# US 2004/0078900 A1 · Impregnating and bonding agent for textiles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0078900 A1
- Document ID: US20040078900A1
- Status: Published application
- Kind: A1
- Application number: 10/368,169
- Filed: 2003-02-18
- Published: 2004-04-29
- Earliest claimed: 2002-06-03
- Inventors: Ralph Schaefer; Siegfried Wallenwein; Frank Scholl; Johann Wonner
- Web page: https://patentgrep.com/patent/US20040078900A1

## CPC

- D06M 15/39: Aldehyde resins; Ketone resins; Polyacetals
- D06M 15/423: Amino-aldehyde resins
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS

## Abstract

Impregnating and bonding agent for textiles, comprising a mixture of a resorcinol-formaldehyde precondensate A, a rubber latex B and a melamine-formaldehyde resin C, impregnating process and reinforced rubber articles produced using the impregnates.

## Claims

### Claim 1

An impregnating and bonding agent for textiles, comprising a mixture of a resorcinol-formaldehyde precondensate A, a rubber latex B and a melamine-formaldehyde resin C.

### Claim 2 (depends on 1)

An impregnating and bonding agent for textiles as is claimed in claim 1, wherein said resorcinol-formaldehyde precondensate A and said melamine-formaldehyde resin C are present in a mass ratio (each based on solid resin) of 9:1 to 1:9.

### Claim 3 (depends on 1)

An impregnating and bonding agent for textiles as is claimed in claim 1, wherein the ratio of the sum total of the masses (solids fraction in each case) of said resins A and C to the mass of said rubber (solids fraction) in said latex B is 1:1.5 to 1:15.

### Claim 4 (depends on 1)

An impregnating and bonding agent for textiles as is claimed in claim 1, wherein the amount-of-substance ratio in said resorcinol-formaldehyde precondensate A of the building blocks derived from formaldehyde and the building blocks derived from resorcinol is 1:1.05 to 1:2.

### Claim 5 (depends on 1)

An impregnating and bonding agent for textiles as is claimed in claim 1, wherein the amount-of-substance ratio in said melamine-formaldehyde resin C between the building blocks derived from formaldehyde and from melamine is between 1.5:1 to 6:1.

### Claim 6 (depends on 1)

An impregnating and bonding agent for textiles as is claimed in claim 1, wherein said latex B contains a mass fraction of at least 5%, in the solids fraction, of building blocks derived from 2-vinylpyridine.

### Claim 7 (depends on 1)

An impregnating and bonding agent for textiles as is claimed in claim 1, wherein said latex B is a mixture of latices, at least one mass fraction of 10% being present of a latex which contains building blocks derived from vinylpyridine.

### Claim 8 (depends on 1)

A process for producing a textile reinforcement having enhanced adhesion to rubber, which comprises said textile reinforcement being treated with an impregnating and bonding agent as claimed in claim 1 and subsequently dried.

### Claim 9

A rubber article having enhanced adhesion between a textile reinforcement and said rubber, wherein said textile reinforcement has been impregnated with an impregnating and bonding agent comprising a mixture of a resorcinol-formaldehyde precondensate A, a rubber latex B and a melamine-formaldehyde resin C and has been vulcanized with a rubber mixture into a rubber article.