# US 2004/0079408 A1 · Isoelectronic surfactant suppression of threading dislocations in metamorphic epitaxial layers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079408 A1
- Document ID: US20040079408A1
- Status: Published application
- Kind: A1
- Application number: 10/281,302
- Filed: 2002-10-23
- Published: 2004-04-29
- Earliest claimed: 2002-10-23
- Assignees: The Boeing Company
- Inventors: Christopher M. Fetzer; James H. Ermer; Richard R. King; Peter C. Colter
- Web page: https://patentgrep.com/patent/US20040079408A1

## CPC

- H10F 71/127: {The active layers comprising only Group III-V materials, e.g. GaAs or InP}
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3202: {Materials thereof}
- H10P 14/3211: {Silicon, silicon germanium or germanium}
- H10P 14/3221: {Arsenides}
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3418: {Phosphides}
- Y02E 10/544: Solar cells from Group III-V materials
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method of reducing propagation of threading dislocations into active areas of an optoelectronic device having a III-V material system includes growing a metamorphic buffer region in the presence of an isoelectronic surfactant. A first buffer layer may be lattice matched to an adjacent substrate and a second buffer layer may be lattice matched to device layers disposed upon the second buffer layer. Moreover, multiple metamorphic buffer layers fabricated in this manner may be used in a single given device allowing multiple layers to have their band gaps and lattice constants independently selected from those of the rest of the device.

## Claims

### Claim 1

A method of reducing threading dislocations in a device, comprising growing a metamorphic buffer region in the presence of an isoelectronic surfactant.

### Claim 2 (depends on 1)

The method of claim 1, further comprising slowing a nucleation of dislocation loops in said buffer region.

### Claim 3 (depends on 1)

The method of claim 1, wherein said isoelectronic surfactant mediates a manner in which relaxation occurs in said buffer region.

### Claim 4 (depends on 1)

The method of claim 1, further comprising relaxing said buffer region in the presence of said isoelectronic surfactant.

### Claim 5 (depends on 1)

The method of claim 1, further comprising making said buffer region with a plurality of buffer layers.

### Claim 6 (depends on 1)

The method of claim 1, further comprising changing a material composition of said buffer region between a lowermost portion to an uppermost portion.

### Claim 7 (depends on 6)

The method of claim 6, further comprising increasing a concentration of an element in said material concentration from said lowermost portion to said uppermost portion.

### Claim 8 (depends on 6)

The method of claim 6, further comprising decreasing a concentration of an element in said material concentration from said lowermost portion to said uppermost portion.

### Claim 9 (depends on 1)

The method of claim 1, wherein said device includes one of tensile stained epitaxial layers and compressively strained epitaxial layers.

### Claim 10

A method of growing a device having a III-V material system, comprising:
growing a plurality of buffer layers in a buffer region adjacent a device layer;
introducing a first isoelectronic surfactant into the buffer region;
altering a material composition within said buffer region; and
allowing at least one of said buffer layers to relax in the presence of said first surfactant.

### Claim 11 (depends on 10)

The method of claim 10, wherein introducing said first surfactant occurs in the absence of changing a free-electron concentration in said buffer region by said first surfactant.

### Claim 12 (depends on 10)

The method of claim 10, further comprising increasing a concentration of an element in said material concentration from a lowermost portion of said buffer region to an uppermost portion of said buffer region.

### Claim 13 (depends on 10)

The method of claim 10, further comprising decreasing a concentration of an element in said material concentration from a lowermost portion of said buffer region to an uppermost portion of said buffer region.

### Claim 14 (depends on 10)

The method of claim 10, wherein altering said material composition includes changing said material composition in a stepped fashion.

### Claim 15 (depends on 10)

The method of claim 10, wherein altering said material composition includes changing said material composition in a smooth fashion.

### Claim 16 (depends on 10)

The method of claim 10, further comprising introducing said first surfactant into at least one of said buffer layers.

### Claim 17 (depends on 16)

The method of claim 16, further comprising introducing a second isoelectronic surfactant into at least another of said buffer layers.

### Claim 18 (depends on 16)

The method of claim 16, wherein introducing said first surfactant includes adding said first surfactant at a start of a growth of said at least one buffer layer.

### Claim 19 (depends on 16)

The method of claim 16, wherein introducing said first surfactant includes adding said first surfactant during a pause of a growth of said at least one buffer layer.

### Claim 20 (depends on 10)

The method of claim 10, wherein said material system comprises GaInP.

### Claim 21 (depends on 20)

The method of claim 20, wherein said first surfactant comprises Sb and said first surfactant is introduced according to a molar ratio of TESb/(TMGa+TMIn) wherein TESb is triethylantimony, TMGa is trimethylgallium, and TMIn is trimethyindium.

### Claim 22 (depends on 21)

The method of claim 21, wherein said ratio is between about 1×10−5 to 1×105.

### Claim 23 (depends on 10)

The method of claim 10, further comprising growing a first buffer layer lattice matched to a substrate disposed immediately adjacent said first buffer layer.

### Claim 24 (depends on 23)

The method of claim 23, further comprising growing a top buffer layer lattice matched to a device layer disposed immediately adjacent said top buffer layer.

### Claim 25 (depends on 10)

The method of claim 10, wherein said device comprises a solar cell.

### Claim 26

A method of growing a device having a III-V material system, comprising:
growing a layer that is lattice matched to a substrate;
introducing a first isoelectronic surfactant into said lattice matched layer;
growing a layer that is lattice mismatched to a substrate; and
allowing said lattice mismatched layer to relax in the presence of said first surfactant.

### Claim 27 (depends on 26)

The method of claim 26, wherein introducing said first surfactant occurs in the absence of changing a free-electron concentration in said buffer region by said first surfactant.

### Claim 28 (depends on 26)

The method of claim 26, wherein said lattice matched layer includes a buffer region.

### Claim 29 (depends on 28)

The method of claim 28, further comprising altering a concentration of an element in a material concentration of said buffer region from a lowermost portion of said buffer region to an uppermost portion of said buffer region.

### Claim 30 (depends on 29)

The method of claim 29, wherein altering said material composition includes changing said material composition in a stepped fashion.

### Claim 31 (depends on 29)

The method of claim 29, wherein altering said material composition includes changing said material composition in a smooth fashion.

### Claim 32 (depends on 26)

The method of claim 26, wherein introducing said first surfactant includes adding said first surfactant at a start of a growth of said lattice matched layer.

### Claim 33 (depends on 26)

The method of claim 26, wherein introducing said first surfactant includes adding said first surfactant during a pause of a growth of said lattice matched layer.

### Claim 34 (depends on 26)

The method of claim 26, wherein said material system comprises GaInP.

### Claim 35 (depends on 26)

The method of claim 26, wherein said first surfactant comprises Sb and said first surfactant is introduced according to a molar ratio of TESb/(TMGa+TMIn) wherein TESb is triethylantimony, TMGa is trimethylgallium, and TMIn is trimethyindium.

### Claim 36 (depends on 35)

The method of claim 35, wherein said ratio is between about 0.001 to 1.0.

### Claim 37 (depends on 26)

The method of claim 26, wherein said device comprises a solar cell.

### Claim 38

A solar cell having a III-V material system, comprising:
a substrate;
an isoelectronic surfactant, buffer region disposed on the substrate;
said buffer region being relaxed in the presence of said surfactant; and
a device layer disposed in such manner that said buffer region is disposed intermediate said substrate and device layer.

### Claim 39 (depends on 38)

The solar cell of claim 38, wherein the at least one subcell is a metamorphic one.

### Claim 40 (depends on 38)

The solar cell of claim 38, wherein said buffer region includes a plurality of buffer layers.

### Claim 41 (depends on 38)

The solar cell of claim 38, wherein said buffer region comprises a changing material composition between a lowermost portion to an uppermost portion of said buffer region.

### Claim 42 (depends on 41)

The solar cell of claim 41, wherein said changing material composition comprises an increasing concentration of an element in said material composition.

### Claim 43 (depends on 41)

The solar cell of claim 41, wherein said changing material composition comprises a decreasing concentration of an element in said material composition.

### Claim 44 (depends on 38)

The solar cell of claim 38, wherein said buffer region further comprises a first buffer layer lattice matched to said substrate.

### Claim 45 (depends on 44)

The solar cell of claim 44, wherein said buffer region further comprises a top buffer layer lattice matched to said device layer.

### Claim 46 (depends on 38)

The solar cell of claim 38, wherein said device layer is lattice mismatched to said substrate.

### Claim 47

A satellite system comprising:
a satellite; and
a solar cell array having a solar cell that includes:
a substrate;
an isoelectronic surfactant, buffer region disposed on said substrate;
said buffer region being relaxed in the presence of said surfactant without changing a free-electron concentration in said buffer region; and
a device layer disposed in such manner that said buffer region is disposed intermediate said substrate and device layer

### Claim 48 (depends on 47)

The satellite system of claim 47, wherein said device layer is lattice matched to said substrate.

### Claim 49 (depends on 47)

The satellite system of claim 47, wherein said device layer is lattice mismatched to said substrate.

### Claim 50 (depends on 47)

The satellite system of claim 47, wherein said solar cell is a metamorphic one.

### Claim 51 (depends on 50)

The satellite system of claim 50, wherein said buffer region includes a plurality of buffer layers.

### Claim 52 (depends on 51)

The satellite system of claim 51, wherein said buffer region comprises a stepped changing material composition between a lowermost portion to an uppermost portion of said buffer region.

### Claim 53 (depends on 51)

The satellite system of claim 51, wherein said buffer region comprises a smooth changing material composition between a lowermost portion to an uppermost portion of said buffer region.

### Claim 54 (depends on 51)

The satellite system of claim 51, wherein said solar cell comprises a III-V material system.

### Claim 55 (depends on 54)

The satellite system of claim 54, wherein said material system comprises GaInP/GaInAs/Ge.

### Claim 56 (depends on 55)

The satellite system of claim 55, wherein an In content of GaInAs is between about 2% and 30%.

### Claim 57 (depends on 56)

The satellite system of claim 56, wherein said GaInP is lattice matched or lattice mismatched to said GaInAs.

### Claim 58 (depends on 54)

The satellite system of claim 54, wherein said material system comprises GaInP/GaInAs/Si.

### Claim 59 (depends on 58)

The satellite system of claim 58, wherein an In content of GaInAs is between about 0% and 50%.

### Claim 60 (depends on 59)

The satellite system of claim 59, wherein said GaInP is lattice matched or lattice mismatched to said GaInAs.

### Claim 61

A III-V device comprising:
a substrate;
a III-V buffer region adjacent said substrate;
said buffer region having an isoelectronic surfactant; and
a device layer adjacent said buffer region.

### Claim 62 (depends on 61)

The device of claim 61, wherein said substrate comprises Si.

### Claim 63 (depends on 61)

The device of claim 61, wherein said buffer region is relaxed.

### Claim 64 (depends on 61)

The device of claim 61, wherein said buffer region in unrelaxed.

### Claim 65 (depends on 61)

The device of claim 61, wherein said device is one of a light emitting diode, a laser diode, a solar cell, an avalanche photo-diode, a positive-intrinsic-negative diode, a heterojunction bipolar transistor, a homojunction bipolar transistor, a high-electron mobility transistor, and a field effect transistor.

### Claim 66

A solar cell comprising:
an upper cell;
a middle cell below said upper cell;
an upper metamorphic buffer layer below said middle cell, said upper metamorphic buffer layer being grown in the presence of one of a first isoelectronic surfactant and a second isoelectronic surfactant;
a lower cell below said upper metamorphic buffer layer;
a lower metamorphic buffer layer below said lower cell, said lower metamorphic buffer layer grown in the presence of one of said first and second isoelectronic surfactants; and
a substrate below said lower metamorphic buffer layer.

### Claim 67 (depends on 66)

The device of claim 66, wherein the upper cell is composed of GaxIn1−P and x is chosen such that layers of said upper cell are substantially lattice matched to the middle cell.

### Claim 68 (depends on 66)

The device of claim 66, wherein the middle cell is composed of one of GaxIn1−As and GaxIn1−AsyP1−y, and x and y are chosen such that a band gap of the middle cell is between 1.3 eV and 1.8 eV.

### Claim 69 (depends on 66)

The device of claim 66, wherein the upper metamorphic buffer layer is graded in composition such that uppermost layers of the upper metamorphic layer are substantially lattice matched to the upper cell.

### Claim 70 (depends on 66)

The device of claim 66, wherein the lower cell is composed of one of GaInAsN, GaInAs, GaInAsNP, and BgaInAs, and is lattice mismatched to the substrate and a band gap of the lower cell is between 0.6 eV and 1.3 eV.

### Claim 71 (depends on 66)

The device of claim 66, where the lower metamorphic buffer layer is graded in composition and lattice matched to the substrate such that uppermost layers of the lower metamorphic buffer layer are substantially lattice matched to the lower cell.

### Claim 72 (depends on 66)

The device of claim 66, further comprising a Ge bottom cell below said lower metamorphic buffer layer.

### Claim 73

A solar cell comprising:
an upper cell;
an upper metamorphic buffer layer below said upper cell, said upper metamorphic buffer layer being grown in the presence of one of a first isoelectronic surfactant and a second isoelectronic surfactant;
a middle cell below said upper metamorphic buffer layer;
a lower cell below said middle cell;
a lower metamorphic buffer layer below said lower cell, said lower metamorphic buffer layer being grown in the presence of one of said first and second isoelectronic surfactants; and
a substrate below said lower metamorphic buffer layer.

### Claim 74 (depends on 73)

The device of claim 73, wherein the upper cell is composed of GaxIn1−xP.

### Claim 75 (depends on 73)

The device of claim 73, wherein the upper metamorphic buffer layer is graded in composition such that uppermost layers of the upper metamorphic buffer layer are substantially lattice matched to the upper cell.

### Claim 76 (depends on 73)

The device of claim 73, wherein the middle cell is composed of one of GaxIn1−xAs and GaxIn1−xAsyP1−y, x and y are chosen such that a band gap of the middle cell is between 1.3 eV and 1.8 eV.

### Claim 77 (depends on 73)

The device of claim 73, wherein the lower cell is composed of one of GaInAsN, GaInAs, GaInAsNP, and BgaInAs, and is lattice mismatched to the substrate, and the band gap of the lower cell is between 0.6 eV and 1.3 eV.

### Claim 78 (depends on 73)

The device of claim 73, wherein the lower metamorphic buffer layer is graded in composition and lattice matched to the substrate such that uppermost layers of the lower metamorphic buffer layer are substantially lattice matched to the lower cell.

### Claim 79 (depends on 73)

The device of claim 73, further comprising a Ge bottom cell below said lower metamorphic buffer layer.

### Claim 80

A solar cell comprising:
an upper cell;
a first upper metamorphic buffer layer below the upper cell, said first upper metamorphic buffer layer being grown in the presence of one of a first isoelectronic surfactant and a second isoelectronic surfactant;
a middle cell below said upper metamorphic buffer layer;
a second upper metamorphic buffer layer below the middle cell, said second upper metamorphic buffer layer being grown in the presence of one of said first and second isoelectronic surfactants;
a lower cell below said second upper metamorphic buffer layer;
a lower metamorphic buffer layer grown in the presence of one of said first isoelectronic surfactant, said second isoelectronic surfactant, and a third isoelectronic surfactant; and
a substrate below said lower metamorphic buffer layer.

### Claim 81 (depends on 80)

The device of claim 80, wherein the upper cell is composed of GaxIn−xP.

### Claim 82 (depends on 80)

The device of claim 80, wherein the first upper metamorphic buffer layer is graded in composition such that uppermost layers of said first upper metamorphic buffer layer are substantially lattice matched to the upper cell.

### Claim 83 (depends on 80)

The device of claim 80, wherein the middle cell is composed of one of GaxIn1−As and GaxIn1−AsyP1−y, and x and y are chosen such that a band gap of the middle cell is between 1.3 eV and 1.8 eV.

### Claim 84 (depends on 80)

The device of claim 80, wherein the second upper metamorphic buffer layer is graded in composition such that uppermost layers of said second upper metamorphic buffer layer are substantially lattice matched to the middle cell.

### Claim 85 (depends on 80)

The device of claim 80, wherein the lower cell is composed of one of GaInAsN, GaInAs, GaInAsNP, and BgaInAs, and is lattice mismatched to the substrate and the band gap of the lower cell is between 0.6 eV and 1.3 eV.

### Claim 86 (depends on 80)

The device of claim 80, wherein the lower metamorphic buffer layer is graded in composition and lattice matched to the substrate such that uppermost layers of the lower metamorphic buffer layer are substantially lattice matched to the lower cell.