# US 2004/0072082 A1 · Photomask, method of manufacturing a photomask, and method of manufacturing an electronic product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0072082 A1
- Document ID: US20040072082A1
- Status: Published application
- Kind: A1
- Application number: 10/615,194
- Filed: 2003-07-09
- Published: 2004-04-15
- Earliest claimed: 2002-07-09
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Sachiyo Ito; Masamitsu Itoh; Masahiko Hasunuma
- Web page: https://patentgrep.com/patent/US20040072082A1

## CPC

- G03F 1/32: Attenuating PSM [att-PSM], e.g. halftone PSM or PSM having semi-transparent phase shift portion,; Preparation thereof
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A photomask comprises a substrate, a translucent film selectively formed on the substrate, and a shading film selectively formed on the translucent film, wherein when the substrate, the translucent film and the shading film have Young's moduli (MPa) E0 E1 and E2, and film thickness (m) d0, d1 and d2 respectively, internal stresses (MPa) of the translucent film and the shading film at room temperature are s1 and s2 respectively, a covering rate by the translucent film defined by an area in which the shading film is not formed is expressed as h, and coefficients are expressed as k1=1.3×10−8, k2=−9.5×10−2, k3=6.0×10−7, and k4=−5.2×10−2 respectively, the substrate, the translucent film and the shading film satisfy a condition given by the following expression: 1 [LeftBracketingBar] 1 E 0 · d 0 · { h · ( k 1 · S 1 E 1 · d 1 + k 2 ) + ( k 3 · S 2 E 2 · d 2 + k 4 ) } [RightBracketingBar] ≦ 1.4 × 10 - 4 ⁢ ( m - 1 )

## Claims

### Claim 1

A photomask comprising:
a substrate;
a translucent film selectively formed on the substrate; and
a shading film selectively formed on the translucent film, wherein
when the substrate, the translucent film and the shading film have Young's moduli (MPa) E0 E1 and E2, and film thickness (m) d0, d1 and d2 respectively, internal stresses (MPa) of the translucent film and the shading film at room temperature are s1 and s2 respectively, a covering rate by the translucent film defined by an area in which the shading film is not formed is expressed as h, and coefficients are expressed as k1=1.3×10−8, k2=−9.5×10−2, k3=6.0×10−7, and k4=−5.2×10−2 respectively, the substrate, the translucent film and the shading film satisfy a condition given by the following expression:
6 [LeftBracketingBar] 1 E 0 · d 0 · { h · ( k 1 · S 1 E 1 · d 1 + k 2 ) + ( k 3 · S 2 E 2 · d 2 + k 4 ) } [RightBracketingBar] ≦ 1.4 × 10 - 4 ⁢ ( m - 1 )
≦1.4×10−4(m−1)

### Claim 2 (depends on 1)

A photomask according to claim 1, wherein the internal stress of the shading film at room temperature is in the range of 500 MPa to 5 GPa.

### Claim 3 (depends on 1)

A photomask according to claim 1, wherein the substrate, the translucent film and the shading film satisfy a condition given by the following expression:
7 [LeftBracketingBar] 1 E 0 · d 0 · { h · ( k 1 · S 1 E 1 · d 1 + k 2 ) + ( k 3 · S 2 E 2 · d 2 + k 4 ) } [RightBracketingBar] ≦ 0.87 × 10 - 4 ⁢ ( m - 1 )
0.87×10−4(m−1)

### Claim 4 (depends on 3)

A photomask according to claim 3, wherein the internal stress of the shading film at room temperature is in the range of 1 GPa to 4.5 GPa.

### Claim 5 (depends on 1)

A photomask according to claim 1, wherein the covering rate h is 100%>h≦30%.

### Claim 6 (depends on 1)

A photomask according to claim 1, wherein the substrate, the translucent film and the shading film are made of quartz, MoSiON and Cr, respectively.

### Claim 7 (depends on 1)

A photomask according to claim 1, wherein a first phase of light that passes through a first area in which the translucent film and the shading film are not formed differs from a second phase of light that passes through a second area in which the translucent film is formed.

### Claim 8

A method of manufacturing a photomask comprising:
forming a translucent film and a shading film sequentially onto a surface of a substrate;
measuring an internal stress in each of the translucent film and the shading film;
determining whether or not a following expression is satisfied when the substrate, the translucent film and the shading film have Young's moduli (MPa) E0 E1 and E2, and film thickness (m) d0, d1 and d2 respectively, internal stresses (MPa) of the translucent film and the shading film at room temperature are s1 and s2 respectively, a virtual covering rate by the translucent film after mask pattern formation defined by an area in which the shading film is not formed is expressed as h, coefficients are expressed as k1=1.3×10−8, k2=−9.5×10−2, k3=6.0×10−7, and k4=−5.2×10−2 respectively, and a predicted warping amount for a desired photomask after the mask pattern formation is defined as A (m−1); and
8 [LeftBracketingBar] 1 E 0 · d 0 · { h · ( k 1 · S 1 E 1 · d 1 + k 2 ) + ( k 3 · S 2 E 2 · d 2 + k 4 ) } [RightBracketingBar] ≦ A ⁡ ( m - 1 )
≦A(m−1)
removing the translucent film and the shading film selectively to be the covering rate h that satisfy the expression based on the determination result.

### Claim 9 (depends on 8)

A method of manufacturing a photomask according to claim 8, wherein the predicted warping amount A is 1.4×10−4 (m−1).

### Claim 10 (depends on 9)

A method of manufacturing a photomask according to claim 9, wherein the internal stress of the shading film at room temperature is in the range of 500 MPa to 5 GPa.

### Claim 11 (depends on 8)

A method of manufacturing a photomask according to claim 8, wherein the predicted warping amount A is 0.87×10−4(m−1).

### Claim 12 (depends on 11)

A method of manufacturing a photomask according to claim 11, wherein the internal stress of the shading film at room temperature is in the range of 1 GPa to 4.5 GPa.

### Claim 13 (depends on 8)

A method of manufacturing a photomask according to claim 8, wherein the virtual covering rate h is 100%>h≦30%.

### Claim 14 (depends on 8)

A method of manufacturing a photomask according to claim 8, wherein a first phase of light that passes through a first area in which the translucent film and the shading film are not formed differs from a second phase of light that passes through a second area in which the translucent film is formed.

### Claim 15

A method of manufacturing an electronic product comprising:
forming a photoresist on a substrate to be processed;
passing light through a photomask having a mask pattern that has a substrate, a translucent film selectively formed on the substrate and a shading film selectively formed on the translucent film to transfer the mask pattern onto the photoresist; wherein when the substrate, the translucent film and the shading film have Young's moduli (MPa) E0 E1 and E2, and film thickness (m) d0, d1 and d2 respectively, internal stresses (MPa) of the translucent film and the shading film at room temperature are s1 and s2 respectively, a covering rate by the translucent film defined by an area in which the shading film is not formed is expressed as h, and coefficients are expressed as k1=1.3×10−8, k2=−9.5×10−2, k3=6.0×10−7, and k4=−5.2×10−2 respectively, the substrate, the translucent film and the shading film satisfy a condition given by the following expression:
9 [LeftBracketingBar] 1 E 0 · d 0 · { h · ( k 1 · S 1 E 1 · d 1 + k 2 ) + ( k 3 · S 2 E 2 · d 2 + k 4 ) } [RightBracketingBar] ≦ 1.4 × 10 - 4 ⁢ ( m - 1 )
≦1.4×10−4(m−1)
developing the photoresist; and
selectively processing the substrate to be processed using the photoresist as a mask.

### Claim 16 (depends on 15)

A method of manufacturing an electronic product according to claim 15, wherein the internal stress of the shading film at room temperature is in the range of 500 MPa to 5 GPa.

### Claim 17 (depends on 15)

A method of manufacturing an electronic product according to claim 15, wherein the substrate, the translucent film and the shading film satisfy a condition given by the following expression:
10 [LeftBracketingBar] 1 E 0 · d 0 · { h · ( k 1 · S 1 E 1 · d 1 + k 2 ) + ( k 3 · S 2 E 2 · d 2 + k 4 ) } [RightBracketingBar] ≦ 0.87 × 10 - 4 ⁢ ( m - 1 )
≦0.87×10−4(m−1)

### Claim 18 (depends on 17)

A method of manufacturing an electronic product according to claim 17, wherein the internal stress of the shading film at room temperature is in the range of 1 GPa to 4.5 GPa.

### Claim 19 (depends on 15)

A method of manufacturing an electronic product according to claim 15, wherein the covering rate h is 100%>h≦30%.

### Claim 20 (depends on 15)

A method of manufacturing an electronic product according to claim 15, wherein a first phase of light that passes through a first area in which the translucent film and the shading film are not formed differs from a second phase of light that passes through a second area in which the translucent film is formed.