# US 2004/0079448 A1 · Spall propagation properties of case-hardened M50 and M50NiL bearings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079448 A1
- Document ID: US20040079448A1
- Status: Published application
- Kind: A1
- Application number: 10/279,488
- Filed: 2002-10-24
- Published: 2004-04-29
- Earliest claimed: 2002-10-24
- Assignees: General Electric Company
- Inventors: Mark Alan Rhoads; Michael Gilbert Johnson; Jonothan Allen Scheetz
- Web page: https://patentgrep.com/patent/US20040079448A1

## CPC

- F16C 33/12: Structural composition; Use of special materials or surface treatments, e.g. for rust-proofing
- C21D 1/78: Combined heat-treatments not provided for above
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C23C 8/26: of ferrous surfaces
- C21D 6/004: {containing Cr and Ni}
- F16C 2204/60: Ferrous alloys, e.g. steel alloys
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A roller bearing that provides ball and roller bearing elements comprised of M50 steel and M50NiL steel having surface hardnesses above 60 HRC, and in the range of 65-72 HRC. The hardness in the surface region is achieved by nitriding the surface to achieve a high hardness and extended life. This improvement is brought about by controlling the microstructure of the alloy by minimizing the formation of retained austenite. The material is tempered as required. The surface is then nitrided, but the nitriding operation is carefully controlled to avoid the formation of intergranular nitrides. Because of the method used to prevent the formation of intergranular nitrides, some carbon may be present to prevent the surface of the steel from becoming depleted of carbon. The hardening element in this nitro-carburizing operation is nitrogen, which forms iron nitride as Fe3N or Fe4N intragranularly. The purpose of the carbon in the operation is to maintain the concentration of carbon in the surface of the bearing so that the properties are not altered by decarburizing the surface. Standard gaseous and plasma nitriding techniques also may be used for the nitriding operation.

## Claims

### Claim 1

A bearing material comprising:
a martensitic steel having a surface region with a hardness in the range of about 64-72 HRC, the surface region being case-hardened to a case depth of 0.002″ to about 0.014″, the surface region having a nitrogen content of up to about 2.35% by weight;
the surface region characterized by the formation of intragranular iron nitride particles and a substantial absence of an intergranular white phase, and the martensitic steel characterized by a substantial absence of retained austenite.

### Claim 2 (depends on 1)

The bearing material of claim 1 wherein the martensitic steel is M50 comprising, in weight percent, about 0.80-0.85% carbon, about 4.00-4.25% chromium, about 4.00-4.50% molybdenum, about 0.15-0.35% manganese, about 0.10-0.25% silicon, about 0.9-1.10% vanadium, 0.015% max. phosphorus, 0.010% max. sulfur, 0.15 max. nickel, 0.25% max. cobalt, 0.25% max. tungsten, 0.10 max. copper and the balance essentially iron and incidental impurities.

### Claim 3 (depends on 1)

The bearing material of claim 1 wherein the martensitic steel is M50NiL comprising, in weight percent, about 0.11-0.15% carbon, about 4.00-4.25% chromium, about 4.00-4.50% molybdenum, about 0.15-0.35% manganese, about 0.10-0.25% silicon, about 3.20-3.60% nickel, about 1.13-1.33% vanadium, 0.015% max. phosphorus, 0.010% max. sulfur, 0.25% max cobalt, 0.25% max. tungsten, 0.10 max. copper and the balance essentially iron and incidental impurities.

### Claim 4 (depends on 1)

The bearing material of claim 1 wherein the intergranular white phase comprises a precipitate selected from the group consisting of gamma prime, ε-nitride and combinations thereof.

### Claim 5 (depends on 1)

The bearing material of claim 1 wherein the case-hardened surface region has a hardness in the range of 66-70 HRC.

### Claim 6 (depends on 5)

The bearing material of claim 5 wherein the steel below the case-hardened surface region has a hardness of no greater than 59 HRC.

### Claim 7 (depends on 1)

The bearing material of claim 1 wherein the case-hardened surface region has a nitrogen content of no greater than about 2% by weight.

### Claim 8 (depends on 7)

The bearing material of claim 7 wherein the case-hardened surface region has a nitrogen content of up to about 1.8% by weight.

### Claim 9 (depends on 1)

The bearing material of claim 1 wherein the surface region is case-hardened to a case depth of about 0.006″ to about 0.014″.

### Claim 10 (depends on 1)

The bearing material of claim 1 wherein the surface region of the bearing has a case depth of about 0.004″ to about 0.012″.

### Claim 11 (depends on 1)

The bearing material of claim 1 wherein the wherein the material is used as at least one bearing element selected from the group consisting of an inner race, an outer race and roller elements.

### Claim 12

A method of manufacturing a bearing element from a martensitic steel, the bearing element characterized by a surface region with a hardness in the range of about 64-72 HRC, the surface region being case-hardened to a preselected depth, the surface region characterized by the formation of intragranular iron nitride particles and a substantial absence of an intergranular white phase, comprising the steps of:
providing a martensitic steel composition;
treating the martensitic steel composition to provide a microstructure substantially free of retained austenite; then
nitriding the martensitic steel composition in a partial pressure of nitrogen at a temperature in the range of 800-1000° F. for a preselected time to achieve a hardness in the range of 64-72 HRC to a preselected depth while obtaining a nitrogen content of up to about 2.35% by weight within the preselected depth.

### Claim 13 (depends on 12)

The method of claim 12 wherein the step of treating the martensitic steel composition to provide a microstructure substantially free of retained austenite further includes the additional steps of:
heating the martensitic steel composition to a temperature sufficient to form a structure completely of austenite;
rapidly quenching the austenite in a quench medium so as to avoid the nose of the TTT curve, thereby completely transforming the austenite to martensite.

### Claim 14 (depends on 13)

The method of claim 13 wherein the step of rapidly quenching is accomplished by a cryogenic quench.

### Claim 15 (depends on 13)

The method of claim 13 wherein the step of rapidly quenching is accomplished by an oil quench.

### Claim 16 (depends on 12)

The method of claim 12 wherein the step of treating the martensitic steel composition to provide a microstructure substantially free of retained austenite further includes the additional steps of multiple aging of the martensitic steel composition in the temperature range of 1000° F. to promote the formation of carbide precipitates to promote the transformation of austenite to a ferrite+graphite structure.

### Claim 17 (depends on 12)

The method of claim 12 wherein the step of nitriding the martensitic steel composition includes nitriding to achieve a preselected depth in the range of about 0.002″ to about 0.014″.

### Claim 18 (depends on 12)

The method of claim 12 wherein the step of nitriding the martensitic steel composition includes nitriding for a preselected time of at least about 25 hours.

### Claim 19 (depends on 12)

The method of claim 12 wherein the martensitic steel composition is selected from the group of alloys consisting of M50 and M50NiL.

### Claim 20 (depends on 19)

The method of claim 19 further including the additional step of carburizing the martensitic steel composition in the temperature range of about 800° F. to about 1000° F. to prevent the decarburization of the surface region of the martensitic steel during the nitriding step, so as to maintain the carbon content of the martensitic composition within the composition of the alloy.

### Claim 21 (depends on 12)

The method of claim 12 further including the additional step of grinding the case-hardened surface region to a preselected depth to remove a portion of the surface.

### Claim 22 (depends on 21)

The method of claim 21 wherein the preselected depth is about 0.002″.

### Claim 23 (depends on 12)

The method of claim 12 wherein the step of nitriding achieves a nitrogen content of up to about 2%.

### Claim 24 (depends on 19)

The method of claim 19 wherein M50NiL composition is nitrided at a temperature of about 900° F. to a preselected depth of about 14 mils to achieve a surface hardness of about 70 HRC, the surface region of the M50NiL composition characterized by a nitrogen content of about 2% by weight at a surface, about 1% nitrogen content at about 8 mils below the surface and about 0.5% nitrogen content at about 14 mils below the surface.

### Claim 25 (depends on 24)

The method of claim 24 wherein M50NiL composition is nitrided at a temperature of about 900° F. to a preselected depth of about 6-10 mils to achieve a surface hardness of about 70 HRC, the surface region of the M50NiL composition characterized by a nitrogen content of about 2% by weight at a surface, about 1% nitrogen content at about 6 mils below the surface and about 0.5% nitrogen content at about 10 mils below the surface.