# US 2004/0079067 A1 · Oil tempered wire for cold forming coil springs

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0079067 A1
- Document ID: US20040079067A1
- Status: Published application
- Kind: A1
- Application number: 10/385,656
- Filed: 2003-03-12
- Published: 2004-04-29
- Earliest claimed: 2002-03-18
- Assignees: Chuo Hatsujo Kabushiki Kaisha
- Inventors: Hidetoshi Yoshikawa; Tomohiro Nakano; Takayuji Sakakibara; Masami Wakita
- Web page: https://patentgrep.com/patent/US20040079067A1

## CPC

- C21D 8/06: during manufacturing of rods or wires
- C21D 9/525: {for wire, for rods (C21D9/54 takes precedence)}
- C21D 9/60: with induction heating
- C21D 9/02: for springs
- Y02P 10/25: Process efficiency
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

[OBJECT] An oil-tempered wire for a cold-formed coil spring having a quality equivalent of or higher than a hot-formed coil spring is provided. A cold-formed coil spring made from the oil-tempered wire is also provided. [MEANS FOR SOLVING THE PROBLEM] Material used is the steel which contains, in weight percentage, 0.35 to 0.55% C, 1.8 to 3.0% Si, 0.5 to 1.5% Mn, 0.5 to 3.0% Ni, and 0.1 to 1.5% Cr. The ferrite fraction in the microscopic structure of this material is set to 50% or less. Hot rolled wire is cold drawn with a predetermined reduction of area, and a heat treatment using high frequency induction heating is conducted. It is preferable to set the maximum heating temperature between 900° C. to 1020° C. (favorably 950° C.) and the holding time between 5 to 20 seconds. It is preferable to make the oil-tempered material to have the grain size number of 9 or more, and the tensile strength from 1830 to 1980 MPa.

## Claims

### Claim 1

An oil-tempered wire for a cold-formed coil spring characterized by being made from steel comprising, in weight percentage, 0.35 to 0.55% C, 1.8 to 3.0% Si, 0.5 to 1.5% Mn, 0.5 to 3.0% Ni, and 0.1 to 1.5% Cr, and by being heat treated with high frequency induction heating.

### Claim 2 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the material is hot-rolled to a wire with a predetermined diameter, the wire is cold drawn with a predetermined reduction of area, and then the drawn wire is heat treated with a high frequency induction heating.

### Claim 3 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the ferrite fraction in the microscopic structure of the steel before the heat treatment with a high frequency induction heating is 50% or less.

### Claim 4 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the maximum heating temperature in the high frequency induction heating is 1020° C. or lower.

### Claim 5 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the maximum heating temperature in the high frequency induction heating is 950° C. or lower.

### Claim 6 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the maximum heating temperature in the high frequency induction heating is 940° C. or higher.

### Claim 7 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the maximum heating temperature in the high frequency induction heating is 900° C. or higher.

### Claim 8 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein a holding time at the maximum heating temperature in the high frequency induction heating is 5 seconds or more.

### Claim 9 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein a holding time at the maximum heating temperature in the high frequency induction heating is 20 seconds or less.

### Claim 10 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the grain size number after the heat treatment is set to be 9 or more.

### Claim 11 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the tensile strength after the heat treatment is set to be from 1830 to 1980 MPa.

### Claim 12 (depends on 1)

The oil-tempered wire for a cold-formed coil spring according to claim 1, wherein the material further comprises 0.01 to 0.025% N and 0.05 to 0.5% V, and the P content is restricted to 0.01% or less, and the S content is restricted to 0.01% or less.

### Claim 13 (depends on 1)

A cold-formed coil spring made from the oil-tempered wire according to claim 1.