# US 2004/0079279 A1 · Epitaxial CoSi2 on MOS devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079279 A1
- Document ID: US20040079279A1
- Status: Published application
- Kind: A1
- Application number: 10/280,668
- Filed: 2002-10-25
- Published: 2004-04-29
- Earliest claimed: 2002-10-25
- Assignees: The Board of Trustees of the University of Illinois
- Inventors: Chong Wee Lim; Chan Soo Shin; Ivan Georgiev Petrov; Joseph E. Greene
- Web page: https://patentgrep.com/patent/US20040079279A1

## CPC

- C30B 1/00: Single-crystal growth directly from the solid state (unidirectional demixing of eutectoid materials C30B3/00; under a protective fluid C30B27/00)
- C30B 25/02: Epitaxial-layer growth
- C30B 29/10: Inorganic compounds or compositions
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

An SixNy or SiOxNy liner is formed on a MOS device. Cobalt is then deposited and reacts to form an epitaxial CoSi2 layer underneath the liner. The CoSi2 layer may be formed through a solid phase epitaxy or reactive deposition epitaxy salicide process. In addition to high quality epitaxial CoSi2 layers, the liner formed during the invention can protect device portions during etching processes used to form device contacts. The liner can act as an etch stop layer to prevent excessive removal of the shallow trench isolation, and protect against excessive loss of the CoSi2 layer.

## Claims

### Claim 1

A method for forming an epitaxial CoSi2 layer on a MOS device having a Si substrate, said method comprising the steps of:
forming an SixNy or SiOxNy liner on the MOS device; and
depositing Co through a solid phase epitaxy or reactive deposition epitaxy salicide process to form an epitaxial CoSi2 layer underneath the liner on Si portions of the device.

### Claim 2 (depends on 1)

The method as defined in claim 1 wherein said step of depositing comprises solid phase epitaxy and the method further comprises a step of post-annealing to enhance interaction between Si and Co.

### Claim 3 (depends on 2)

The method as defined in claim 2 wherein said step of post-annealing is conducted at approximately 700° C.

### Claim 4 (depends on 1)

The method as defined in claim 1 wherein said step of forming comprises one of a thermal or plasma-enhanced nitridation process.

### Claim 5 (depends on 1)

The method as defined in claim 1 wherein said step of forming forms an approximately 5 Å to 300 Å liner.

### Claim 6 (depends on 5)

The method as defined in claim 5 wherein said step of forming forms an approximately 15 Å liner.

### Claim 7 (depends on 5)

The method as defined in claim 5 wherein said step of depositing comprises forming approximately 10 Å to 1000 Å CoSi2.

### Claim 8 (depends on 7)

The method as defined in claim 7 wherein said step of depositing comprises forming approximately 300 Å CoSi2.

### Claim 9 (depends on 1)

The method as defined in claim 1 wherein x=1, and y ranges from 0.01-1.33.

### Claim 10

A method for fabricating a MOS device having an epitaxial CoSi2 silicide layer, the device including a Si substrate, a gate, source/drain junction regions formed in the Si substrate, and shallow trench isolations formed in the Si substrate, the method comprising the steps of:
forming an SixNy or SiOxNy liner on the MOS device;
depositing Co to form an epitaxial CoSi2 layer underneath the liner on Si portions of the device through a solid phase epitaxy or reactive deposition epitaxy salicide process;
forming an interlevel dielectric layer;
etching to selectively remove the interlevel dielectric layer at the gate and the source/drain junction region;
etching to remove the liner from the gate and the source/drain junction regions; and
forming electrical contacts to the CoSi2 layer at the gate and the source/drain junction regions.

### Claim 11 (depends on 10)

The method as defined in claim 10 wherein said step of depositing comprises solid phase epitaxy and the method further comprises a step of post-annealing to enhance interaction between Si and Co.

### Claim 12 (depends on 11)

The method as defined in claim 11 wherein said step of post-annealing is conducted at approximately 700° C.

### Claim 13 (depends on 12)

The method as defined in claim 12 wherein said step of depositing comprises one of a thermal or plasma-enhanced nitridation process.

### Claim 14 (depends on 10)

The method as defined in claim 10 wherein said step of forming an SixNy or SiOxNy liner forms an approximately 5 Å to 300 Å liner.

### Claim 15 (depends on 14)

The method as defined in claim 14 wherein said step of forming an SixNy or SiOxNy liner forms an approximately 15 Å liner.

### Claim 16 (depends on 14)

The method as defined in claim 14 wherein said step of depositing comprises forming approximately 10 Å to 1000 Å CoSi2.

### Claim 17 (depends on 16)

The method as defined in claim 16 wherein said step of depositing comprises forming approximately 300 Å COSi2.

### Claim 18 (depends on 10)

The method as defined in claim 10 wherein x=1, and y ranges from 0.01-1.33.