# US 2004/0072985 A1 · Biodegradable polyester polymer and method for preparing the same using compressed gas

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072985 A1
- Document ID: US20040072985A1
- Status: Published application
- Kind: A1
- Application number: 10/682,760
- Filed: 2003-10-08
- Published: 2004-04-15
- Earliest claimed: 2002-10-08
- Assignees: Korea Institute of Science and Technology
- Inventors: Youn-Woo Lee; Soo Hyun Kim; Young Ha Kim; Jong-Sung Lim; Jong Min Park; Ji Won Pack
- Web page: https://patentgrep.com/patent/US20040072985A1

## CPC

- C08G 63/64: Polyesters containing both carboxylic ester groups and carbonate groups
- C08G 63/08: Lactones or lactides
- C08G 63/6882: {derived from hydroxy carboxylic acids}
- C08G 63/81: using solvents (C08G63/79 takes precedence)
- C08G 63/823: {for the preparation of polylactones or polylactides}
- Y02P 20/54: using solvents, e.g. supercritical solvents or ionic liquids
- Y10T 428/2982: Particulate matter [e.g., sphere, flake, etc.]
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

In polymerizing biodegradable polymer material, a compressed gas is used as a reaction solvent for a solution-polymerization, in order to prepare biodegradable polyester homopolymer and copolymer with a high molecular weight in a fine powder form with a particle size of 0.01˜1000 μm.

## Claims

### Claim 1

A method for preparing polyester polymer in a particle form comprising:
adding one or more cyclic monomer in a high pressure reactor;
adding an organic metal catalyst or acid catalyst and an initiator; and
pressurizing and injecting a compressed gas solvent selected from the group consisting of HFC-23, HFC-32, HFC-152a, HFC-143a, HFC-134a, HFC-125, HFC-227ea, HFC-236fa, HFC-245fa, HFC-254cb, SF6, HFC-4-10-mee, C-318 (perfluoro cyclobutane), HCFC-22, HCFC-141b, HCFC-142b, HCFC-225ca/cb, dimethylether, N2O, propane, butane or their mixture, or their mixture with CO2, to solution-polymerize the monomer.

### Claim 2 (depends on 1)

The method of claim 1, additionally comprising the step after polymerization is completed, in which an antisolvent dissolving the reaction solvent but not dissolving the produced polymer to form a single phase is introduced, and thereby the pure polymer is precipitated.

### Claim 3 (depends on 2)

The method of claim 2, wherein the antisolvent is directly introduced into a reaction container.

### Claim 4 (depends on 2)

The method of claim 2, wherein the polymer in the polymerization-completed reaction container is sprayed into a precipitator and the antisolvent is introduced into the precipitator.

### Claim 5 (depends on 2)

The method of claim 2, wherein as the antisolvent, CO2, HFCs, HCFCs, SF6, FCs, hydrocarbon, ether or their mixture is used.

### Claim 6 (depends on 1)

The method of claim 1, wherein as the cyclic monomer, one or more selected from the group consisting of lactides, lactones, cyclic carbonates, cyclic anhydrides and thiolactones are used.

### Claim 7 (depends on 1)

The method of claim 1, wherein as the cyclic monomer, one or more compounds selected from the group consisting of a compound (A) represented by the general formula (I) and a compound (B) represented by the general formula (II) are used:
3
(wherein R1 and R2 are hydrogen atom or alkyl group of C1-C4)
4
(wherein n is an integer of 2 to 5).

### Claim 8 (depends on 7)

The method of claim 7, wherein the compound (A) is L-lactide, D-lactide, D,L-lactide, or glycolide

### Claim 9 (depends on 7)

The method of claim 7, wherein the compound (B) is ε-caprolactone.

### Claim 10 (depends on 1)

The method of claim 1, wherein two or more monomers are used to be co-polymerized.

### Claim 11 (depends on 1)

The method of claim 1, wherein the organic metal catalyst is selected from the group consisting of a tin-based catalyst comprising stannous octoate, stannic chloride, stannous oxide, stannous octylester, stannous chloride dihydrate and tetraphenyl tin; a zinc-based catalyst comprising zinc powder, diethyl zinc, zinc octoate, zinc chloride and zinc oxide; and an aluminum-based catalyst comprising aluminum chloride and aluminum ethoxide

### Claim 12 (depends on 1)

The method of claim 1, wherein the acid catalyst is zinc bis(2,2-dimethyl-3,5-heptanedionato-O,O′).

### Claim 13 (depends on 1)

The method of claim 1, wherein as the initiator, 1,6-hexanediol is used.

### Claim 14 (depends on 1)

The method of claim 1, wherein the compressed gas reaction solvent completely dissolves polymer to perform a uniform solution-polymerization.

### Claim 15 (depends on 1)

The method of claim 1, wherein a reaction temperature is 25 to 250° C.

### Claim 16 (depends on 1)

The method of claim 1, wherein reaction time is 0.2 to 50 hours, and an yield is 70% or higher.

### Claim 17 (depends on 1)

The method of claim 1, wherein a reaction pressure is 40 to 700 bar.

### Claim 18 (depends on 1)

The method of claim 1, wherein the amount of monomer is 1˜50 wt % based on the supercritical fluid.

### Claim 19 (depends on 1)

The method of claim 1, wherein the molar ratio of the catalyst and the initiator is 10−4 to 10−2 based on monomer, respectively.

### Claim 20 (depends on 1)

A biodegradable polyester homopolymer or copolymer polymerized according to the preparation method of claim 1, which has a molecular weight of 2,000 to 1,000,000 g/mol and a particle size of 0.01 to 1,000 μm, and does not include a residual harmful solvent.