# US 2004/0072431 A1 · Method for fabricating semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072431 A1
- Document ID: US20040072431A1
- Status: Published application
- Kind: A1
- Application number: 10/679,377
- Filed: 2003-10-07
- Published: 2004-04-15
- Earliest claimed: 2002-10-08
- Assignees: Hynix Semiconductor Inc.
- Inventors: Dong Suk Shin
- Web page: https://patentgrep.com/patent/US20040072431A1

## CPC

- H10P 70/234: {the processing being the formation of vias or contact holes}
- H10P 50/283: {by chemical means}
- H10W 20/081: {by forming openings in the dielectric parts}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for fabricating a semiconductor device wherein the lower portion of a contact hole is cleaned, and doped with an impurity for reducing contact resistance is disclosed. The method comprises: sequentially forming a buffer layer and an interlayer insulating film on a semiconductor substrate; etching the interlayer insulating film and the buffer layer to form a contact hole exposing the semiconductor substrate; performing a cleaning process of a lower portion of the contact hole; doping an impurity into the surface of the semiconductor substrate exposed by the contact hole; and forming a conductive layer filling the contact hole on the entire surface of the resulting structure.

## Claims

### Claim 1

A method for fabricating a semiconductor device, comprising the steps of:
sequentially forming a buffer layer and an interlayer insulating film on a semiconductor substrate;
etching the interlayer insulating film and the buffer layer to form a contact hole exposing the semiconductor substrate;
performing a cleaning process of a lower portion of the contact hole;
doping an impurity into the surface of the semiconductor substrate exposed by the contact hole; and
forming a conductive layer filling the contact hole on the entire surface of the resulting structure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the buffer layer comprises a nitride film.

### Claim 3 (depends on 1)

The method of claim 1, wherein the interlayer insulating film comprises an oxide film.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cleaning process comprises sequentially performing a dry cleaning process for removing a portion damaged during the contact hole etching process, and a wet cleaning process for removing carbon composite residues and a native oxide film.

### Claim 5 (depends on 4)

The method of claim 4, wherein the dry cleaning process is performed using a plasma of mixture gas of NH3, O2, HE and N2 for 1 to 5 minutes with a bias power ranging from 1 to 10 kW in the direction of the semiconductor substrate.

### Claim 6 (depends on 4)

The method of claim 4, wherein the dry cleaning process is performed using a plasma of mixture gas of NH3 and N2, and the resulting structure is further subjecting to an annealing process for 1 to 10 minutes at a temperature ranging from 100 to 500° C.

### Claim 7 (depends on 4)

The method of claim 4, wherein the wet cleaning process is performed using a solution selected from the group consisting of H2O2, H2SO4, NH4OH, HF, BOE solutions, and combinations thereof as a cleaning solution.

### Claim 8 (depends on 1)

The method of claim 1, wherein the step of doping an impurity into the surface of the semiconductor substrate is performed by ion-implanting an impurity into the lower portion of the contact hole;

### Claim 9 (depends on 8)

The method of claim 8, wherein the ion-implanting process is performed by implanting P or As having a dose ranging from 1E10 to 1E20 atoms/cm2 with an implantation energy ranging from 10 to 100 keV.

### Claim 10 (depends on 8)

The method of claim 8, wherein the ion-implanting process further comprises exposing the surface of the semiconductor substrate exposed by the contact hole to a PH3/N2 gas atmosphere to diffuse P into the exposed the semiconductor substrate.

### Claim 11 (depends on 10)

The method of claim 10, wherein the surface of the semiconductor substrate is exposed to PH3/N2 gas atmosphere for 5 to 60 minutes under a pressure ranging from 0.1 to 10 Torr and at a temperature ranging from 400 to 700° C.

### Claim 12 (depends on 1)

The method of claim 1, wherein the conductive layer consists of a polysilicon layer formed in a low pressure chemical vapor deposition process using a mixture gas of mono silane (MS), PH3 and N2 as a reaction gas under a pressure ranging from 0.1 to 10 Torr and at a temperature ranging from 400 to 700° C.

### Claim 13 (depends on 12)

The method of claim 12, wherein the flow rate of mono silane ranges from 500 to 5000 sccm.

### Claim 14 (depends on 12)

The method of claim 12, wherein the flow rate of N2 ranges from 100 to 5000 sccm.

### Claim 15 (depends on 12)

The method of claim 12, wherein the H2 gas contains 1% of PH3 gas and has a flow rate ranging from 10 to 1000 sccm.

### Claim 16 (depends on 1)

The method of claim 1, wherein a thickness of the conductive layer ranges from 1000 to 5000 Å.

### Claim 17 (depends on 1)

The method of claim 1, wherein the conductive layer consists of a polysilicon layer having 1.0E19 to 3.0E20 atoms/cc of P therein.

### Claim 18 (depends on 1)

The method of claim 1, wherein the impurity concentration of the conductive layer from the contact interface to a height ranging from 50 to 500 Å ranges from 1.5E20 to 3.0E20 atoms/cc