# US 2004/0079453 A1 · Nickel-base alloy and its use in casting and welding operations

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079453 A1
- Document ID: US20040079453A1
- Status: Published application
- Kind: A1
- Application number: 10/280,391
- Filed: 2002-10-25
- Published: 2004-04-29
- Earliest claimed: 2002-10-25
- Inventors: Jon Raymond Groh; Michael Joseph Gambone
- Web page: https://patentgrep.com/patent/US20040079453A1

## CPC

- C22C 19/055: {with the maximum Cr content being at least 20% but less than 30%}
- C22C 19/056: {with the maximum Cr content being at least 10% but less than 20%}
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An alloy has a composition of, in weight percent, from about 16 percent to about 21 percent chromium, from about 6 percent to about 12 percent iron, from about 6 percent to about 12 percent cobalt, from about 2.8 percent to about 3.3 percent molybdenum, from about 5 percent to about 5.4 percent niobium, from 0 to about 2 percent tantalum, from about 0.65 percent to about 1.15 percent titanium, from about 0.2 percent to about 0.8 percent aluminum, from about 0.01 percent to about 0.05 percent carbon, from about 0.005 percent to about 0.01 percent boron, less than about 0.1 percent zirconium, balance nickel and impurities. A molten mass of this composition may be cast into a mold for solidification. The solid material may be welded either in a rework/repair process or to join it to a second article.

## Claims

### Claim 1

A composition of matter having a composition consisting essentially of, in weight percent, from about 16 percent to about 21 percent chromium, from about 6 percent to about 12 percent iron, from about 6 percent to about 12 percent cobalt, from about 2.8 percent to about 3.3 percent molybdenum, from about 5 percent to about 5.4 percent niobium, from zero to about 2 percent tantalum, from about 0.65 percent to about 1.15 percent titanium, from about 0.2 percent to about 0.8 percent aluminum, from about 0.01 percent to about 0.05 percent carbon, from about 0.005 percent to about 0.01 percent boron, less than about 0.1 percent zirconium, balance nickel and impurities.

### Claim 2 (depends on 1)

The composition of matter of claim 1, wherein the tantalum content is less than about 1 percent.

### Claim 3 (depends on 1)

The composition of matter of claim 1, wherein the total of iron plus cobalt is from about 17 to about 19 percent.

### Claim 4 (depends on 1)

The composition of matter of claim 1, wherein the iron content is from about 8 percent to about 9.5 percent.

### Claim 5 (depends on 1)

The composition of matter of claim 1, wherein the chromium content is about 18 percent, the iron content is about 9 percent, the cobalt content is about 9 percent, the molybdenum content is about 3 percent, the niobium content is about 5 percent, the tantalum content is less than about 0.01 percent, the titanium content is about 1 percent, the aluminum content is about 0.5 percent, the carbon content is about 0.03 percent, and the boron content is about 0.007 percent.

### Claim 6

A method of providing a cast article, comprising the steps of:
providing a molten mass of metal having a composition consisting essentially of, in weight percent, from about 16 percent to about 21 percent chromium, from about 6 percent to about 12 percent iron, from about 6 percent to about 12 percent cobalt, from about 2.8 percent to about 3.3 percent molybdenum, from about 5 percent to about 5.4 percent niobium, from 0 to about 2 percent tantalum, from about 0.65 percent to about 1.15 percent titanium, from about 0.2 percent to about 0.8 percent aluminum, from about 0.01 percent to about 0.05 percent carbon, from about 0.005 percent to about 0.01 percent boron, less than about 0.1 percent zirconium, balance nickel and impurities; and
casting molten mass of metal into a mold to form the cast article.

### Claim 7 (depends on 6)

The method of claim 6, including an additional step, after the step of casting, of hot isostatic pressing the cast article.

### Claim 8 (depends on 6)

The method of claim 6, including an additional step, after the step of casting, of heat treating the cast article.

### Claim 9 (depends on 6)

The method of claim 6, wherein the step of providing the billet includes the step of providing the billet having an iron content of from about 8 percent to about 9.5 percent.

### Claim 10 (depends on 6)

The method of claim 6, including an additional step, after the step of casting, of placing the cast article into service at a maximum service temperature of at least about 1300° F.

### Claim 11 (depends on 6)

The method of claim 6, including an additional step, after the step of casting, of welding the cast article.

### Claim 12

A method of preparing a welded article, comprising the steps of:
providing a piece of material having a composition consisting essentially of, in weight percent, from about 16 percent to about 21 percent chromium, from about 6 percent to about 12 percent iron, from about 6 percent to about 12 percent cobalt, from about 2.8 percent to about 3.3 percent molybdenum, from about 5 percent to about 5.4 percent niobium, from 0 to about 2 percent tantalum, from about 0.65 percent to about 1.15 percent titanium, from about 0.2 percent to about 0.8 percent aluminum, from about 0.01 percent to about 0.05 percent carbon, from about 0.005 percent to about 0.01 percent boron, less than about 0.1 percent zirconium, balance nickel and impurities; and
welding the piece of material to form the welded article.

### Claim 13 (depends on 12)

The method of claim 12, including an additional step, after the step of welding, of heating treating the welded article.

### Claim 14 (depends on 12)

The method of claim 12, wherein the step of providing includes the step of providing the piece of cast material.

### Claim 15 (depends on 12)

The method of claim 12, wherein the step of welding includes the step of surface welding the piece of material.

### Claim 16 (depends on 12)

The method of claim 12, wherein the step of welding includes the step of joining the piece of material to a second piece of material.