method of claim 34, wherein a third portion of at least one of the first insulating layer and the first pixel defining layer is treated with the first treatment and the second treatment.

### Claim 36 (depends on 34)

The method of claim 34, further comprising depositing at least one of a second insulating layer and a second pixel defining layer on at least a portion of at least one of the first insulating layer and the first pixel defining layer.

### Claim 37 (depends on 34)

The method of claim 34, wherein:
the step of treating at least a first portion, comprises treating with at least one of an UV-ozone treatment or an oxygen-plasma treatment to provide a high surface energy; and
the step of treating a second portion, comprises treating with a fluorine gas mixture.

### Claim 38 (depends on 34)

The method of claim 34, wherein:
the step of treating at least a first portion, comprises treating with a fluorine gas mixture; and
the step of treating a second portion, comprises treating with at least one of an UV-ozone treatment or an oxygen-plasma treatment to provide a high surface energy.