# US 2004/0079118 A1 · Method of forming a phosphorus doped optical core using a PECVD process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079118 A1
- Document ID: US20040079118A1
- Status: Published application
- Kind: A1
- Application number: 10/279,366
- Filed: 2002-10-23
- Published: 2004-04-29
- Earliest claimed: 2002-10-23
- Assignees: Applied Materials, Inc.; A Delaware Corporation
- Inventors: Hichem M'Saad; Anchuan Wang; Sang Ahn
- Web page: https://patentgrep.com/patent/US20040079118A1

## CPC

- G02B 6/132: by deposition of thin films
- C23C 16/401: {containing silicon}
- C23C 16/505: using radio frequency discharges
- G02B 2006/12169: {Annealing}
- G02B 2006/12176: {Etching}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Embodiments of the present invention provide a highly uniform low cost production worthy solution for manufacturing low propagation loss optical waveguides on a substrate. In one embodiment, the present invention provides a method of forming a PSG optical waveguide on an undercladding layer of a substrate that includes forming at least one silicate glass optical core on said undercladding layer using a plasma enhanced chemical vapor deposition process including a silicon source gas, an oxygen source gas, and a phosphorus source gas, wherein the oxygen source gas and silicon source gas have a ratio of oxygen atoms to silicon atoms greater than 20:1.

## Claims

### Claim 1

A method of forming an optical waveguide on an undercladding layer of a substrate, the method comprising:
forming at least one silicate glass optical core on said undercladding layer using a plasma enhanced chemical vapor deposition process including a silicon source gas, an oxygen source gas, and a phosphorus source gas;
wherein the oxygen source gas and silicon source gas have a ratio of oxygen atoms to silicon atoms greater than 20:1.

### Claim 2 (depends on 1)

The method of claim 1 further comprising a termination step wherein all source gases, except the oxygen source gas, are evacuated from the deposition chamber after the optical core is formed.

### Claim 3 (depends on 2)

The method of claim 2 wherein the termination step comprises an N2O plasma purge step lasting between about 5 to 10 seconds.

### Claim 4 (depends on 2)

The method of claim 2 wherein the oxygen source gas includes N2O, CO2, or CO and the phosphorous source gas includes PH3.

### Claim 5 (depends on 1)

The method of claim 1 wherein the contrast between the refractive index of the optical core and the refractive index of the undercladding layer is less than 2%.

### Claim 6 (depends on 5)

The method of claim 5 wherein the contrast between the refractive index of the optical core and the refractive index of the undercladding layer is in the range between about 0.6% to 1.0%.

### Claim 7 (depends on 1)

The method of claim 1 wherein the plasma enhanced chemical vapor deposition process comprises pressure of less than 10 Torr and an RF energy in the range of about 1-2 Watts/cm2.

### Claim 8 (depends on 1)

The method of claim 1 wherein the phosphorous content of the optical core is in the range of about 6.5 wt. % to 11.0 wt. %.

### Claim 9 (depends on 1)

The method of claim 1 wherein the thickness of the optical core is greater than about 4.5 μm.

### Claim 10 (depends on 9)

The method of claim 9 wherein the thickness of the optical core is in the range of 4.5 μm to 7.2 μm.

### Claim 11 (depends on 1)

The method of claim 1 wherein the refractive index of the optical core is less than 1.5.

### Claim 12 (depends on 11)

The method of claim 11 wherein the refractive index of the optical core is in the range of about 1.46 to 1.475.

### Claim 13 (depends on 1)

The method of claim 1 wherein the phosphorous source gas includes PH3.

### Claim 14 (depends on 13)

The method of claim 13 wherein the phosphorous source gas is PH3 diluted in N2.

### Claim 15 (depends on 13)

The method of claim 13 wherein the phosphorous source gas is PH3 diluted in an inert gas.

### Claim 16 (depends on 13)

The method of claim 13 wherein the phosphorous source gas is 100% PH3.

### Claim 17 (depends on 1)

The method of claim 1 wherein the oxygen source gas is N2O, CO2, or CO.

### Claim 18 (depends on 1)

The method of claim 1 wherein the deposition temperature is greater than 300° C.

### Claim 19 (depends on 1)

The method of claim 1 wherein the deposition temperature is between about 400° C. to 550° C.

### Claim 20 (depends on 1)

The method of claim 1 further comprising an anneal step.

### Claim 21 (depends on 20)

The method of claim 20 wherein the anneal step includes an ambient of steam, molecular oxygen, or molecular nitrogen, at a temperature between about 1000° C. to 1100° C. for between about 2 to 4 hours.

### Claim 22 (depends on 20)

The method of claim 20 wherein the anneal step includes an ambient of steam at a temperature between about 1000° C. to 1100° C. for between about 2 hours.

### Claim 23

A substrate processing system comprising:
a process chamber comprising a chamber wall and chamber lid;
an RF power supply operatively coupled to the process chamber;
a pedestal for holding a substrate during substrate processing;
a gas delivery system configured to introduce gases into the process chamber, including sources for a silicon-containing gas, an oxygen-containing gas, and a phosphorous containing gas;
a controller for controlling the gas delivery system, chamber pressure, and RF power levels;
a memory coupled to the controller, the memory comprising a computer-readable medium having a computer-readable program embodied therein for directing operation of the substrate processing system to form an optical core on a substrate, the computer-readable program including
instructions to flow a gaseous mixture containing flows of the silicon-containing gas, the oxygen-containing gas, and the phosphorous containing gas;
instructions to maintain a pressure of less than 10 Torr within the process chamber; and
instructions to provide an RF power density between about 1 to 2 Watts/cm2 into the process chamber, and in accordance therewith, generate a plasma from the gaseous mixture and deposit a phosphorous doped silicate glass optical core, wherein the oxygen-containing gas and silicon-containing gas have a ratio of oxygen atoms to silicon atoms greater than 20:1.

### Claim 24 (depends on 23)

The substrate processing system of claim 23 wherein the computer-readable program further includes instructions for a termination step wherein all source gases, except the oxygen-containing gas, are evacuated from the deposition chamber after the optical core is formed.

### Claim 25 (depends on 23)

The substrate processing system of claim 23 wherein the computer-readable program further includes instructions for forming an optical core having a thickness in the range of 4.5 μm to 7.2 μm.

### Claim 26 (depends on 23)

The substrate processing system of claim 23 wherein the computer-readable program further includes instructions for forming an optical core having a contrast between the refractive index of the optical core and the refractive index of an undercladding layer in the range between about 0.6% to 1.0% and a phosphorous content in the range of about 6.5 wt. % to 11.0 wt. %.

### Claim 27

A computer-readable storage medium having a computer-readable program embodied therein for directing operation of a substrate processing system including a process chamber; an RF power supply; and a gas delivery system configured to introduce gases into the process chamber, the computer-readable program including instructions for operating the substrate processing system to form an optical core on a substrate disposed in the processing chamber in accordance with the following:
establishing a pressure of less than 10 Torr in said processing chamber;
generating an RF power density of between about 1 to 2 Watts/cm2; and
providing a silicon source gas, an oxygen source gas, and a phosphorous source gas in said processing chamber, wherein the oxygen source gas and silicon source gas have a ratio of oxygen atoms to silicon atoms greater than 20:1.

### Claim 28 (depends on 27)

The computer-readable storage medium of claim 27 wherein the computer-readable program further includes instructions for a termination step wherein all source gases, except the oxygen-containing gas, are evacuated from the deposition chamber after the optical core is formed.

### Claim 29 (depends on 27)

The computer-readable storage medium of claim 27 wherein the computer-readable program further includes instructions for forming an optical core having a thickness in the range of 4.5 μm to 7.2 μm.

### Claim 30 (depends on 27)

The computer-readable storage medium of claim 27 wherein the computer-readable program further includes instructions for forming an optical core having a contrast between the refractive index of the optical core and the refractive index of an undercladding layer in the range between about 0.6% to 1.0% and a phosphorous content in the range of about 6.5 wt. % to 11.0 wt. %.