# US 2004/0079114 A1 · Low-temperature fabrication of glass optical components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079114 A1
- Document ID: US20040079114A1
- Status: Published application
- Kind: A1
- Application number: 10/283,402
- Filed: 2002-10-29
- Published: 2004-04-29
- Earliest claimed: 2002-10-29
- Assignees: Corning Incorporated
- Inventors: Bruce G. Aitken; Dilip K. Chatterjee; Daniel H. Raguin
- Web page: https://patentgrep.com/patent/US20040079114A1

## CPC

- G02B 5/045: {Prism arrays}
- C03B 11/082: {having profiled, patterned or microstructured surfaces}
- C03B 11/086: {of coated dies (use of materials as release or lubricating compositions C03B40/02)}
- C03B 19/06: by sintering, {e.g. by cold isostatic pressing of powders and subsequent sintering, by hot pressing of powders, by sintering slurries or dispersions not undergoing a liquid phase reaction}
- C03C 3/32: Non-oxide glass compositions, e.g. binary or ternary halides, sulfides or nitrides of germanium, selenium or tellurium
- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- G02B 3/0031: {Replication or moulding, e.g. hot embossing, UV-casting, injection moulding}
- G02B 3/005: {arranged along a single direction only, e.g. lenticular sheets (G02B3/0043 takes precedence)}
- G02B 3/0056: {arranged along two different directions in a plane, e.g. honeycomb arrangement of lenses (G02B3/0043 takes precedence; miniaturised objectives for electronic devices employing wafer level optics G02B13/0085)}
- G02B 3/06: with cylindrical or toric faces
- C03B 2201/80: Non-oxide glasses or glass-type compositions
- C03B 2201/82: Fluoride glasses, e.g. ZBLAN glass
- C03B 2201/86: Chalcogenide glasses, i.e. S, Se or Te glasses
- C03B 2201/88: Chalcohalide glasses, i.e. containing one or more of S, Se, Te and one or more of F, Cl, Br, I
- C03B 2215/16: Metals or alloys, e.g. Ni-P, Ni-B, amorphous metals
- C03B 2215/17: comprising one or more of the noble meals, i.e. Ag, Au, platinum group metals
- C03B 2215/41: Profiled surfaces
- C03B 2215/412: fine structured, e.g. fresnel lenses, prismatic reflectors, other sharp-edged surface profiles
- C03B 2215/414: Arrays of products, e.g. lenses
- C03B 2215/60: Aligning press die axes
- C03C 2217/77: Coatings having a rough surface
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In one aspect, a method is provided for molding from glass complex optical components such as lenses, microlens, arrays of microlenses, and gratings or surface-relief diffusers having fine or hyperfine microstructures suitable for optical or electro-optical applications. In another aspect, mold masters or patterns, which define the profile of the optical components, made on metal alloys, particularly titanium or nickel alloys, or refractory compositions, with or without a non-reactive coating are provided. Given that molding optical components from oxide glasses has numerous drawbacks, it has been discovered in accordance with the invention that non-oxide glasses substantially eliminates these drawbacks. The non-oxide glasses, such as chalcogenide, chalcohalide, and halide glasses, may be used in the mold either in bulk, planar, or power forms. In the mold, the glass is heated to about 10-110° C., preferably about 50° C., above its transition temperature (Tg), at which temperature the glass has a viscosity that permits it to flow and conform exactly to the pattern of the mold.

## Claims

### Claim 1

A method of making a precision optical element, the method comprises:
a) providing a non-oxide glass with a glass transition temperature (Tg) of up to about 550° C.;
b) providing a mold having an active surface that has an optical finish that can be used with or without a protective coating, wherein said active surface is either optionally: (A) coated with a layer of non-reactive material, or (B) made from a material having a crystallization temperature higher than at least an operational temperature, or (C) both made from a material having a crystallization temperature higher than at least an operational temperature and coated with said non-reactive material;
c) placing said glass in said mold;
d) heating said mold and glass to an operational temperature from about 10° C. to about 110° C. above the Tg; and
e) pressing the mold when the viscosity of the glass reaches about 106-1012 poise.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said glass is in the form of a frit powder, planar body, regular or irregularly shaped bulk-solid, or a combination thereof.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said glass is a chalcogenide glass.

### Claim 4 (depends on 3)

The method according to claim 3, wherein said glass is a sulfide glass.

### Claim 5 (depends on 4)

The method according to claim 4, wherein said sulfide is selected from the group consisting of GeAs2S2, As2S3, Ga2S3, and Is2S3.

### Claim 6 (depends on 3)

The method according to claim 3, wherein said glass is a selenide glass.

### Claim 7 (depends on 3)

The method according to claim 3, wherein said glass is a telluride glass.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said glass is a chalco-halide glass.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said glass is a halide glass.

### Claim 10 (depends on 1)

The method according to claim 1, wherein said layer of non-reactive material is boron nitride.

### Claim 11 (depends on 1)

The method according to claim 1, wherein said mold further comprises at least a first portion and a second portion.

### Claim 12 (depends on 1)

The method according to claim 1, wherein said active surface is made from either a titanium alloy or a nickel alloy.

### Claim 13 (depends on 1)

The method according to claim 1, wherein at least an active, molding surface is formed of a titanium alloy with a composition, in terms of weight percent, comprising about 98-80% Ti, 1-10% Al, and 1-10% V.

### Claim 14 (depends on 1)

The method according to claim 1, wherein at least an active, molding surface is formed of a material selected from: a titanium alloy; a nickel alloy; a silicon carbide; a silicon nitride; or a refractory ceramic composite of silicon carbide and silicon nitride.

### Claim 15 (depends on 1)

The method according to claim 1, wherein said operational temperature is in the ranges from about 20° C. to about 90° C. above Tg.

### Claim 16 (depends on 21)

The method according to claim 21, wherein said operational temperature is in the range from about 30-70° C. above Tg.

### Claim 17 (depends on 1)

The method according to claim 1, wherein said viscosity of the glass is about 107-1011 poise.

### Claim 18 (depends on 17)

The method according to claim 17, wherein said viscosity of the glass is about 109 poise.

### Claim 19 (depends on 1)

The method according to claim 1, further comprising applying heat and pressure to said glass in said mold until said glass sags and deforms into a desired conformation of said optical element.

### Claim 20 (depends on 19)

The method according to claim 19, wherein said pressure is applied mechanically between said first portion driven into said second portion of said mold.

### Claim 21 (depends on 1)

The method according to claim 1, further comprises the step of inserting blocks into the mold.

### Claim 22 (depends on 21)

The method according to claim 21 wherein said blocks are inserted when said glass is in the form of a wafer or powder.

### Claim 23 (depends on 1)

The method according to claim 1, further comprises the step of placing on a molding surface of said blocks a layer of material, which is non-reactive with said glass at the operational temperature.

### Claim 24 (depends on 1)

The method according to claim 1, further comprises the steps of hardening said glass in the mold, removing the glass, and further processing a resultant glass article.

### Claim 25 (depends on 1)

The method according to claim 1, wherein said heating and pressing steps are performed in an ambient air atmosphere.

### Claim 26 (depends on 1)

The method according to claim 1, wherein said optical element has surface features of less than a millimeter.

### Claim 27 (depends on 1)

The method according to claim 1, wherein said optical element has fine microstructures of less than or equal to about 100 microns.

### Claim 28 (depends on 1)

The method according to claim 1, wherein said optical element has hyperfine microstructures of less than or equal to about 10 microns.

### Claim 29 (depends on 1)

The method according to claim 1, wherein said optical element is a lens, microlens, array of lens or microlens, grating, surface relief diffuser, or fresnel lens.

### Claim 30 (depends on 1)

The method according to claim 1, wherein said optical element is part of a forward-looking infrared (FLIR) system.

### Claim 31 (depends on 1)

A precision optical element made according to the method of claim 1.

### Claim 32

A method of making an opto-electronic element, the method comprising:
providing a non-oxide glass having a glass transition temperature (Tg) up to 550° C. as granular, planar, or bulk-solid items; providing a two part mold having an active surface with an optical finish that can be used with or without a protective coating, wherein said active surface is either optionally: (A) coated with a layer of non-reactive material, or (B) made from either a titanium alloy or a nickel alloy, or (C) both made from either a titanium alloy or a nickel alloy and coated with said non-reactive material; charging said mold with said glass, heating said mold to an operational temperature of at least 10° C. above said Tg; and hot-pressing said glass at a viscosity of about 107 to 1012 poise.

### Claim 33 (depends on 32)

The method according to claim 32, wherein said hot-pressing step occurs in an oxygen-containing atmosphere.

### Claim 34 (depends on 32)

The method according to claim 32, wherein said operation temperature does not exceeding about 110° C. above said Tg.

### Claim 35 (depends on 32)

The method according to claim 32, wherein said mold has a metallic active surface absent a protective coating.

### Claim 36 (depends on 32)

The method according to claim 32, wherein at least an active, molding surface is formed of a material selected from: a titanium alloy; nickel alloy; a silicon carbide; a silicon nitride; or a refractory ceramic composite of silicon carbide and silicon nitride.

### Claim 37 (depends on 32)

The method according to claim 32, wherein at least an active, molding surface is formed of a titanium alloy with a composition, in terms of weight percent, comprising about 98-80% Ti, 1-10% Al, and 1-10% V.

### Claim 38 (depends on 32)

The method according to claim 32, wherein said glass is a chalcogenide glass.

### Claim 39 (depends on 38)

The method according to claim 38, wherein said glass is a sulfide glass

### Claim 40 (depends on 38)

The method according to claim 38, wherein said glass is selenide glass.

### Claim 41 (depends on 38)

The method according to claim 38, wherein said glass is a telluride glass.

### Claim 42 (depends on 32)

The method according to claim 32, wherein said glass is a chalcohalide glass.

### Claim 43 (depends on 32)

The method according to claim 32, wherein said glass is a halide glass.

### Claim 44 (depends on 32)

The method according to claim 32, wherein said opto-electronic element has either fine or hyperfine microstructures.

### Claim 45 (depends on 32)

The method according to claim 32, wherein said opto-electronic element is either a lens, microlens, array of lenses or microlenses, diffraction grating, surface relief diffuser, or fresnel lens.

### Claim 46 (depends on 32)

The method according to claim 32, wherein said optical element is part of a forward-looking infrared (FLIR) system.

### Claim 47

A precision optical element comprising: a non-oxide glass body with either fine or hyperfine microstructures formed by a hot-molding or embossing method.

### Claim 48 (depends on 47)

The precision optical element according to claim 47, wherein said optical element is either a lens, microlens, array of lenses or microlenses, diffraction grating, surface relief diffuser, or fresnel lens.

### Claim 49 (depends on 47)

The precision optical element according to claim 47, wherein said optical element is part of a forward-looking infrared (FLIR) system.

### Claim 50 (depends on 47)

The precision optical element according to claim 47, wherein said glass is a chalcogenide glass.

### Claim 51 (depends on 50)

The precision optical element according to claim 50, wherein said glass is a sulfide glass

### Claim 52 (depends on 50)

The precision optical element according to claim 50, wherein said glass is selenide glass.

### Claim 53 (depends on 50)

The precision optical element according to claim 50, wherein said glass is a telluride glass.

### Claim 54 (depends on 47)

The precision optical element according to claim 47, wherein said glass is a chalco-halide glass.

### Claim 55 (depends on 47)

The precision optical element according to claim 47, wherein said glass is a halide glass.

### Claim 56

A precision optical element formed from a non-oxide glass by a molding or embossing method, wherein the method comprises: providing a glass having a glass transition temperature (Tg) up to 550° C. as granular, planar, or bulk-solid items; providing a two part mold having an active surface with an optical finish, which may be used with or without a protective coating, wherein said active surface is either optionally: (A) coated with a layer of non-reactive material, or (B) made from either a titanium alloy or a nickel alloy, or (C) both made from either a titanium alloy or a nickel alloy and coated with said non-reactive material; charging said mold with said glass, heating said mold to an operational temperature of at least 10° C. above said Tg; and hot-pressing said glass.

### Claim 57 (depends on 56)

The precision optical element according to claim 56, wherein said temperature is at least about 50° C. above said Tg.

### Claim 58 (depends on 47)

The precision optical element according to claim 47, wherein the method further comprises inserting blocks into said mold, at least one of said blocks presents a section that faces said wafer or powder.

### Claim 59 (depends on 47)

The precision optical element according to claim 47, the method further comprises placing on a surface of said blocks a layer of non-reactive material that is non-reactive with said glass at said operational temperature.

### Claim 60 (depends on 47)

The precision optical element according to claim 47, wherein said non-reactive material is boron nitride.