# US 2004/0079197 A1 · Preparation of alloys by the armstrong method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079197 A1
- Document ID: US20040079197A1
- Status: Published application
- Kind: A1
- Application number: 10/654,493
- Filed: 2003-09-03
- Published: 2004-04-29
- Earliest claimed: 2002-09-07
- Assignees: International Titanium Powder, LLC
- Inventors: Donn Reynolds Armstrong; Richard Paul Anderson; Lance E. Jacobsen
- Web page: https://patentgrep.com/patent/US20040079197A1

## CPC

- B22F 9/28: starting from gaseous metal compounds
- C01B 21/06: Binary compounds of nitrogen with metals, with silicon, or with boron, {or with carbon, i.e. nitrides; Compounds of nitrogen with more than one metal, silicon or boron}(azides C01B21/08)
- C22B 34/1272: {reduction of titanium halides, e.g. Kroll process}
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

A method and apparatus for making alloys or ceramics by the subsurface injection of an equilibrium vapor of a boiling liquid of the ceramic or alloys constituents is disclosed. Various powders and products are disclosed.

## Claims

### Claim 1

A method of producing an alloy or ceramic by the exothermic subsurface reduction of a mixed halide vapor of the alloy or ceramic constituents with liquid alkali or alkaline earth metal or mixtures thereof, comprising providing a liquid mixture of halides of the alloy or ceramic constituents in a preselected atomic ratio, boiling the liquid until an equilibrium with the vapor is attained, and thereafter introducing the equilibrium vapor into the liquid reductant metal to form an alloy or ceramic powder of the equilibrium vapor constituents in the preselected atomic ratio.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reductant metal is Na or Mg.

### Claim 3 (depends on 2)

The method of claim 2, wherein the halide is a chloride.

### Claim 4 (depends on 3)

The method of claim 3, wherein the alloy is principally Ti.

### Claim 5 (depends on 4)

The method of claim 4, wherein the alloy is principally Ti and includes Al and V.

### Claim 6 (depends on 5)

The method of claim 5, wherein the alloy is substantially 6% Al and 4% V with the remainder substantially Ti.

### Claim 7 (depends on 1)

The method of claim 1, wherein the reductant metal is present in excess of the stoichiometric amount.

### Claim 8 (depends on 7)

The method of claim 7, wherein the reductant metal is present in the range of from about 20 to about 50 times the stoichiometric amount.

### Claim 9 (depends on 7)

The method of claim 7, wherein the reductant metal is present as a flowing stream.

### Claim 10 (depends on 1)

The method of claim 1, wherein the vapor is introduced into the liquid metal by subsurface injection at greater than sonic velocity.

### Claim 11 (depends on 1)

The method of claim 1, wherein the ceramic is one or more of a nitride or a carbide or a boride mixture thereof.

### Claim 12 (depends on 1)

The method of claim 1, wherein the alloy includes one or more of Ti, Al, Sb, Be, B, Ta, Zr, V, Nb, Mo, Ga, U, Re, or Si.

### Claim 13 (depends on 12)

The method of claim 12, wherein the alloy includes one or more of Ti, Al, Ta, Zr, V, Nb, Mo, Ga, Re, or Si.

### Claim 14 (depends on 1)

The method of claim 1, wherein at least some of the liquid halides are under pressure prior to forming the liquid mixture of halides.

### Claim 15 (depends on 1)

A powder produced by the method of claim 1.

### Claim 16 (depends on 15)

A solid produced from the powder of claim 15.

### Claim 17

A method of producing an alloy by the exothermic subsurface reduction of a mixed halide vapor of the alloy constituents with liquid alkali or alkaline earth metal or mixtures thereof, comprising providing a liquid mixture of halides of the alloy constituents in a preselected atomic ratio, boiling the liquid until an equilibrium with the vapor is attained, and thereafter injecting the equilibrium vapor into the liquid reductant metal at greater than sonic velocity to form an alloy powder of the equilibrium vapor constituents in the preselected atomic ratio.

### Claim 18 (depends on 17)

The method of claim 17, wherein the reductant metal is Na or Mg.

### Claim 19 (depends on 18)

The method of claim 18, wherein the halide is a chloride.

### Claim 20 (depends on 19)

The method of claim 19, wherein the alloy is principally Ti.

### Claim 21 (depends on 20)

The method of claim 20, wherein the alloy is principally Ti and includes Al and V.

### Claim 22 (depends on 21)

The method of claim 21, wherein the alloy is substantially 6% Al and 4% V with the remainder substantially Ti.

### Claim 23 (depends on 22)

The method of claim 22, wherein the reductant metal is present in excess of the stoichiometric amount.

### Claim 24 (depends on 23)

The method of claim 23, wherein the reductant metal is present in the range of from about 20 to about 50 times the stoichiometric amount.

### Claim 25 (depends on 24)

The method of claim 24, wherein the reductant metal is present as a flowing stream.

### Claim 26 (depends on 17)

The method of claim 17, wherein the reductant metal is Na and the halide is a chloride and the alloy includes one or more of Ti, Al, Sb, Be, B, Ta, Zr, V, Nb, Mo, Ga, U, Re, or Si.

### Claim 27 (depends on 26)

The method of claim 26, wherein the alloy includes one or more of Ti, Al, Ta, Zr, V, Nb, Mo, Ga, Re, or Si.

### Claim 28 (depends on 17)

The method of claim 17, wherein one or more of the liquid halides is maintained under pressure.

### Claim 29 (depends on 17)

A powder produced by the method of claim 17.

### Claim 30 (depends on 29)

A solid produced from the powder of claim 29.

### Claim 31

An apparatus for producing an alloy or ceramic by the subsurfaces reduction of a mixed halide vapor of the alloy or ceramic constituents with liquid alkali metal or alkaline earth metal or mixtures thereof, a container for storing each of the constituents in liquid form, a storage container for liquid alkali metal or alkaline earth metal or mixtures thereof, a boiler in communication with each of said containers for storing each of the constituents in liquid form, heating mechanism in heat exchange relationship with said boiler, a reactor in communication with said boiler and said storage container for the liquid metal, pumping mechanism for transferring a predetermined atomic ratio of each liquid constituent to said boiler, and pumping mechanism for transferring liquid metal from said storage container thereto to said reactor, whereby equilibrium vapor from said boiler infected subsurface of the liquid metal in said reactor produces an alloy or ceramic powder of the constituents in the predetermined atomic ratios.