# US 2004/0072104 A1 · Method for forming ultra fine contact holes in semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072104 A1
- Document ID: US20040072104A1
- Status: Published application
- Kind: A1
- Application number: 10/623,419
- Filed: 2003-07-18
- Published: 2004-04-15
- Earliest claimed: 2002-07-19
- Inventors: Sang-Tae Choi; Seung-Weon Paek
- Web page: https://patentgrep.com/patent/US20040072104A1

## CPC

- G03F 7/40: Treatment after imagewise removal, e.g. baking
- H10P 50/73: {using masks for insulating materials}
- H10P 76/2043: {using an anti-reflective coating}
- H10P 76/4088: {Processes for improving the resolution of the masks}
- Y10S 430/143: Electron beam
- Y10S 430/146: Laser beam
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for forming an ultra fine contact hole includes: forming a KrF photoresist pattern on a semiconductor substrate providing an insulation layer, the KrF photoresist pattern exposing a predetermined region for forming a contact hole on the insulation layer; forming a chemically swelling process (CSP) chemical material-containing layer being reactive to the KrF photoresist pattern on an entire surface of the semiconductor substrate; forming a chemical material-containing pattern encompassing the KrF photoresist pattern by reacting the chemical material-containing layer with the KrF photoresist pattern through a chemically swelling process to decrease a critical dimension of the contact hole; rinsing the semiconductor substrate; and increasing a thickness of a sidewall of the chemical material-containing pattern to a predetermined thickness by performing a resist flow process (RFP) that makes the chemical material-containing pattern flowed to decrease the critical dimension (CD) of the contact hole.

## Claims

### Claim 1

A method for forming an ultra fine contact hole in a semiconductor device with use of a KrF light source, the method comprising:
forming a KrF photoresist pattern on an insulation layer disposed on a semiconductor substrate, the KrF photoresist pattern exposing a predetermined region of the insulation layer for forming a contact hole in the insulation layer;
forming a chemically swelling process (CSP) by depositing a chemical material-containing layer that is reactive to the KrF photoresist pattern on an entire surface of the photoresist pattern and insulating layer;
forming a chemical material-containing pattern encompassing the KrF photoresist pattern by reacting the chemical material-containing layer with the KrF photoresist pattern through the chemically swelling process to decrease a critical dimension of the contact hole;
rinsing the semiconductor substrate; and
increasing a thickness of a sidewall of the chemical material-containing pattern to a predetermined thickness by performing a resist flow process (RFP) that makes the chemical material-containing pattern flowed to decrease the critical dimension (CD) of the contact hole.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the CSP chemical material-containing layer has a resist composition comprising de-ionized (DI) water, a cross-linker, a solvent and a photo acid generator (PAG), wherein the DI water constitues about 90% of the above composition while the remaining components constitute about 10% thereof.

### Claim 3 (depends on 1)

The method as recited in claim 1, wherein the CSP chemical material-containing layer has a thickness ranging from about 1000 Å to about 3000 Å.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the CSP is carried out by employing a series of processes including a heat process, a photo-exposure process and an electron beam exposure process.

### Claim 5 (depends on 4)

The method as recited in claim 4, wherein the heat process is carried out at a temperature ranging from about 90° C. to about 130° C.

### Claim 6 (depends on 4)

The method as recited in claim 4, wherein the photo-exposure process uses photo-exposure energy ranging of above about 20 mJ/cm to about 30 mJ/cm2 in case of using the KrF light source.

### Claim 7 (depends on 1)