# US 2004/0072387 A1 · Method of fabricating and mounting flip chips

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072387 A1
- Document ID: US20040072387A1
- Status: Published application
- Kind: A1
- Application number: 10/372,280
- Filed: 2003-02-25
- Published: 2004-04-15
- Earliest claimed: 2002-10-12
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Soon-Min Hong; Young-Jun Moon; Min-Young Park; Sea-Gwang Choi
- Web page: https://patentgrep.com/patent/US20040072387A1

## CPC

- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/90: Bond pads, in general
- H10W 72/07251: {characterised by changes in properties of the bump connectors during connecting}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/251: {Materials}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/29: Bond pads specially adapted therefor
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating and mounting a flip chip includes using an environmentally friendly plasma gas, which minimizes safety hazards during an implementation of the method and does not require an additional heat source during a reflow process thereof. That is, the method includes reflowing a solder bump using an argon-hydrogen plasma process. The argon-hydrogen plasma process used to fabricate the flip chip includes maintaining a pressure in a chamber at 250 to 270 mtorr, feeding a mixed gas of argon with 10 to 20% hydrogen to the chamber to generate a plasma with power of 100 to 200 W, and exposing the flip chip to the plasma for 30 to 120 seconds. Additionally, an argon-hydrogen plasma process used to mount the flip chip includes maintaining pressure in a chamber at 100 to 400 mtorr, feeding a mixed gas of argon with 0 to 20% hydrogen to the chamber to generate a plasma with power of 10 to 50 W, and exposing the flip chip to the plasma for 10 to 120 seconds.

## Claims

### Claim 1

A method of fabricating a flip chip having a solder bump, the method comprising:
bonding the solder bump to an under bump metallurgy layer formed on the flip chip; and
reflowing the solder bump using an argon-hydrogen plasma process.

### Claim 2 (depends on 1)

The method as set forth in claim 1, wherein the argon-hydrogen plasma process includes reflowing the solder bump using a mixed gas of argon with 10 to 20% hydrogen.

### Claim 3 (depends on 1)

The method as set forth in claim 1, wherein the argon-hydrogen plasma process includes reflowing the solder bump using a pressure in a range of 250 to 270 mtorr.

### Claim 4 (depends on 1)

The method as set forth in claim 1, wherein the argon-hydrogen plasma process includes reflowing the solder bump using a plasma power in a range of 100 to 200 W.

### Claim 5 (depends on 1)

The method as set forth in claim 1, wherein the argon-hydrogen plasma process includes exposing the flip chip to an argon-hydrogen plasma for 30 to 120 seconds to reflow the solder bump.

### Claim 6

A method of fabricating a flip chip, the method comprising:
depositing a plating seed layer on the flip chip;
patterning a photoresist coated on the plating seed layer;
depositing an under bump metallurgy layer on a resulting patterned structure;
removing the photoresist and the plating seed layer from the flip chip;
bonding a solder bump to the under bump metallurgy layer; and
reflowing the solder bump using an argon-hydrogen plasma process.

### Claim 7 (depends on 6)

The method as set forth in claim 6, wherein the argon-hydrogen plasma process includes:
maintaining a pressure in a range of 250 to 270 mtorr;
providing a mixed gas of argon with 10 to 20% hydrogen with power in a range of 100 to 200 W to generate a plasma thereof; and
exposing the flip chip to the plasma for 30 to 120 seconds.

### Claim 8 (depends on 6)

The method as set forth in claim 6, wherein the under bump metallurgy layer comprises a Cu layer and a Ni layer.

### Claim 9 (depends on 6)

The method as set forth in claim 6, wherein the reflowing of the solder bump includes self-aligning the solder bump melted and reshaped in a form of a sphere by using the argon-hydrogen plasma process so as to position the solder bump at a center of the under bump metallurgy layer.

### Claim 10

A method of reflowing a flip chip having a solder bump, the method comprising reflowing the solder bump on an under bump metallurgy layer of the flip chip using an argon-hydrogen plasma process.

### Claim 11 (depends on 10)

The method as set forth in claim 10, wherein:
the reflowing of the solder bump includes removing a surface oxide film of the solder bump using the argon-hydrogen plasma process, and
the argon-hydrogen plasma process includes:
maintaining a pressure in a range of 250 to 270 mtorr;
providing a mixed gas of argon with 10 to 20% hydrogen with power in a range of 100 to 200 W to generate a plasma thereof; and
exposing the flip chip to the plasma for 30 to 120 seconds.

### Claim 12

A method of self-aligning a flip chip having a solder bump, the method comprising self-aligning a solder ball of the solder bump melted and reshaped in a form of a sphere using an argon-hydrogen plasma process so as to position the solder ball at a center of an under bump metallurgy layer of the flip chip.

### Claim 13 (depends on 12)

The method as set forth in claim 12, wherein the argon-hydrogen plasma process includes:
maintaining a pressure in a range of 250 to 270 mtorr;
providing a mixed gas of argon with 10 to 20% hydrogen with power in a range of 100 to 200 W to generate a plasma thereof; and
exposing the solder bump to the plasma for 30 to 120 seconds.

### Claim 14

A method of mounting a flip chip having a solder bump on a circuit board, the method comprising:
etching the solder bump of the flip chip using an argon-hydrogen plasma process; and
mounting the flip chip on the circuit board.

### Claim 15 (depends on 14)

The method as set forth in claim 14, wherein the argon-hydrogen plasma process includes:
maintaining a pressure in a range of 100 to 400 mtorr;
providing a mixed gas of argon with 0 to 20% hydrogen with power in a range of 10 to 50 W to generate a plasma thereof; and
exposing the flip chip to the plasma for 10 to 120 seconds.

### Claim 16 (depends on 14)

The method as set forth in claim 14, wherein the mounting of the flip chip comprises performing the mounting within two hours after the argon-hydrogen plasma process is completed.

### Claim 17 (depends on 1)

The method as set forth in claim 1, wherein the bonding of the solder bump to the under bump metallurgy layer comprises bonding a solder ball of the solder bump to the under bump metallurgy layer using a laser beam.

### Claim 18 (depends on 17)

The method as set forth in claim 17, wherein the laser beam is an Nd:YAG laser beam having a wavelength of about 1064 nm, an electric current of about 65 A, and a pulse rate of about 3 ms.

### Claim 19 (depends on 1)

The method as set forth in claim 1, wherein the reflowing of the solder bump includes:
removing an oxide film of the solder bump using argon ions of the argon-hydrogen plasma process;
providing a reductive atmosphere to prevent re-oxidizing of the solder bump and wet the under bump metallurgy layer using hydrogen ions of the argon-hydrogen plasma process; and
reshaping the solder bump in a form of a sphere and centering the reshaped solder bump at a center of the under bump metallurgy layer using the argon-hydrogen plasma process.

### Claim 20 (depends on 19)

The method as set forth in claim 19, wherein the reflowing of the solder bump further includes forming an intermetallic compound between the solder bump and the under bump metallurgy layer.

### Claim 21 (depends on 1)

The method as set forth in claim 1, wherein the reflowing of the solder bump does not include using a flux to wet the under bump metallurgy layer.

### Claim 22 (depends on 14)

The method as set forth in claim 14, wherein the etching of the solder bump includes:
removing an oxide film of the solder bump using argon ions of the argon-hydrogen plasma process without re-melting the solder bump reflowed on an under bump metallurgy layer of the flip chip; and
providing a reductive atmosphere to prevent re-oxidizing of the solder bump using hydrogen ions of the argon-hydrogen plasma process.

### Claim 23 (depends on 14)

The method as set forth in claim 14, wherein the mounting of the flip chip on the circuit board comprises:
positioning the flip chip with respect to the circuit board to have the solder bump contact a corresponding layer of the circuit board; and
bonding the flip chip on the circuit board by heating the flip chip and the circuit board.

### Claim 24 (depends on 23)

The method as set forth in claim 23, wherein the mounting of the flip chip on the circuit board further comprises providing a nitrogen atmosphere during the heating of the flip chip and the circuit board.

### Claim 25

A flip chip comprising:
a substrate;
an integrated circuit form on the substrate; and
an under bump metallurgy layer formed on a surface of the substrate; and
a solder bump formed on the under bump metallurgy layer, wherein the solder bump has a reflowed structure of a solder exposed to an argon-hydrogen plasma.

### Claim 26 (depends on 25)

The flip chip as set forth in claim 25, wherein the solder bump is a solder ball exposed to the argon-hydrogen plasma resulting from a mixed gas of argon with 10 to 20% hydrogen, at a pressure of 250 to 270 mtorr and power of 100 to 200 W, for 30 to 120 seconds.