# US 2004/0079457 A1 · Al-Mg-Si series alloy plate, method for manufacturing the same and Al-Mg-Si series alloy material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079457 A1
- Document ID: US20040079457A1
- Status: Published application
- Kind: A1
- Application number: 10/376,266
- Filed: 2003-03-03
- Published: 2004-04-29
- Earliest claimed: 2002-03-01
- Assignees: Showa Denko K.K.
- Inventors: Kazuo Kimura; Nobuhiko Akagi
- Web page: https://patentgrep.com/patent/US20040079457A1

## CPC

- C22C 21/06: with magnesium as the next major constituent
- C22C 21/02: with silicon as the next major constituent
- C22C 21/08: with silicon
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A method for manufacturing an Al—Mg—Si series alloy plate includes the steps of hot-rolling and subsequently cold-rolling an Al—Mg—Si series alloy ingot. The Al—Mg—Si series alloy ingot consists of Si: 0.2 to 0.8 mass %, Mg: 0.3 to 1 mass %, Fe: 0.5 mass % or less, Cu: 0.5 mass % or less, at least one of elements selected from the group consisting of Ti: 0.1 mass % or less and B: 0.1 mass % or less and the balance being Al and inevitable impurities. Heat-treating for holding a rolled ingot at 200 to 400° C. for 1 hour or more is performed after a completion of the hot-rolling but before a completion of the cold-rolling.

## Claims

### Claim 1

A method for manufacturing an Al—Mg—Si series alloy plate, the method comprising:
hot-rolling and subsequently cold-rolling an Al—Mg—Si series alloy ingot,
wherein said Al—Mg—Si series alloy ingot consists of Si: 0.2 to 0.8 mass %, Mg: 0.3 to 1 mass %, Fe: 0.5 mass % or less, Cu: 0.5 mass % or less, at least one of elements selected from the group consisting of Ti: 0.1 mass % or less and B: 0.1 mass % or less and the balance being Al and inevitable impurities, and
wherein heat-treating for holding a rolled ingot at 200 to 400° C. for 1 hour or more is performed after a completion of said hot-rolling but before a completion of said cold-rolling.

### Claim 2 (depends on 1)

The method for manufacturing an Al—Mg—Si series alloy plate as recited in claim 1, wherein Mn and Cr contained as impurities in said ingot are controlled such that a content of Mn is 0.1 mass % or less and a content of Cr is 0.1 mass % or less.

### Claim 3 (depends on 1, 2)

The method for manufacturing an Al—Mg—Si series alloy plate as recited in claim 1 or 2, wherein said heat-treating is performed after said completion of said hot-rolling but before said cold-rolling.

### Claim 4 (depends on 1, 2)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in claim 1 or 2, wherein said heat-treating is performed during said cold-rolling.

### Claim 5 (depends on 1, 2, 3, 4)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 4, wherein said heat-treating is performed at 220 to 280° C. for 1 to 10 hours.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 5, further comprising homogenization processing of said alloy ingot performed at 500° C. or above.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 6, wherein said cold-rolling after said heat-treating is performed at a reduction ratio of 20% or more.

### Claim 8 (depends on 7)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in claim 7, wherein said reduction ratio is 30% or more.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 8, further comprising final annealing performed at 200° C. or below after said completion of said cold-rolling.

### Claim 10 (depends on 9)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in claim 9, wherein said final annealing is performed at 110 to 150° C.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 10, further comprising preheating said alloy ingot to 450 to 580° C. before performing said hot-rolling.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 11, wherein said hot-rolling includes a plurality of passes, and wherein a material temperature before one of said passes is set to be 450 to 350° C. and a cooling rate after said one of said passes is set to be 50° C./minute or more.

### Claim 13 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Si content of said alloy ingot is 0.32 to 0.6 mass %.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Mg content of said alloy ingot is 0.35 to 0.55 mass %.

### Claim 15 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Fe content of said alloy ingot is 0.1 to 0.25 mass %.

### Claim 16 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Cu content of said alloy ingot is 0.1 mass % or less.

### Claim 17 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Ti content of said alloy ingot is 0.005 to 0.05 mass %.

### Claim 18 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a B content of said alloy ingot is 0.06 mass % or less.

### Claim 19 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Mn content of said alloy ingot is controlled to be 0.05 mass % or less.

### Claim 20 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

The method for manufacturing said Al—Mg—Si series alloy plate as recited in any one of claims 1 to 12, wherein a Cr content of said alloy ingot is controlled to be 0.05 mass % or less.

### Claim 21

An Al—Mg—Si series alloy material consisting of Si: 0.2 to 0.8 mass %, Mg: 0.3 to 1 mass %, Fe: 0.5 mass % or less, Cu: 0.5 mass % or less, at least one of elements selected from the group consisting of Ti: 0.1 mass % or less and B: 0.1 mass %, and the balance being Al and inevitable impurities, wherein electrical conductivity of said alloy material is 55 to 60% (IACS).

### Claim 22 (depends on 21)

The Al—Mg—Si series alloy material as recited in claim 21, wherein tensile strength of said alloy material is 140 to 240 N/mm2.

### Claim 23 (depends on 21, 22)

The Al—Mg—Si series alloy material as recited in claim 21 or 22, wherein Mn and Cr as impurities of said alloy are controlled to be Mn: 0.1 mass % or less and Cr: 0.1 mass % or less.

### Claim 24 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20)

An Al—Mg—Si series alloy plate manufactured by said method as recited in any one of claims 1 to 20.

### Claim 25 (depends on 24)

The Al—Mg—Si series alloy plate as recited in claim 24, wherein said Al—Mg—Si series alloy plate is a member selected from the group consisting of a heat dissipation member, an electrically conductive member, a casing member, a light reflecting member or its supporting member.

### Claim 26 (depends on 24)

The Al—Mg—Si series alloy plate as recited in claim 24, wherein said Al—Mg—Si series alloy plate is a member selected from the group consisting of a plasma display rear surface chassis member, a plasma display box member and a plasma display exterior member.

### Claim 27 (depends on 24)

The Al—Mg—Si series alloy plate as recited in claim 24, wherein said Al—Mg—Si series alloy plate is a member selected from the group consisting of a liquid crystal display rear chassis member, a liquid crystal display bezel member, a liquid crystal display reflecting sheet member, a liquid crystal display reflecting sheet supporting member and a liquid crystal display box material.