# US 2004/0072669 A1 · Forsterite glass-ceramics of high crystallinity and chrome content

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072669 A1
- Document ID: US20040072669A1
- Status: Published application
- Kind: A1
- Application number: 10/674,855
- Filed: 2003-09-30
- Published: 2004-04-15
- Earliest claimed: 2001-08-14
- Assignees: Corning Incorporated
- Inventors: George H. Beall; Joseph E. Pierson; Linda R. Pinckney
- Web page: https://patentgrep.com/patent/US20040072669A1

## CPC

- C03C 13/046: {Multicomponent glass compositions}
- C03C 4/0071: {for laserable glass}
- C03C 10/0045: {containing SiO2, Al2O3 and MgO as main constituents}
- H01S 3/162: {transition metal}
- H01S 3/1623: {chromium, e.g. Alexandrite}
- H01S 3/1658: {Mg2SiO4 (Forsterite)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL

## Abstract

A composition for a glass-ceramic material that contains a crystallinity of at least about 30% by weight of forsterite components at a liquidus temperature of about 1525 ° C. or below. The glass-ceramic has a composition, in weight percent on an oxide basis, consisting essentially of about: 40-60% SiO2; 10-25% Al2O3; 18-30% MgO; 3-10% Na2O; 0-10% K2O; >5-15% TiO2. The invention further comprises a method for achieving high crystalline yield at such a low liquidus with increased solubility of high levels of chromium ions. The glass-ceramics can be used in drawing optical fibers and as gain media in amplifier and laser devices for near infrared wavelengths.

## Claims

### Claim 1

A transparent glass-ceramic containing a predominant crystal phase of forsterite, the glass-ceramic having a composition, in weight percent on an oxide basis, consisting essentially of about:
40-60% SiO2;
10-25% Al2O3;
18-30% MgO;
3-10% Na2O;
0-10% K2O;
>5-15% TiO2; and
said glass-ceramic has a crystallinity of at least about 30% by weight of forsterite components at a liquidus temperature of about 1525° C. or below.

### Claim 2 (depends on 1)

The glass-ceramic according to claim 1, wherein Na2O and K2O are both present in about a 1:1 molar ratio.

### Claim 3 (depends on 1)

The glass-ceramic according to claim 1, wherein said TiO2 content by weight in said composition is greater than about 6%, and less than about 9%.

### Claim 4 (depends on 1)

The glass-ceramic according to claim 1, wherein said composition further includes, in weight percent on an oxide basis, up to about 1.3% chromium oxide.

### Claim 5 (depends on 4)

The glass-ceramic according to claim 4, wherein said composition includes, in weight percent on an oxide basis, about 0.05% to about 0.75% chromium oxide.

### Claim 6 (depends on 1)

The glass-ceramic according to claim 1, wherein said composition further includes, in weight percent on an oxide basis, up to about 20% GeO2.

### Claim 7 (depends on 1)

The glass-ceramic according to claim 1, wherein said composition includes a transition metal ion selected from the group consisting of Ni2+, V3+, Co2+, Cr4+, Cu2+, Cu1+, Mn2+, Fe2+, and Ti3+.

### Claim 8 (depends on 1)

The glass-ceramic according to claim 1, wherein said crystallinity is about 35% or more by weight of forsterite components.

### Claim 9 (depends on 1)

The glass-ceramic according to claim 1, wherein crystals in the crystal phase have a size no larger than about 60 nm.

### Claim 10 (depends on 1)

The glass-ceramic according to claim 1, wherein crystals in the crystal phase have a size between about 10 nm to about 35 nm.

### Claim 11

A transparent glass-ceramic with a crystallinity of at least about 30% by weight of forsterite components at a liquidus temperature of about 1525° C. or below, having a composition, in weight percent on an oxide basis, consisting essentially of about:
43-55% SiO2;
11-16% Al2O3;
20-26% MgO;
3.5-6.5% Na2O;
3.0-8.0% K2O;
5.5-9.0% TiO2.

### Claim 12 (depends on 11)

The glass-ceramic according to claim 11, wherein Na2O and K2O are both present in about a 1:1 molar ratio.

### Claim 13 (depends on 11)

The glass-ceramic according to claim 11, wherein said TiO2 content by weight in said composition is greater than about 6%, and less than about 9%.

### Claim 14 (depends on 11)

The glass-ceramic according to claim 11, wherein said composition further includes, in weight percent on an oxide basis, up to about 1.3% chromium oxide.

### Claim 15 (depends on 14)

The glass-ceramic according to claim 14, wherein said composition includes, in weight percent on an oxide basis, about 0.05% to about 0.7% chromium oxide.

### Claim 16 (depends on 11)

The glass-ceramic according to claim 11, wherein said composition further includes, in weight percent on an oxide basis, up to about 20% GeO2.

### Claim 17 (depends on 11)

The glass-ceramic according to claim 11, wherein said composition includes a transition metal ion selected from the group consisting of Ni2+, V3+, Co2+, Cu2+, Cu1+, Mn2+, Fe2+and Ti3+.

### Claim 18 (depends on 11)

The glass-ceramic according to claim 11, wherein said crystallinity is about 35% or more by weight of forsterite components.

### Claim 19 (depends on 11)

The glass-ceramic according to claim 11, wherein crystals in the crystal phase have a size no larger than about 60 nm.

### Claim 20 (depends on 11)

The glass-ceramic according to claim 11, wherein crystals in the crystal phase have a size between about 10 nm to about 35 nm.

### Claim 21

A method of dissolving at least 30% by weight of forsterite component in a glass-ceramic, the method comprising:
providing a R2O—MgO—Al2O3—SiO2 glass composition, wherein R is an alkali ion, containing, in weight percent, at least about 3% of Na2O coupled with greater than 5% of TiO2;
melting said glass at a temperature between about 1575° C. to about 1650° C.

### Claim 22 (depends on 21)

The method according to claim 21, wherein said glass has a composition, in weight percent on an oxide basis, consisting essentially of about: 40-60% SiO2; 10-25% Al2O3; 18-30% MgO; 3-10% Na2O; 0-10% K2O; >5-15% TiO2.

### Claim 23 (depends on 21)

The method according to claim 21, further comprising achieving at least 30% by weight of forsterite component in said glass-ceramic at a liquidus temperature of about 1525° C. or below.

### Claim 24 (depends on 22)

The method according to claim 22, wherein Na2O and K2O are both present in about a 1:1 molar ratio.

### Claim 25 (depends on 22)

The method according to claim 22, wherein said TiO2 content by weight in said composition is greater than about 6%, and less than about 9%.

### Claim 26 (depends on 22)

The method according to claim 22, wherein said composition further includes, in weight percent on an oxide basis, up to about 1.3% chromium oxide.

### Claim 27 (depends on 26)

The method according to claim 26, wherein said composition includes, in weight percent on an oxide basis, about 0.05% to about 0.7% chromium oxide.

### Claim 28 (depends on 22)

The method according to claim 22, wherein said composition further includes, in weight percent on an oxide basis, up to about 20% GeO2.

### Claim 29 (depends on 22)

The method according to claim 22, wherein said composition includes a transition metal ion selected from the group consisting of Ni2+, V3+, Co2+, Cr4+, Cu2+, Cu1+, Mn2+, Fe2+, and Ti3+.

### Claim 30 (depends on 22)

The method according to claim 22, wherein said crystallinity is about 35% or more by weight of forsterite components.

### Claim 31 (depends on 22)

The method according to claim 22, wherein crystals in the crystal phase have a size no larger than about 60 nm.

### Claim 32 (depends on 22)

The method according to claim 22, wherein crystals in the crystal phase have a size between about 10 nm to about 35 nm.

### Claim 33

An optical element selected from the group consisting of an optical fiber, a gain-medium, a laser, and an amplifier, said element comprising: a transparent glass-ceramic containing a crystallinity of at least about 30% by weight of forsterite component at a liquidus temperature of about ≦1525° C.±5° C. or below, the glass-ceramic having a composition,. in weight percent on an oxide basis, consisting essentially of about: 40-60% SiO2; 10-25% Al2O3; 18-30% MgO; 3-10% Na2O; 0-10% K2O; and >5-15% TiO2.

### Claim 34 (depends on 33)

The optical element according to claim 33, wherein Na2O and K2O are both present in about a 1:1 molar ratio.

### Claim 35 (depends on 33)

The optical element according to claim 33, wherein said TiO2 content by weight in said composition is greater than about 6%, and less than about 9%.

### Claim 36 (depends on 33)

The optical element according to claim 33, wherein said composition further includes, in weight percent on an oxide basis, up to about 1.3% chromium oxide.

### Claim 37 (depends on 36)

The optical element according to claim 36, wherein said composition includes, in weight percent on an oxide basis, about 0.05% to about 0.7% chromium oxide.

### Claim 38 (depends on 33)

The optical element according to claim 33, wherein said composition further includes, in weight percent on an oxide basis, up to about 20% GeO2.

### Claim 39 (depends on 33)

The optical element according to claim 33, wherein said composition includes a transition metal ion selected from the group consisting of Ni2+, V3+, Co2+, Cr4+, Cu2+, Cu1+, Mn2+, Fe2+, and Ti3+.

### Claim 40 (depends on 33)

The optical element according to claim 33, wherein said crystallinity is about 35% or more by weight of forsterite components.

### Claim 41 (depends on 33)

The optical element according to claim 33, wherein crystals in the crystal phase have a size no larger than about 50 mn.

### Claim 42 (depends on 33)

The optical element according to claim 33, wherein crystals in the crystal phase have a size between about 10 nm to about 35 nm.