# US 2004/0079478 A1 · Adhesives for vehicle body manufacturing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079478 A1
- Document ID: US20040079478A1
- Status: Published application
- Kind: A1
- Application number: 10/661,499
- Filed: 2003-09-15
- Published: 2004-04-29
- Earliest claimed: 2000-11-06
- Assignees: Sika AG, vorm. Kaspar Winkler & Co.
- Inventors: Peter W. Merz
- Web page: https://patentgrep.com/patent/US20040079478A1

## CPC

- C09J 5/00: Adhesive processes in general; Adhesive processes not provided for elsewhere, e.g. relating to primers
- B60R 13/06: Sealing strips (sealing arrangements for vehicle windows, windscreens, non-fixed roofs, doors, or similar devices B60J10/00)
- B62D 27/026: {Connections by glue bonding (in general F16B11/00; processes C09J5/00)}
- C09J 5/06: involving heating of the applied adhesive
- C09J 9/00: Adhesives characterised by their physical nature or the effects produced, e.g. glue sticks (C09J7/00 takes precedence)
- C09J 2400/163: in the substrate
- Y10T 156/1034: Overedge bending of lamina about edges of sheetlike base
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B60R: VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISE PROVIDED FOR
- B62D: MOTOR VEHICLES; TRAILERS (steering, or guiding on a desired track, of agricultural machines or implements A01B69/00; wheels, castors, axles, increasing wheel adhesion B60B; vehicle tyres, tyre inflation or tyre changing B60C; connections between vehicles of a train or the like B60D; vehicles for use on rail and road, amphibious or convertible vehicles B60F; suspension arrangements B60G; heating, cooling, ventilating or other air treating devices B60H; windows, windscreens, non-fixed roofs, doors or similar devices, protective coverings for vehicles not in use B60J; propulsion plant arrangements, auxiliary drives, transmissions, controls, instrumentation or dashboards B60K; electric equipment or propulsion of electrically-propelled vehicles B60L; power supply for electrically-propelled vehicles B60M; passenger accommodation not otherwise provided for B60N; adaptations for load transportation or to carry special loads or objects B60P; arrangement of signalling or lighting devices, the mounting or supporting thereof or circuits therefor, for vehicles in general B60Q; vehicles, vehicle fittings or vehicle parts not otherwise provided for B60R; servicing, cleaning, repairing, supporting, lifting, or manoeuvring, not otherwise provided for, B60S; brake arrangements, brake control systems or parts thereof B60T; air-cushion vehicles B60V; motor-cycles, accessories therefor B62J, B62K; testing of vehicles G01M)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Two-component systems are described which are suitable for underlining, adhesive bonding of the crimped fold and sealing of auto body sections, particularly for crimped fold sealing of add-on vehicle parts. The two-component systems attain the requisite grip strength for mounting the add-on parts on the body as well as the requisite strength and dimensional stability for the production process up to and with the CIP passage, within the predetermined cycle time, on the basis of cross-linking of the sealant composition twice. In one embodiment, the surface of the two-component system is pre-cross-linked by a UV-induced reaction and by the cross-linking of the two-component system to the extent of portability. In addition, two-component systems are described which cross-link intentionally only partially up to a consistency that permits a rugged course of the process through cleaning baths and which harden completely only by means of a further hardening process, for instance in the CIP forced circulation oven.

## Claims

### Claim 1

A two-component system having one resin component and one hardener component, wherein hardening is effected in that the system cross-links by means of at least two non-identical hardening processes, one hardening process being a reaction proceeding at room temperature between at least one resin and at least one hardener, and at least a further cross-linking system is present which cross-links by means of a hardening process in which the active ingredients of the cross-linking system react by means of a photochemical and/or thermally activatable reaction, and the active ingredients of the cross-linking system which hardens by means of photochemical reaction contain a resin which may be reacted by means of a photoactivator and contain a photo-inducible photoactivator, and the active ingredients of the cross-linking system that hardens by thermal activation contain a resin which may be reacted by means of a thermoactivator and a thermo-inducible thermoactivator.

### Claim 2 (depends on 1)

The two-component system of claim 1, wherein, in addition, a hardening process by means of moisture takes place.

### Claim 3 (depends on 1)

The two-component system of claim 1, wherein the hardening is effected in at least two stages, and at least the first stage leads to only partial cross-linking.

### Claim 4 (depends on 3)

The two-component system of claim 3, wherein, as a result of the partial cross-linking, a consistency or strength results which makes a rugged process in auto body construction possible up to and with a CIP passage.

### Claim 5 (depends on 1)

The two-component system of claim 1, wherein it has a pot life of at least 30 minutes.

### Claim 6 (depends on 1)

The two-component system of claim 1, wherein the two-component reaction is not set into motion until by a brief thermal heating.

### Claim 7 (depends on 1)

The two-component system of claim 1, wherein the active ingredients of the one hardening process include or comprise compounds which can react with at least one active ingredient of at least one other hardening process and/or water, and substances reacting with one another at room temperature without activation are packed in different components of the two-component system.

### Claim 8 (depends on 1)

The two-component system of claim 1, wherein one of the hardening processes is a photochemical reaction.

### Claim 9

A method for sealing an auto body section by application of a sealant composition to the body section to be sealed, followed by a multi-step hardening of the sealant composition, said method comprising:
(a) preparing a sealant composition comprising at least one resin and at least one hardener;
(b) applying the sealant composition to said body section at room temperature to initiate hardening of the sealant composition; and
(c) cross-linking the sealant composition by a photochemical and/or thermally activatable reaction; wherein the active ingredients of the cross-linking system which hardens by means of photochemical reaction include a resin which reacts by means of a photoactivator and a photo-inducible photoactivator, and the active ingredients of the cross-linking system that hardens by thermal activation include a resin which reacts by means of a thermoactivator and a thermo-inducible thermoactivator.

### Claim 10 (depends on 9)

The method for sealing an auto body portion according to claim 9, wherein before passing through a CIP oven, the system is at least partially cured by means of thermal induction and/or a photoinduced hardening process.

### Claim 11

A method for crimp fold sealing a metal auto body section by application of a sealant composition to a body section to be sealed, followed by hardening of the sealant composition, wherein the sealant composition comprises at least one resin and at least one hardener, and the hardening is effected by means of at least two non-identical hardening processes, one of the hardening processes including a room temperature hardening and at least one further hardening step including a photochemical and/or thermally activatable hardening.

### Claim 12 (depends on 11)

The method of claim 11, wherein one hardening process is a photochemical hardening.

### Claim 13 (depends on 9)

The method of claim 9, wherein the photochemical hardening and/or thermally activatable hardening is performed before a coating or wetting of the body section.

### Claim 14 (depends on 11)

The method of claim 11, wherein partial hardening is performed before painting of the body section.

### Claim 15 (depends on 11)

The method of claim 11, wherein the sealant composition is hardened by means of two non-identical hardening processes, which are performed before coating or wetting of the body section.

### Claim 16 (depends on 11)

The method of claim 11, wherein one of the hardening processes comprises a photochemical reaction which primarily hardens the outer surface of the sealant, and the at least one other hardening process comprises a reaction which hardens either a contact region of the sealant with the body section, or internal regions of the sealant.

### Claim 17 (depends on 11)

The method of claim 11, wherein one hardening process is a thermal hardening by partial heating of the adhesive and/or, at least in a first stage, is effected without an oven.

### Claim 18 (depends on 11)

The method of claim 11, wherein the non-identical hardening processes are performed at a time interval between them of less than 2 hours.

### Claim 19 (depends on 18)

The method of claim 18, wherein the hardening processes are performed in a time interval between them of less than 1 hours.

### Claim 20 (depends on 11)

The method of claim 11, wherein the hardening processes are selected from oven hardening, inductive hardening, hardening by a hot-air blower, photochemical cross-linking, reactive rehardening without a special energy supply, or combinations thereof.

### Claim 21 (depends on 11)

The method of claim 11, wherein the hardening processes effect at least a partial hardening and are performed to at least a surface hardness of the sealant composition that is sufficient for touchability or grip strength for manual handling, and/or up to a leaching resistance in circulating cleaning baths at a temperature of up to 70° C. for degreasing oily auto body parts, phosphating, and/or electronic immersion painting and/or an outdoor exposure time under tropical climatic conditions of more than three weeks.

### Claim 22 (depends on 11)

The method of claim 11, wherein partial hardening of at least one of the non-identical hardening processes is effected until the sealant has a strength at least such that in the further course of the process, sacrifices in terms of appearance from air inclusions between the adhesive and the sealant are reduced.

### Claim 23 (depends on 11)

The method of claim 11, wherein, in the basic body in white phase, a crimped fold sealant is prepared which is partially hardened with UV radiation and thermally together with adhesive bonding of the crimped fold in such a way that add-on parts thus produced can be transported and after passing through at least one cleaning bath and one painting operation, can be completely thermally hardened in an oven together with painting.

### Claim 24 (depends on 2)

The two-component system of claim 2, wherein the hardening is effected in at least two stages, and at least the first stage leads to only partial cross-linking.

### Claim 25 (depends on 24)

The two-component system of claim 24, wherein, as a result of the partial cross-linking, a consistency or strength results which makes a rugged process in auto body construction possible up to and with a CIP passage.

### Claim 26 (depends on 6)

The two-component system of claim 6, wherein the brief thermal heating is in the range 50-150° C.

### Claim 27 (depends on 12)

The method of claim 12, wherein photochemical hardening and/or at least one stage of a thermal hardening is performed before coating or wetting of the body section.

### Claim 28 (depends on 13)

The method of claim 13, wherein the thermal hardening performed before a different kind of coating or wetting of the body section is performed before degreasing and/or painting.

### Claim 29 (depends on 27)

The method of claim 27, wherein the thermal hardening performed before coating or wetting of the body section is performed before degreasing and/or painting.

### Claim 30 (depends on 15)

The method of claim 15, wherein the hardening performed before coating or wetting of the body section is performed before painting.

### Claim 31 (depends on 16)

The method of claim 16, wherein one of the hardening processes is a photochemical reaction.

### Claim 32 (depends on 31)

The method of claim 31, wherein another hardening process is a two-component reaction.

### Claim 33 (depends on 17)

The method of claim 17, wherein said heating is effected by inductive heating, IR radiation, and/or a hot-air blower.

### Claim 34 (depends on 22)

The method of claim 22, wherein the sealant strength is in the contact region with the body section.

### Claim 35 (depends on 23)

The method of claim 23, wherein visual or functional sacrifices are not present in the sealant.

### Claim 36 (depends on 11)

The method of claim 11, wherein the hardening processes are selected from oven hardening, inductive hardening, hardening by a hot-air blower, photochemical cross-linking, reactive rehardening without a special energy supply, or combinations thereof.

### Claim 37 (depends on 11)

The method of claim 11, wherein the hardening processes effecting at least a partial hardening are performed to at least a surface hardness of the sealant composition that is sufficient for touchability or grip strength for manual handling, and/or up to a leaching resistance in circulating cleaning baths at a temperature of up to 70° C. for degreasing oily auto body parts, phosphating, and/or electronic immersion painting and/or an outdoor exposure time under tropical climatic conditions of more than three weeks.

### Claim 38 (depends on 11)

The method of claim 11, wherein at least one of the first hardening processes is performed until the sealant has a strength at least such that in the further course of the process, sacrifices in terms of appearance from air inclusions between the adhesive and the sealant are reduced.

### Claim 39 (depends on 11)

The method of claim 11, wherein, in the basic body in white phase, a crimped fold sealant is prepared which is prehardened both with UV rays and thermally together with the adhesive bonding of the crimped fold in such a way that the add-on parts thus produced can be transported and after passing through at least one cleaning bath and one painting operation, can be completely thermally hardened in the oven together with the painting.

### Claim 40 (depends on 38)

The method of claim 38, wherein the sealant strength is in the contact region with the body section.

### Claim 41 (depends on 39)

The method of claim 39, wherein visual or functional sacrifices are not present in the sealant.

### Claim 42 (depends on 9)

The method according to claim 9, wherein the sealant composition is a two-component composition A+B where A comprises a resin containing acrylate groups and/or epoxy groups, a UV initiator and a thermally unstable initiator and B comprises a compound reactable with acrylate and/or epoxy groups, optionally further including a compound containing silane groups.

### Claim 43 (depends on 11)

The method according to claim 11, wherein the sealant composition is a two-component composition A+B where A comprises a resin containing acrylate groups and/or epoxy groups, a UV initiator and a thermally unstable initiator and B comprises a compound reactable with acrylate and/or epoxy groups, optionally further including a compound containing silane groups.