# US 2004/0079468 A1 · Process for producing carpet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079468 A1
- Document ID: US20040079468A1
- Status: Published application
- Kind: A1
- Application number: 10/658,084
- Filed: 2003-09-09
- Published: 2004-04-29
- Earliest claimed: 2002-09-13
- Inventors: Raymond Joseph Reisdorf; Loic Pierre Rolland
- Web page: https://patentgrep.com/patent/US20040079468A1

## CPC

- B32B 27/12: next to a fibrous or filamentary layer
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 37/1027: {Pressing using at least one press band}
- B32B 37/12: characterised by using adhesives
- B32B 37/1207: {Heat-activated adhesive (B32B37/04 takes precedence)}
- D06N 7/0076: {the back coating or pre-coat being a thermoplastic material applied by, e.g. extrusion coating, powder coating or laminating a thermoplastic film}
- D06N 7/0081: {with at least one extra fibrous layer at the backing, e.g. stabilizing fibrous layer, fibrous secondary backing}
- B32B 37/08: characterised by the cooling method
- B32B 37/1036: {Pressing between one press band and a cylinder}
- B32B 37/153: {at least one layer is extruded and immediately laminated while in semi-molten state}
- B32B 37/20: involving the assembly of continuous webs only
- B32B 2305/18: Fabrics, textiles
- B32B 2307/7248: Odour barrier
- B32B 2471/00: Floor coverings (B32B2419/04 takes precedence)
- B32B 2471/02: Carpets
- D06N 2201/0263: Polyamide fibres
- D06N 2201/06: Animal fibres, e.g. hair, wool, silk
- D06N 2203/042: Polyolefin (co)polymers
- D06N 2203/061: Polyesters
- D06N 2213/065: Two back coatings one next to the other
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- D06N: WALL, FLOOR, OR LIKE COVERING MATERIALS, e.g. LINOLEUM, OILCLOTH, ARTIFICIAL LEATHER, ROOFING FELT, CONSISTING OF A FIBROUS WEB COATED WITH A LAYER OF MACROMOLECULAR MATERIAL; FLEXIBLE SHEET MATERIAL NOT OTHERWISE PROVIDED FOR

## Abstract

A process for preparation of a tufted polyamide-type fiber carpet is provided. A primary backing tufted with yarn comprised of at least 85% by weight of fibers selected from the group nylon fibers, wool fibers, and blends thereof is provided. A molten polymer adhesive is provided on the back side of the tufted primary backing, the polymer adhesive consisting of at least 85% by weight of one or more ethylene copolymers each comprised of 50 to 95 weight % of ethylene, and 5-50 weight % of at least one comonomer selected from the group of esters and carboxylic acids. The tufted primary backing and the molten polymer adhesive layer are compressed under a moving belt that applies a pressure of at least 1 N/cm2 for a period of at least 5 seconds during which time the polymer adhesive remains in a molten state. The molten polymer adhesive then cooled to a temperature below the melting point of said molten adhesive. A secondary backing may be placed over the molten polymer adhesive on the back of the primary backing.

## Claims

### Claim 1

A process for preparation of a tufted polyamide-type fiber carpet comprising
providing a primary backing tufted with yarn comprised of at least 85% by weight of fibers selected from the group nylon fibers, wool fibers, and blends thereof, said tufted primary backing having a carpet side and an opposite back side,
providing a molten polymer adhesive on the back side of the tufted primary backing, said polymer adhesive consisting of at least 85% by weight of one or more ethylene copolymers each comprised of 50 to 95 weight % of ethylene, and 5-50 weight % of at least one comonomer selected from the group of esters and carboxylic acids,
compressing said tufted primary backing and said molten polymer adhesive layer under a moving belt that applies a pressure of at least 1 N/cm2 for a period of at least 5 seconds during which time the polymer adhesive remains in a molten state,
cooling said molten polymer adhesive to a temperature below the melting point of said molten adhesive.

### Claim 2 (depends on 1)

The process of claim 1 wherein prior to compressing said tufted primary backing and molten polymer adhesive under a moving belt, a secondary backing is placed over the molten polymer adhesive on the back of the primary backing.

### Claim 3 (depends on 1)

The process of claim 1 further comprising the step of introducing the tufted primary backing with the molten polymer adhesive into a nip and compressing molten polymer adhesive into said tufted primary backing in said nip.

### Claim 4 (depends on 1)

The process of claim 1 wherein compressing said tufted primary backing and said molten polymer adhesive layer under a moving belt comprises compressing tufted primary backing and said molten polymer adhesive layer between a moving belt and a rotating heated drum with an outer heated surface, wherein the heated drum has a diameter of from 1 to 3 meters, the outer heated surface of the drum and the moving belt travel at substantially the same speed in the range of 10 to 30 m/minute, and the surface of the drum is heated to a temperature within the range of 130 to 180° C.

### Claim 5 (depends on 4)

The process of claim 4 wherein the belt presses the primary backing against the heated drum with a pressure of from 2 to 10 N/cm2.

### Claim 6 (depends on 2)

The process of claim 2 wherein compressing said tufted primary backing, said molten polymer adhesive layer, and said secondary backing under a moving belt comprises the step of compressing tufted primary backing, said molten polymer adhesive layer and said secondary backing between two moving belts, wherein the moving belts are heated to a temperature within the range of 130 to 200° C. over a distance of 3 to 10 meters, and wherein the two moving belts travel at substantially the same speed in the range of 10 to 30 m/minute.

### Claim 7 (depends on 6)

The process of claim 6 wherein the two moving belts squeeze the primary backing, the molten polymer adhesive and the secondary backing together under a pressure of from 2 to 10 N/cm2.

### Claim 8 (depends on 1)

The process of claim 1 wherein the extrusion temperature of the molten polymer adhesive is in the range of 150 to 325° C.

### Claim 9 (depends on 2)

The process of claim 2 further comprising the step of introducing a reinforcing grid between the back side of the tufted primary backing and the secondary backing prior to compressing said tufted primary backing, said molten polymer adhesive layer, and said secondary backing in said nip.

### Claim 10 (depends on 1)

The process of claim 1 wherein the comonomer selected from the group of esters and carboxylic acids consists of vinyl acetate, butyl acrylate, methyl acrylate, methacrylic acid, and acrylic acid.

### Claim 11 (depends on 10)

The process of claim 10 wherein the polymer adhesive is a terpolymer containing 50-90 weight % ethylene, 5-20 weight % butyl acrylate, and 5-20 weight % methacrylic acid.

### Claim 12 (depends on 10)

The process of claim 10 wherein at least 20 weight % of the polymer adhesive is a copolymer containing 50-95 weight % ethylene and 5-50 weight % metharcylic acid.

### Claim 13 (depends on 12)

The process of claim 12 wherein at least 20 weight % of the polymer adhesive is a copolymer containing 50-95 weight % ethylene and 5-50 weight % vinyl acetate.

### Claim 14 (depends on 1)

The process of claim 1 wherein the polymer adhesive has a melt index of at least 150 according to ASTM D-1238 @190° C. with a weight of 2.16 Kg.

### Claim 15 (depends on 14)

The process of claim 14 wherein the polymer adhesive has a melt index in the range of 200 to 800 according to ASTM D-1238 @190° C. with a weight of 2.16 Kg.