# US 2004/0079151 A1 · Encapsulated float and method for making same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079151 A1
- Document ID: US20040079151A1
- Status: Published application
- Kind: A1
- Application number: 10/282,401
- Filed: 2002-10-29
- Published: 2004-04-29
- Earliest claimed: 2002-10-29
- Inventors: Ricardo Canales
- Web page: https://patentgrep.com/patent/US20040079151A1

## CPC

- G01F 23/76: characterised by the construction of the float
- B29C 44/18: Filling preformed cavities {(B29C44/1204 takes precedence)}
- G01F 23/32: using rotatable arms or other pivotable transmission elements
- B29C 44/14: the preformed part being a lining {(B29C44/1209 takes precedence)}
- G01F: MEASURING VOLUME, VOLUME FLOW, MASS FLOW OR LIQUID LEVEL; METERING BY VOLUME
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A float, including rubber material for sensing liquid levels having a chemically resistant protective covering said float having greater resistance to attach from chemicals, such as hydrocarbons, acids, and chlorinated solvents, said float may be made to include magnets, guiding devices or sensors. Also disclosed is the method for manufacturing the float of this invention including the steps of milling acrylonitrile rubber, phenolic resin, sulfur and various additives in a Banbury mill and mixing at an elevated temperature below 250°, compression molding at up to 900 psi pressure between 250° and 350° F., cooling and filling a pre made protective skin container with the mixture, closing the container and heating the sealed container to bond the mixture to the container skin.

## Claims

### Claim 1

A float for liquid level sensing comprising:
a body including rubber material,
and a protective covering for said body.

### Claim 2 (depends on 1)

A float in accordance with claim 1 wherein the rubber material is synthetic rubber.

### Claim 3 (depends on 1)

A float in accordance with claim 1 wherein the rubber material is acrylonitrile rubber.

### Claim 4 (depends on 1)

A float in accordance with claim 1 wherein the protective covering is made of plastic.

### Claim 5 (depends on 3)

A float in accordance with claim 3 wherein the protective covering is polyethylene.

### Claim 6 (depends on 3)

A float in accordance with claim 3 wherein the protective covering is polypropylene.

### Claim 7 (depends on 1)

A float in accordance with claim 1 wherein said protective covering is bonded to said float body.

### Claim 8 (depends on 1)

A float in accordance with claim 1 wherein said float body includes a magnet therein.

### Claim 9 (depends on 1)

A float in accordance with claim 1 including a guiding device extending out of said body and protective coating.

### Claim 10 (depends on 1)

A float in accordance with claim 1 wherein said float body includes an insert therein.

### Claim 11

A float including rubber material for liquid level sensing wherein the improvement comprises:
encapsulating the body within a protective chemical-resistant plastic covering.

### Claim 12 (depends on 11)

A float in accordance with claim 11 wherein the encapsulating protective covering is a preformed polyethylene container.

### Claim 13 (depends on 11)

A float in accordance with claim 11 wherein the encapsulating protective covering is a preformed polypropylene container.

### Claim 14 (depends on 11)

A float in accordance with claim 11 wherein the rubber material is acrylonitrile.

### Claim 15 (depends on 11)

A float in accordance with claim 11 wherein the rubber material and the plastic covering are bonded.

### Claim 16

A method of encapsulating a float for liquid level sensing with a protective skin comprising:
A first step, to a Banbury mill mixer or the like mix by weight about
30.0% to 55.0% acrylonitrile rubber
0.5% to 4.2% zinc oxide
1.0% to 15.0% stearic acid
0.1% to 2.0% retarder SAX salicylic acid (O-hydroxybenzoic acid) C6H4(OH) (COOH)
3.0% to 22% mistron vapor Mg3Si4O10 (OH)2
0.3% to 2.75% coumarone Indene resin absorbed on synthetic calcium
Silicate (72% cumar P-25) and
8.0% to 15.0% sulfur
mix said components for between about 60 to 180 minutes while maintaining the temperature of the mixture to below about 250° F.,
a second step comprising taking the mixture of the first step transferring it to a suitably sized roller mill or the like and adding by weight about
12.0% to 40.0% phenolic resin (C6H6O.CH20)X
2.5% to 10.0% carbon black
0.25% to 1.5% Altax C14H8N2S4
1.75% to 15% epoxy-resin and
1.0% to 5.0% blowing agent
mixing said components for about 15 to 50 minutes while maintaining the temperature of the mixture to below about 200° F.;
a third step comprising transferring the mixture of the second step to a compression tool where the mixture is subjected to a pressure of about 20-900 lbs. per cubic inch for between about 5 to 45 minutes at a temperature of between about 200° F. to 350° F., removing the mixture from the compression tool and cooling
a fourth step, placing a sufficient amount of the material of the third step to fill a plastic container of the desired shape and size;
a fifth step of placing the plastic container into the desired finish mold tool and heating to between about 250° F. and 550° F. for between about 20 to 180 minutes to allow the acrylonitrile rubber to expand into intimate contact with the interior surface of the plastic container, whereby a rubber based float with a protective coating is produced.

### Claim 17 (depends on 16)

A method as described in claim 16 wherein the mixture of the first step has a Shore A hardness of between about 15 to 90.

### Claim 18 (depends on 16)

A method as described in claim 16 wherein the blowing agent is (NO)2C3H10N4.

### Claim 19 (depends on 16)

A method as described in claim 16 wherein the mixture of the second step has a Shore A hardness of between about 15 to 90.

### Claim 20 (depends on 16)

A method as described in claim 16 wherein the mixture of the third step has a Shore A hardness of between about 15 to 90.

### Claim 21 (depends on 16)

A method as described in claim 16 wherein a magnet may be added at step 3.

### Claim 22 (depends on 16)

A method as described in claim 16 wherein an insert may be added at step 3.

### Claim 23 (depends on 16)

A method as described in claim 16 wherein guides may be added at step 3.

### Claim 24 (depends on 16)

A method in accordance with claim 16 wherein the mixture comprises by weight:
37.04% to 37.5% acrylonitrile rubber
0.84% to 1.01 % zinc oxide
1.67% to 2.02% stearic acid
0.21% to 0.51% retarder SAX salicylic acid (O-hydroxybenzoic acid) C6H4(OH) (COOH)
14.14% to 15.83% mistron vapor Mg3Si4O10 (OH)2
0.83% to 1.35% coumarone Indene resin absorbed on synthetic calcium silicate (72% cumar P-25) and
10.10% to 10.83% sulfur
22.22% to 22.50% phenolic resin (C6H6O.CH20)X
3.33% to 4.03% carbon black
0.63% to 0.84% Altax C14H8N2S4
2.50% to 2.70% epoxy-resin and
3.33% to 4.04% blowing agent (NO)2C5H10N4
the mixture of the third step is subjected to a pressure of about 350 to 410 lbs. per cubic inch for between about 10 to 18 minutes at a temperature of between about 265° F. to 275° F.
heating the mixture of the third step to between about 250° F. and 500° F. for between about 30 to 70 minutes.

### Claim 25 (depends on 24)

A method in accordance with claim 24 wherein the mixture of the first step has a Shore A hardness of between about 65 to 75.

### Claim 26 (depends on 24)

A method in accordance with claim 24 wherein the mixture of the second step has a Shore A hardness of between about 65 to 75.

### Claim 27 (depends on 24)

A method in accordance with claim 24 wherein the mixture of the third step has a Shore A hardness of between about 65 to 75.

### Claim 28 (depends on 24)

A method in accordance with claim 24 wherein a magnet is added during step three.

### Claim 29 (depends on 24)

A method in accordance with claim 24 wherein a guide is added during step three.

### Claim 30 (depends on 24)

A method in accordance with claim 24 wherein an insert is added during step three.

### Claim 31

A float for sensing liquid level produced by the process comprises:
a) mixing a rubber material and resin in a mill;
b) adding a blowing agent to the mixture of step a);
c) subjecting the mixture of step b) to pressure and heat to form float body material;
d) filling a preformed plastic container with the float body material of step c);
e) heating the filled container of step d) until the float body material expands into intimate contact with the preformed plastic container.

### Claim 32 (depends on 31)

A product in accordance with claim 31 wherein the temperature of step A is below about 250° F.

### Claim 33 (depends on 31)

A product in accordance with claim 31 wherein the temperature of step B is below about 250° F.

### Claim 34 (depends on 32)

A product in accordance with claim 32 wherein resin is added at step B.

### Claim 35 (depends on 31)

A product in accordance with claim 31 wherein the temperature of step C is below about 200° F. to 350° F.

### Claim 36 (depends on 31)

A product in accordance with claim 31 wherein the temperature of step C wherein the pressure is between about 20 and 900 lbs. per cubic inch.

### Claim 37 (depends on 31)

A product in accordance with claim 31 wherein a magnet is added at step C.

### Claim 38 (depends on 31)

A product in accordance with claim 31 wherein an insert is added at step C.

### Claim 39 (depends on 31)

A product in accordance with claim 31 wherein a guiding device is added at step C.

### Claim 40 (depends on 31)

A product in accordance with claim 31 wherein the plastic container is polyethylene.

### Claim 41 (depends on 31)

A product in accordance with claim 31 wherein the plastic container is polypropylene.

### Claim 42 (depends on 37)

A product in accordance with claim 37 wherein the temperature of step D is between about 250° F. and 550° F.

### Claim 43

A float for liquid level sensing having a chemically resistant protective plastic covering made by the process of:
a first step, by weight mixing
30.0% to 55.0% acrylonitrile rubber
0.5% to 4.2% zinc oxide
1.0% to 15.0% stearic acid
0.1% to 2.0% retarder SAX salicylic acid (O-hydroxybenzoic acid) C6H4(OH) (COOH)
3.0% to 22% mistron vapor Mg3Si4O10 (OH)2
0.3% to 2.75% coumarone Indene resin absorbed on synthetic calcium
Silicate (72% cumar P-25) and
8.0% to 15.0% sulfur
for between about 60 to 180 minutes while maintaining the temperature of the mixture to below about 250° F.,
said blended mixture to have a shore A hardness of between about 15 to 90
a second step comprising taking the mixture of the first step and adding by weight about
12.0% to 40.0% phenolic resin (C6H6O.CH20)X
2.5% to 10.0% carbon black
0.25% to 1.5% Altax C14H8N2S4
1.75% to 15% epoxy-resin and
1.0% to 5.0% blowing agent (NO)2C5H10N4
mixing said components for about 15 to 50 minutes while maintaining the temperature of the mixture to below about 200° F.;
said blended mixture having a shore A hardness of between about 15 and 90;
a third step comprising transferring the mixture of the second step to a compression tool where the mixture is subjected to a pressure of about 20-900 lbs. per cubic inch for between about 5 to 45 minutes at a temperature of between about 200° F. to 350° F., removing the mixture from the compression tool and cooling
said mixture to have a Shore A hardness of between 15 to 90;
a fourth step, adding to said mixture any magnets, inserts or guides;
a fifth step, placing a sufficient amount of the mixture of step 3 to fill a plastic container of the desired shape and size;
placing the plastic container into the desired finish mold tool and heating to between about 250° F. and 550° F. for between about 20 to 180 minutes to allow the mixture to expand into intimate contact with the interior surface of the plastic container, cool and inspect for defects.