# US 2004/0079681 A1 · Recycle process for a metal bearing sludge concentrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079681 A1
- Document ID: US20040079681A1
- Status: Published application
- Kind: A1
- Application number: 10/328,020
- Filed: 2002-12-26
- Published: 2004-04-29
- Earliest claimed: 2001-12-31
- Inventors: Yu Cheng Lin
- Web page: https://patentgrep.com/patent/US20040079681A1

## CPC

- C22B 7/006: {Wet processes}
- C23F 1/46: Regeneration of etching compositions
- C23G 1/36: Regeneration of waste pickling liquors
- C02F 11/00: Treatment of sludge; Devices therefor
- C02F 2101/20: Heavy metals or heavy metal compounds
- C22B 15/00: Obtaining copper
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23G: CLEANING OR DE-GREASING OF METALLIC MATERIAL BY CHEMICAL METHODS OTHER THAN ELECTROLYSIS
- C02F: TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE (separation in general B01D; special arrangements on waterborne vessels of installations for treating water, waste water or sewage, e.g. for producing fresh water, B63J; adding materials to water to prevent corrosion C23F; treating radioactively-contaminated liquids G21F9/04; regeneration of reactants for recirculation into processes, see the relevant places for the processes)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A recycling treatment of heavy metal sludge uses a cracking process which releases macromolecular agglutinant and a metal hydrate mixture. Next the mixture is acidified in a primary homogenization process and then a primary separation process separates the macromolecular agglutinant and acid solution with metal ions. A second homogenization process adjusts the pH value of the acid solution with metal ions to be alkaline and then a second separation process separates copper oxide and the remaining salt solution with oxidant. Lastly, salt compounds and oxidant solution is separated through the use of a crystal separation process.

## Claims

### Claim 1

A recycling treatment of heavy metal sludge which includes:
The cracking process, in which the sludge is mixed with a sulphuric acid solution and peroxide proportional to the sludge in weight and treated under high temperature and normal pressure,
After a certain period of reaction, macromolecular agglutinant and a metal hydrate mixture are released;
The primary homogenization process, which adjusts the pH value of the mixture after the cracking process to be acidic;
The primary separation process, which mixes the acid mixture from the primary homogenization process to separate macromolecular agglutinant and acid solution with metal ions;
The second homogenization process, which adjusts the pH value of the acid solution with metal ions to be alkaline;
The second separation process, which separates copper oxide and the remaining salt solution with oxidant after second homogenization; and
The crystal separation process, which treats the remaining acid exhausted liquid after second separation to filter out salt compounds and oxidant solution.

### Claim 2 (depends on 1)

For the cracking process mentioned in claim 1 of the heavy metal sludge recycling treatment, the weight ratio of peroxide and sludge is 0.5-2 to 40-50.

### Claim 3 (depends on 1)

The peroxide used in the cracking process mentioned in claim 1 of the heavy metal sludge recycling treatment can be hydrogen peroxide, dibutyl peroxide, dicumyl peroxide, (tertbutyl peroxide) hexene, (tertbutyl peroxide) hexane.

### Claim 4 (depends on 1)

The primary homogenization process mentioned in claim 1 uses one or more acid solution including sulphuric acid, hydrochloric acid, nitric acid and micro etching exhausted liquid to change the pH value.

### Claim 5 (depends on 1)

The secondary homogenization process mentioned in claim 1 uses one or more alkaline solution including sodium hydroxide, lime, ammonia and etching exhausted liquid to change the pH value.

### Claim 6 (depends on 1)

The temperature used in the cracking process mentioned in claim 1 is between 200° C. and 250° C.

### Claim 7 (depends on 1)

The time needed for the process of cracking mentioned in claim 1 is three to six hours.

### Claim 8 (depends on 1)

The best pH value for primary homogenization process mentioned in claim 1 should be 2 to 7.

### Claim 9 (depends on 1)

The best pH value for secondary homogenization process mentioned in claim 1 should be 7 to 10.

### Claim 10 (depends on 1)

The products of the crystal separation process mentioned in claim 1 include: sodium sulphate, ammiaonia sulfate, sodium chloride, sodium chloride, sodium nitrate, ammonium nitrate, calcium sulphate and calcium chloride.

### Claim 11 (depends on 1)

The digesting process mentioned in claim 1 is used to mix either the existing micro etching exhausted liquid from a printed circuit board factory or any normal acid with the sludge mixture in the process of cracking.

### Claim 12 (depends on 1)

The digesting process mentioned in claim 1 can further use the hydrate treated in primary separation or the hydrate can be used in the primary homogenization and/or secondary homogenization to be mixed with the sludge mixture.

### Claim 13 (depends on 1)

The copper oxide produced in the process as described in claim 1 contains a copper content of 30-50% of its weight.

### Claim 14 (depends on 1)

For the macromolecular agglutinant mentioned in claim 1 in the patent application, the content of macromolecule is 20-40% in weight.

### Claim 15 (depends on 1)

For the oxidant solution mentioned in claim 1 in the patent application, the oxidizing ability can reach the standard of sewage discharge of COD 200 to 500 ppm after adding 3.0-9.0 permillage in weight.