# US 2004/0079259 A1 · Method of manufacturing cementitious materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079259 A1
- Document ID: US20040079259A1
- Status: Published application
- Kind: A1
- Application number: 10/282,025
- Filed: 2002-10-29
- Published: 2004-04-29
- Earliest claimed: 2002-10-29
- Inventors: Felix Manig
- Web page: https://patentgrep.com/patent/US20040079259A1

## CPC

- C04B 18/22: Rubber {, e.g. ground waste tires}
- C04B 28/18: containing mixtures of the silica-lime type
- Y02P 40/60: Production of ceramic materials or ceramic elements, e.g. substitution of clay or shale by alternative raw materials, e.g. ashes
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method of manufacturing cementitious materials. The method comprises combining together approximately 12 parts sand with 1 part lime to form a sand and lime mixture where mixture has a sufficient water content to permit at least partial hydration of the lime. The sand and lime mixture is maintained at a temperature of approximately 60° Celsius for a period of between two and four hours. Thereafter water is mixed into the sand and lime mixture at a weight ratio of from between 5 to 15 percent. Pieces of shredded automobile or truck tires are then added to the sand, lime and water mixture at a weight ratio of between 5 and 15 percent. The combination is then subjected to an autoclave process where it is maintained at a pressure of approximately 16 Bar and at temperatures of between 160 and 180 degrees Celsius for between four and eight hours during which the mixture is allowed to cure and harden.

## Claims

### Claim 1

A method of manufacturing cementitious materials, the method comprising the steps of:
(i) combining together approximately 12 parts sand with 1 part lime to form a sand and lime mixture, said sand and lime mixture having a sufficient water content to permit at least partial hydration of said lime;
(ii) maintaining said sand and lime mixture at a temperature of approximately 60° Celsius for a period of between two and four hours;
(iii) mixing water into said sand and lime mixture at a weight ratio of from between 5 to 15 percent;
(iv) adding and mixing pieces of shredded automobile or truck tires to said sand, lime and water mixture at a weight ratio of between 5 and 15 percent;
(v) subjecting said sand, lime, water and shredded tire mixture to an autoclave process wherein said mixture is maintained at a pressure of approximately 16 Bar and at temperatures of between 160 and 180 degrees Celsius for between four and eight hours during which said mixture is allowed to cure and harden.

### Claim 2 (depends on 1)

The method as claimed in claim 1 wherein said tires are shredded into pieces of approximately three to four millimetres in size prior to combining with said sand, lime and water mixture.

### Claim 3 (depends on 1)

The method as claimed in claim 1 including the step of placing said sand, lime, water and shredded tire mixture into a mold or press to form said mixture into a desired shape and thereafter subjecting said desired shape to said autoclave process.

### Claim 4 (depends on 1)

The method as claimed in claim 1 wherein upon subjecting said sand, lime, water and shredded tire mixture to said autoclave process, said pieces of shredded tires expand creating small pockets or voids within said material, upon curing and hardening of said material said voids becoming permanently maintained within said material.

### Claim 5

A cementitious material comprising:
(i) 60 to 80 percent by weight sand, gravel or aggregate;
(ii) 5 to 15 percent by weight portland cement;
(iii) 5 to 15 percent by weight water; and
(iv) 5 to 15 percent by weight shredded automobile tires, truck tires, or recycled rubber.

### Claim 6 (depends on 5)

The material as claimed in claim 5 wherein said automobile tires, truck tires, or recycled rubber are shredded to a size of approximately three to four millimetres.

### Claim 7 (depends on 6)

The material as claimed in claim 6 wherein upon heating, said shredded pieces of automobile tires, truck tires, or recycled rubber expand creating small pockets or voids within said material such that upon curing and hardening of said material said voids are permanently maintained within said material.

### Claim 8 (depends on 7)

The material as claimed in claim 7 formed into blocks such that upon curing said blocks comprise concrete blocks.

### Claim 9

A method of manufacturing cementitious materials, the method comprising the steps of:
(i) forming a mixture of sand, cement, water and fragmented rubber or plastic material, said sand component comprising from 60 to 80 percent by weight of said mixture, said cement component comprising from 5 to 15 percent by weight of said mixture, said water component comprising from 5 to 15 percent by weight of said mixture, said fragmented rubber or plastic material comprising from 5 to 15 percent by weight of said mixture;
(ii) subjecting said sand, cement, water and fragmented rubber or plastic mixture to an autoclave process wherein said fragments of rubber or plastic material expand creating small pockets or voids within said mixture, said mixture curing and hardening during said autoclave process such that said pockets or voids become permanently entrained within said hardened mixture.

### Claim 10 (depends on 9)

The method as claimed in claim 9 wherein said fragments of rubber or plastic material are formed through shredding automobile or truck tires into fragments having a size range of from three to four millimetres.

### Claim 11 (depends on 9)

The method as claimed in claim 9 wherein said autoclave process is carried out at a temperature of from 160° to 180° Celsius, at a pressure of approximately 16 Bar, and for a time period of from four to eight hours.

### Claim 12

The method as claimed in claimed 9 including the further step of pressing said sand, cement, water and fragmented rubber or plastic mixture into molds prior to subjecting said mixture to said autoclave process such that said autoclave process results in the production of concrete products of a desired shape.