- Earliest claimed: 2001-01-19
- Assignees: Centre National De La Recherche Scientifique; Universite de Montpellier II
- Inventors: Pascal Etienne
- Web page: https://patentgrep.com/patent/US20040071426A1

## CPC

- G02B 6/13: Integrated optical circuits characterised by the manufacturing method
- G02B 6/132: by deposition of thin films
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A method for manufacturing an optical waveguide component with several layers stacked on a silicon substrate. The layers include a buffer layer, a first substrate, a guiding layer on the buffer layer and including an optical waveguide, and an outer layer as protection against external stresses. The layers are made from an organic-inorganic hybrid using a sol-gel process. An additional layer is disposed on the guiding layer so that a symmetrical structure is produced that has the same refractive index around the waveguide in the guiding layer.

## Claims

### Claim 1

Method for manufacturing a waveguide component with several layers stacked on a silicon substrate, of the type comprising a buffer layer deposited on said substrate, a guiding layer deposited on the buffer layer and allowing the fabrication of a waveguide device, and an outer protection layer against external stresses, the layers being made in an organic-inorganic hybrid using the sol-gel process, characterized in that on guiding layer (3) an additional layer (4) is deposited so as to obtain a symmetrical structure having the same refractive index around the waveguide device made in the guiding layer (3).

### Claim 2 (depends on 1)

Method according to claim 1, characterized in that the additional layer (4) deposited on guiding layer (3) is a second buffer layer having the same refractive index as the first buffer layer (2).

### Claim 3 (depends on 2)

Method according to claim 2, characterized in that the second buffer layer (4) is made from the same solution as the first buffer layer (2) deposited on the silicon substrate (1).

### Claim 4 (depends on 2, 3)

Method according to either of claims 2 or 3, characterized in that the waveguide device is made in guiding layer (3) by exposing the zones of this layer which are to form the waveguide device to ultraviolet radiation or to laser through the additional layer (4) deposited on guiding layer (3).

### Claim 5 (depends on 4)

Method according to claim 4, characterized in that exposure to ultraviolet radiation is made after fabricating the protection layer (5).

### Claim 6 (depends on 1, 2, 3, 4, 5)

Method according to any of claims 1 to 5, characterized in that the guiding layer (3) is made from the same solution as buffer layers (2) and (4) after adding a photoinitiator.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

Method according to any of claims 1 to 6, characterized in that the first buffer layer (2) on substrate (1) is dried after being deposited, at a temperature lying between 900 and 120° C., advantageously at 100° C., for a time of 15 minutes to one hour, advantageously for 30 minutes.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

Method according to any of claims 1 to 7, characterized in that the guiding layer (3) after being deposited is dried at a temperature lying between 60 and 80° C., advantageously at 60° C., for a time of 10 to 45 minutes, advantageously for 30 minutes.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

Method according to any of claims 1 to 8, characterized in that insulating layer (4) deposited on guiding layer (3) is dried after its deposition at a temperature lying between 60 and 80° C., advantageously at 60° C., for a time of 20 to 45 minutes, advantageously for 30 minutes.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

Method according to any of claims 1 to 9, characterized in that the protection layer, after being deposited, is dried at a temperature advantageously of 60° C. for a time of 20 to 45 minutes, advantageously for 30 minutes.

### Claim 11 (depends on 4, 5, 6, 7, 8, 9, 10)

Method according to any of claims 4 to 10, characterized in that ultraviolet radiation is used advantageously with a wavelength of 325 nm, radiation advantageously being applied for a time of a few seconds to a few minutes depending upon the photoinitiator used.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

Method according to any of claims 1 to 11, characterized in that the component after being insulated by ultraviolet radiation, is annealed at a temperature lying between 100 and 120° C., advantageously at 100° C., for a time of 20 to 45 minutes, advantageously for 30 minutes.

### Claim 13 (depends on 1, 2, 3)

Method according to any of claims 1 to 3, characterized in that the guiding layer (3) is insulated immediately after it has been deposited, by ultraviolet radiation or laser, in that the non-insulated parts are then dissolved, and in that the additional layer is deposited on the guiding layer after dissolution of the non-insulated parts.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13)

Waveguide component fabricated according to the method of any of claims 1 to 13, characterized in that an additional insulating layer (4) is made on the guiding layer, and in that the material around the waveguide device fabricated in guiding layer (3) has a symmetrical structure relative to the guiding layer having the same refractive index.

### Claim 15 (depends on 14)

Waveguide component according to claim 14, characterized in that the additional layer (4) deposited on guiding layer (3) is a second buffer layer made from the same solution as the buffer layer (2) deposited on the silicon substrate (1).