# US 2004/0072435 A1 · Method of integrating L - shaped spacers in a high performance CMOS process via use of an oxide - nitride - doped oxide spacer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072435 A1
- Document ID: US20040072435A1
- Status: Published application
- Kind: A1
- Application number: 10/267,206
- Filed: 2002-10-09
- Published: 2004-04-15
- Earliest claimed: 2002-10-09
- Assignees: Chartered Semiconductor Manufacturing Ltd.
- Inventors: Elgin Quek
- Web page: https://patentgrep.com/patent/US20040072435A1

## CPC

- H10D 30/0229: {forming drain regions and lightly-doped drain [LDD] simultaneously, e.g. using implantation through a T-shaped mask}
- H10D 30/0227: {having both lightly-doped source and drain extensions and source and drain regions self-aligned to the sides of the gate, e.g. lightly-doped drain [LDD] MOSFET or double-diffused drain [DDD] MOSFET}
- H10D 30/601: {having lightly-doped drain or source extensions, e.g. LDD IGFETs or DDD IGFETs (lightly doped source or drain extensions for TFTs H10D30/6715)}
- H10D 64/015: {removing at least parts of gate spacers, e.g. disposable spacers}
- H10D 84/0184: {Manufacturing their gate sidewall spacers}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 30/0212: {using self-aligned silicidation}
- H10D 64/021: {using multiple gate spacer layers, e.g. bilayered sidewall spacers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A process for fabricating a complimentary metal oxide semiconductor (CMOS), device featuring composite insulator spacer shapes which allow P channel (PMOS), short channel effects to be minimized, and allow reductions in resistance for N channel (NMOS), source/drain extension regions to be realized, has been developed. The process features initial composite insulator spacers formed in the sides of gate structures after definition of the NMOS and PMOS source/drain extension regions. The initial composite insulator spacer, comprised of an underlying silicon oxide component, an L-shaped silicon nitride component, and an overlying doped oxide component, is then used for definition of the PMOS heavily doped source/drain region, allowing for adequate space between the heavily doped source/drain and channel regions, thus reducing the risk of short channel effects. After removal of the doped oxide component, the L-shaped composite insulator spacer is used to define, via ion implantation procedures, an NMOS heavily doped region, featuring a portion of the heavily doped source/drain region formed underlying a horizontal feature of the L-shaped silicon nitride component, therefore compensating a portion of the NMOS source/drain extension region, and resulting in the desired reduction in source/drain resistance.

## Claims

### Claim 1

A method of forming a complimentary metal oxide semiconductor (CMOS), device on a semiconductor substrate, comprising the steps of:
providing a first gate structure on an underlying gate insulator layer, located in a first region of said semiconductor substrate to be used for an N channel metal oxide semiconductor (NMOS), element of said CMOS device, and providing a second gate structure on said underlying gate insulator layer, located in a second region of said semiconductor substrate to be used for a P channel metal oxide semiconductor (PMOS), element of said CMOS device;
forming an N type, source/drain extension (SDE), region in a portion of said first region of said semiconductor substrate not covered by said first gate structure;
forming a P type, source/drain extension (SDE), region in a portion of said second region of said semiconductor substrate not covered by said second gate structure;
depositing a composite insulator layer comprised of an underlying silicon oxide layer, a silicon nitride layer, and an overlying doped oxide layer;
performing an anisotropic dry etch procedure to form a first composite insulator spacer comprised of an overlying doped oxide component, an L-shaped silicon nitride component, and an underlying L-shaped silicon oxide component, on the sides of said first gate structure, and to form a second composite insulator shape comprised of an overlying doped oxide component, an L-shaped silicon nitride component, and an underlying L-shaped silicon oxide component, on the sides of said second gate structure;
forming a heavily doped P type source/drain region in a portion of said second region of said semiconductor substrate not covered by said second gate structure, or by said second composite insulator spacer;
removing said doped oxide components resulting in a first L-shaped composite insulator spacer located on the sides of said first gate structure, and resulting in a second L-shaped composite insulator spacer located on the sides of said second gate structure;
forming a first heavily doped N type source/drain region in a portion of said first region of said semiconductor substrate not covered by said first gate structure or by said first L-shaped composite spacer, and forming a second heavily doped N type source/drain region in a portion of said first region of said semiconductor substrate, directly underlying horizontal feature of said L-shaped silicon nitride component of said first L-shaped composite insulator spacer; and
forming metal silicide layers on the top surface of said first gate structure, on the top surface of said second gate structure, on the top surface of said first heavily doped N type source/drain region, and on the top surface of said heavily doped P type source/drain region.

### Claim 2 (depends on 1)

The method of claim 1, wherein said gate insulator layer is a silicon dioxide layer, obtained via thermal oxidation procedures at a thickness between about 12 to 25 Angstroms.

### Claim 3 (depends on 1)

The method of claim 1, wherein said gate structures are polysilicon gate structures, defined from a polysilicon layer which in turn is obtained via LPCVD procedures at thickness between about 1200 to 2000 Angstroms, either deposited intrinsically than doped either N type, or P type, via ion implantation procedures, or in situ doped during deposition via the addition of arsine, or phosphine, to a silane ambient.

### Claim 4 (depends on 1)

The method of claim 1, wherein said N type SDE region is formed via implantation of arsenic or phosphorous ions at an energy between about 1 to 5 KeV, at a dose between about 5E14 to 2E15 atoms/cm2.

### Claim 5 (depends on 1)

The method of claim 1, wherein said P type SDE region is formed via implantation of boron ions at an energy between about 0.4 to 1 KeV, at a dose between about 1E14 to 1.5E15 atoms/cm.

### Claim 6 (depends on 1)

The method of claim 1, wherein said underlying silicon oxide layer of said composite insulator layer, is obtained via LPCVD or PECVD procedures, at a thickness between about 50 to 150 Angstroms.

### Claim 7 (depends on 1)

The method of claim 1, wherein said silicon nitride layer of said composite insulator layer, is obtained via LPCVD or PECVD procedures, at a thickness between about 150 to 350 Angstroms.

### Claim 8 (depends on 1)

The method of claim 1, wherein said doped oxide layer of said composite insulator layer, is a phosphosilicate glass (PSG) layer, obtained via PECVD procedures at a thickness between about 450 to 700 Angstroms, and comprised with a weight percent of phosphorous between about 3 to 5.

### Claim 9 (depends on 1)

The method of claim 1, wherein said anisotropic dry etch procedure used to define the composite insulator spacers, is an anisotropic reactive ion etch (RIE), procedure, performed using CHF3 as an etchant for said doped oxide layer and for said underlying silicon oxide layer, and using Cl2 or CF4 as an etchant for said silicon nitride layer.

### Claim 10 (depends on 1)

The method of claim 1, wherein said heavily doped P type source/drain region is formed via implantation of boron ions at an energy between about 3 to 6 KeV, at a dose between about 2E15 to 5E15 atoms/cm2.

### Claim 11 (depends on 1)

The method of claim 1, wherein said doped oxide components of the composite insulator spacers, are removed using buffered hydrofluoric (BHF) acid, or a dilute hydrofluoric (DHF) acid, with an etch rate ratio of said doped oxide component to silicon oxide, between about 10 to 1, to 15 to 1.

### Claim 12 (depends on 1)

The method of claim 1, wherein said first heavily doped N type source/drain region is formed via implantation of arsenic at an energy between about 35 to 65 KeV, at a dose between about 2E15 to 6E15 atoms/cm2.

### Claim 13 (depends on 1)

The method of claim 1, wherein said second heavily doped N type source/drain region is formed via identical implantation procedure used to form said first heavily doped N type source/drain region, via implantation of arsenic at an energy between about 35 to 65 KeV, at a dose between about 2E15 to 6E15 atoms/cm2, however formed only in a portion of said first region of said semiconductor substrate located directly underlying said horizontal feature of said L-shaped, silicon nitride component.

### Claim 14 (depends on 1)

The method of claim 1, wherein said metal silicide layer is comprised of either titanium silicide, nickel silicide, or cobalt silicide.

### Claim 15

A method of forming a complimentary metal oxide semiconductor (CMOS), device on a semiconductor substrate, featuring a composite insulator spacer used as a mask to define an implanted P channel metal oxide semiconductor (PMOS), source/drain region, followed by the use of a partially etched, L shape composite insulator spacer as a mask to define an implanted N channel metal oxide semiconductor (NMOS), source/drain region, comprising the steps of:
providing a first region of said semiconductor substrate to be used as an NMOS region, and providing a second region of said semiconductor substrate to be used as a PMOS region;
forming a shallow trench isolation (STI), region, in a portion of said semiconductor located between said NMOS region and said PMOS region, with said STI region filled with a first silicon oxide layer;
forming an N well region in said PMOS region;
growing a silicon dioxide gate insulator layer on portions of said semiconductor substrate not occupied by said STI region;
forming a first polysilicon gate structure on a first portion of said underlying silicon dioxide gate insulator layer, located in said NMOS region, and forming a second polysilicon gate structure on a second portion of said underlying silicon dioxide gate insulator layer, located in said PMOS region;
performing a first ion implantation procedure to form an N type, source/drain extension (SDE), region in a portion of said NMOS region not covered by said first polysilicon gate structure;
performing a second ion implantation procedure to form a P type, source/drain extension (SDE), region in a portion of said PMOS region not covered by said second polysilicon gate structure;
depositing a composite insulator layer comprised of an underlying, second silicon oxide layer, a silicon nitride layer, and an overlying doped oxide layer;
performing an anisotropic reactive ion etching (RIE) procedure to form a first composite insulator spacer on the sides of said first polysilicon gate structure, with said first composite insulator spacer comprised of an overlying doped oxide component, an L-shaped silicon nitride component, and an underlying L-shaped silicon oxide component, and to form a second composite insulator shape on the sides of said second polysilicon gate structure, with said second composite insulator spacer comprised of an overlying doped oxide component, an L-shaped silicon nitride component, and an underlying L-shaped silicon oxide component;
performing a third ion implantation procedure to form a heavily doped P type source/drain region in a portion of said PMOS region not covered by said second polysilicon gate structure, or by said second composite insulator spacer;
performing a wet etch procedure to remove said doped oxide components, resulting in a first L-shaped composite insulator spacer located on the sides of said first polysilicon gate structure, and resulting in a second L-shaped composite insulator spacer located on the sides of said second polysilicon gate structure;
performing a fourth ion implantation procedure to form a first heavily doped N type source/drain region in a portion of said NMOS region not covered by said first polysilicon gate structure or by said first L-shaped composite spacer, and forming a second heavily doped N type source/drain region in a portion of said NMOS region, directly underlying horizontal feature of said L-shaped silicon nitride component of said first L-shaped composite insulator spacer, with said second heavily doped N type source/drain region located shallower in said semiconductor substrate than said first heavily doped N type source/drain region; and
forming metal silicide layers on the top surface of said first polysilicon gate structure, on the top surface of said second polysilicon gate structure, on the top surface of said first heavily doped N type source/drain region, and on the top surface of said heavily doped P type source/drain region.

### Claim 16 (depends on 15)

The method of claim 15, wherein said first silicon oxide layer, located in said STI region, is an undoped silicon oxide layer, obtained via LPCVD or PECVD procedures using tetraethylorthosilicate (TEOS), as a source.

### Claim 17 (depends on 15)

The method of claim 15, wherein said silicon dioxide gate insulator layer is obtained via thermal oxidation procedures at a thickness between about 12 to 25 Angstroms.

### Claim 18 (depends on 15)

The method of claim 15, wherein said first polysilicon gate structure and said second polysilicon gate structure, are defined from a polysilicon layer which in turn is obtained via LPCVD procedures, at thickness between about 1200 to 2000 Angstroms, either deposited intrinsically and than doped either N type, or P type, via ion implantation procedures, or doped in situ during deposition via the addition of arsine, or phosphine, to a silane ambient.

### Claim 19 (depends on 15)

The method of claim 15, wherein said first ion implantation procedure, used to form said N type SDE region, is performed using arsenic or phosphorous ions at an energy between about 1 to 5 KeV, at a dose between about 5E14 to 2E15 atoms/cm2.

### Claim 20 (depends on 15)

The method of claim 15, wherein said second ion implantation procedure, used to form said P type SDE region, is performed using boron ions at an energy between about 0.4 to 1 KeV, at a dose between about 1E14 to 1.5E15 ______ atoms/cm2.

### Claim 21 (depends on 15)

The method of claim 15, wherein said underlying, second silicon oxide layer is obtained via LPCVD or PECVD procedures, at a thickness between about 50 to 150 Angstroms.

### Claim 22 (depends on 15)

The method of claim 15, wherein said silicon nitride layer is obtained via LPCVD or PECVD procedures, at a thickness between about 150 to 350 Angstroms.

### Claim 23 (depends on 15)

The method of claim 15, wherein said doped oxide layer is a phosphosilicate glass (PSG) layer, obtained via PECVD procedures at a thickness between about 450 to 700 Angstroms, and comprised with a weight percent of phosphorous between about 3 to 5.

### Claim 24 (depends on 15)

The method of claim 15, wherein said anisotropic RIE procedure used to define said first composite insulator spacer and said second composite insulator spacer, is performed using CHF3 as an etchant for said doped oxide layer and for said underlying, second silicon oxide layer, while using Cl2 or CF4 as an etchant for said silicon nitride layer.

### Claim 25 (depends on 15)

The method of claim 15, wherein said third ion implantation procedure, used to form said heavily doped P type source/drain region, is performed using boron ions at an energy between about 3 to 6 KeV, at a dose between about 2E15 to SE15 atoms/cm2.

### Claim 26 (depends on 15)

The method of claim 15, wherein said wet etch procedure, used to remove said doped oxide components of the composite insulator spacers, is performed using a buffered hydrofluoric (BHF) acid, or a dilute hydrofluoric (DHF) acid solution, with an etch rate ratio of said doped oxide component to said first silicon oxide layer, located in said STI region, between about 10 to 1, to 15 to 1.

### Claim 27 (depends on 15)

The method of claim 15, wherein said fourth ion implantation procedure, used to form said first heavily doped N type source/drain region, and to form said second heavily doped N type source/drain region, is performed using arsenic ions at an energy between about 35 to 65 KeV, at a dose between about 2E15 to 6E15 atoms/cm2.

### Claim 28 (depends on 15)

The method of claim 15, wherein said metal silicide layer is comprised of either titanium suicide, nickel silicide, or cobalt silicide.