# US 2004/0072671 A1 · Sol-gel derived porous microcomposite of perfluorinated ion-exchange polymer and metal oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072671 A1
- Document ID: US20040072671A1
- Status: Published application
- Kind: A1
- Application number: 10/680,334
- Filed: 2003-10-07
- Published: 2004-04-15
- Earliest claimed: 1994-01-12
- Assignees: E. I. Du Pont de Nemours and Company
- Inventors: Mark Andrew Harmer; Qun Sun
- Web page: https://patentgrep.com/patent/US20040072671A1

## CPC

- B01J 21/08: Silica
- B01J 31/10: sulfonated
- B01J 31/165: {Polymer immobilised coordination complexes, e.g. organometallic complexes}
- B01J 31/2419: {comprising P as ring member}
- B01J 31/4007: {of catalysts containing polymers}
- B01J 35/60: characterised by their surface properties or porosity
- C07C 2/02: by addition between unsaturated hydrocarbons
- C07C 2/66: Catalytic processes
- C07C 5/2266: {with hydrides or organic compounds (C07C5/2246 takes precedence)}
- C07C 5/2273: {with ion-exchange resins}
- C07C 5/2562: {with hydrides or organic compounds (C07C5/2543 takes precedence)}
- C07C 41/30: by increasing the number of carbon atoms, e.g. by oligomerisation
- C07C 45/46: Friedel-Crafts reactions
- C07C 67/04: by reacting carboxylic acids or symmetrical anhydrides onto unsaturated carbon-to-carbon bonds
- C07C 201/08: by substitution of hydrogen atoms by nitro groups
- B01J 35/615: {100-500 m2/g}
- B01J 35/617: {500-1000 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/638: {more than 1.0 ml/g}
- B01J 35/643: {less than 2 nm}
- B01J 35/647: {2-50 nm}
- B01J 35/651: {50-500 nm}
- B01J 35/653: {500-1000 nm}
- B01J 35/69: bimodal
- B01J 2231/10: Polymerisation reactions involving at least dual use catalysts, e.g. for both oligomerisation and polymerisation
- B01J 2231/323: Hydrometalation, e.g. bor-, alumin-, silyl-, zirconation or analoguous reactions like carbometalation, hydrocarbation
- B01J 2231/4205: C-C cross-coupling, e.g. metal catalyzed or Friedel-Crafts type
- B01J 2231/52: Isomerisation reactions
- B01J 2231/54: Metathesis reactions, e.g. olefin metathesis
- B01J 2531/38: Lanthanides other than lanthanum
- B01J 2531/821: Ruthenium
- B01J 2531/825: Osmium
- B01J 2531/842: Iron
- B01J 2531/847: Nickel
- C07C 2521/04: Alumina
- C07C 2521/06: Silicon, titanium, zirconium or hafnium; Oxides or hydroxides thereof
- C07C 2521/08: Silica
- C07C 2521/12: Silica and alumina
- C07C 2523/10: of rare earths
- C07C 2523/14: of germanium, tin or lead
- C07C 2523/26: Chromium
- C07C 2523/28: Molybdenum
- C07C 2523/745: Iron
- C07C 2531/08: Ion-exchange resins
- C07C 2531/10: sulfonated
- C07C 2531/20: Carbonyls
- C07C 2531/26: containing in addition, inorganic metal compounds not provided for in groups C07C2531/02 - C07C2531/24
- C07C 2531/34: of chromium, molybdenum or tungsten
- Y02P 20/584: Recycling of catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Porous microcomposites have been prepared from perfluorinated ion-exchange polymer and metal oxides such as silica using the sol-gel process. Such microcomposites possess high surface area and exhibit extremely high catalytic activity.

## Claims

### Claim 1

A porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 2 (depends on 1)

The microcomposite of claim 1 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups.

### Claim 3 (depends on 1)

The microcomposite of claim 1 wherein the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 4 (depends on 1)

The microcomposite of claim 1 wherein the metal oxide is silica.

### Claim 5 (depends on 4)

The microcomposite of claim 4 wherein the perfluoroinated ion-exchange polymer is prepared from resin having an equivalent weight of about 1070 comprising about 6.3 tetrafluoroethylene molecules for every perfluoro(3,6-dioxa-4-methyl-7-octenesulfonyl fluoride) molecule, and the weight percent of perfluorinated ion-exchange polymer is about 13%.

### Claim 6 (depends on 1)

The microcomposite of claim 1 wherein the weight percentage of perfluorinated ion-exchange polymer is from about 5 to about 80.

### Claim 7 (depends on 1)

The microcomposite of claim 1 wherein the size of the pores is about 0.5 nm to about 30 nm.

### Claim 8 (depends on 1)

The microcomposite of claim 1 wherein said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 9 (depends on 8)

The microcomposite of claim 8 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups, and wherein the metal oxide is silica.

### Claim 10

The process of preparation of a porous microcomposite which comprises perfluorinated ion-exchange polymer containing pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm;
said process comprising the steps of:
a. mixing the perfluorinated ion-exchange polymer with one or more metal oxide precursors in a common solvent;
b. initiating gelation;
c. allowing sufficient time for gelation and aging of the mixture; and
d. removing the solvent.

### Claim 11 (depends on 10)

The process of claim 10 further comprising the steps, after d:
e. acidifying the product of step d by addition of an acid; and
f. removing the excess acid.

### Claim 12 (depends on 11)

The process of claim 11 further comprising at step a, adding to the mixture an amount from about 1 to 80 weight percent of an acid extractable filler particle, whereby said microcomposite further contains pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 13 (depends on 12)

The process of claim 12 wherein the acid extractable filler particle is calcium carbonate.

### Claim 14 (depends on 10)

The process of claim 10 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups.

### Claim 15 (depends on 10)

The process of claim 10 wherein the metal oxide is silica.

### Claim 16 (depends on 11)

The process of claim 11 further comprising after step d and before step e: grinding the product of step d.

### Claim 17

An improved process for the nitration of an aromatic compound wherein the improvement comprises contacting said aromatic compound with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 18 (depends on 17)

The process of claim 17 wherein the aromatic compound is benzene.

### Claim 19 (depends on 17)

The process of claim 17 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 20 (depends on 19)

The process of claim 19 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 21

An improved process for the esterification of a carboxylic acid with an olefin wherein the improvement comprises contacting said carboxylic acid with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 22 (depends on 21)

The process of claim 21 wherein the carboxylic acid is acetic acid and the olefin is cyclohexene.

### Claim 23 (depends on 21)

The process of claim 21 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 24 (depends on 23)

The process of claim 23 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 25

A process for regenerating a catalyst comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 1 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm, comprising the steps of:
(a) contacting the microcomposite with an acid; and
(b) removing the excess acid to yield the regenerated catalyst.

### Claim 26 (depends on 25)

The process of claim 25 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 27 (depends on 26)

The process of claim 26 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 28

An improved process for the dimerization of an alpha substituted styrene wherein the improvement comprises contacting said alpha substituted sytrene with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 1 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 29 (depends on 28)

The process of claim 28 wherein the alpha substituted styrene is alpha methyl styrene.

### Claim 30 (depends on 28)

The process of claim 28 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 31 (depends on 30)

The process of claim 30 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 32

An improved process for the alkylation of an aromatic compound with an olefin wherein the improvement comprises contacting said aromatic compound with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 1 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 33 (depends on 32)

The process of claim 32 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 34 (depends on 33)

The process of claim 33 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 35

An improved process for the polymerization of tetrahydrofuran to polytetramethylene ether acetate wherein the improvement comprises contacting said tetrahydrofuran with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 36 (depends on 35)

The process of claim 35 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 37 (depends on 36)

The process of claim 36 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 38

An improved process for the acylation of an aromatic compound with an acyl halide wherein the improvement comprises contacting said aromatic compound with a catalytic porous microcomposite comprising perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 39 (depends on 38)

The process of claim 38 wherein the aromatic compound is m-xylene and the acyl halide is benzoyl chloride.

### Claim 40 (depends on 38)

The process of claim 38 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups and the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 41 (depends on 40)

The process of claim 40 wherein the metal oxide is silica and said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 42

A process for the isomerization of an olefin, comprising contacting said olefin at isomerization conditions with a catalytic amount of a porous microcomposite, said microcomposite comprising a perfluorinated ion-exchange polymer with pendant sulfonic and/or carboxylic acid groups entrapped within and highly dispersed throughout a network of metal oxide, wherein the weight percentage of perfluorinated ion-exchange polymer in the microcomposite is from about 0.1 to about 90 percent, wherein the size of the pores in the microcomposite is about 0.5 nm to about 75 nm, and wherein the microcomposite optionally further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 43 (depends on 42)

The process of claim 42 wherein the isomerization conditions comprise a temperature of from about 0° C. to about 300° C., a pressure of from about atmospheric to 100 atmospheres, and a weight hourly space velocity of from about 0.1 to 100 hr−1.

### Claim 44 (depends on 43)

The process of claim 43 wherein the isomerization conditions comprise a temperature of from about 25° C. to about 250° C., a pressure of from about atmospheric to 50 atmospheres, and a weight hourly space velocity of from about 0.1 to 10 hr−1.

### Claim 45 (depends on 42)

The process of claim 42 wherein the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups.

### Claim 46 (depends on 42)

The process of claim 42 wherein the metal oxide is silica, alumina, titania, germania, zirconia, alumino-silicate, zirconyl-silicate, chromic oxide and/or iron oxide.

### Claim 47 (depends on 45)

The process of claim 45 wherein the metal oxide is silica.

### Claim 48 (depends on 42)

The process of claim 42 wherein the weight percentage of perfluorinated ion-exchange polymer is from about 5 to about 80.

### Claim 49 (depends on 48)

The process of claim 48 wherein the weight percentage of perfluorinated ion-exchange polymer is from about 5 to about 20.

### Claim 50 (depends on 42)

The process of claim 42 wherein the size of the pores is about 0.5 nm to about 30 nm.

### Claim 51 (depends on 42)

The process of claim 42 wherein said microcomposite further comprises pores having a size in the range of about 75 nm to about 1000 nm.

### Claim 52 (depends on 42)

The process of claim 42 wherein the olefin is a C4 to C40 primary olefin.

### Claim 53 (depends on 52)

The process of claim 52 wherein the olefin is 1-butene, 1-heptene or 1-dodecene.

### Claim 54 (depends on 53)

The process of claim 53 wherein the olefin is 1-butene.

### Claim 55 (depends on 53)

The process of claim 53 wherein the weight percentage of perfluorinated ion-exchange polymer is from about 5 to about 80, the perfluorinated ion-exchange polymer contains pendant sulfonic acid groups, and the metal oxide is silica.

### Claim 56 (depends on 53)

The process of claim 53 wherein the perfluorinated ion-exchange polymer is prepared from resin having an equivalent weight of about 1070 comprising about 6.3 tetrafluoroethylene molecules for every perfluoro (3,6-dioxa4-methyl-7-octenesulfonyl fluoride) molecule, and the weight percent of perfluorinated ion-exchange polymer is about 13%.