# US 2004/0069969 A1 · Magnetic ferrite powder, magnetic ferrite sinter, layered ferrite part, and process for producing layered ferrite part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0069969 A1
- Document ID: US20040069969A1
- Status: Published application
- Kind: A1
- Application number: 10/009,075
- Filed: 2002-02-14
- Published: 2004-04-15
- Earliest claimed: 2000-04-28
- Assignees: TDK Corporation
- Inventors: Masami Endo; Atsuyuki Nakano
- Web page: https://patentgrep.com/patent/US20040069969A1

## CPC

- C04B 35/62675: {characterised by the treatment temperature}
- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- C01G 49/0036: {containing one alkaline earth metal, magnesium or lead}
- C01G 49/0063: {containing zinc}
- C01G 49/0072: {containing manganese}
- C01G 49/009: {Compounds containing iron, with or without oxygen or hydrogen, and containing two or more other elements}
- C04B 35/2633: {containing barium, strontium or calcium}
- C04B 35/265: {Compositions containing one or more ferrites of the group comprising manganese or zinc and one or more ferrites of the group comprising nickel, copper or cobalt}
- C04B 35/6261: {Milling}
- H01F 1/348: {Hexaferrites with decreased hardness or anisotropy, i.e. with increased permeability in the microwave (GHz) range, e.g. having a hexagonal crystallographic structure}
- H01F 17/0033: {with the coil helically wound around a magnetic core}
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/74: by peak-intensities or a ratio thereof only
- C01P 2002/85: by XPS, EDX or EDAX data
- C01P 2004/04: obtained by TEM, STEM, STM or AFM
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/10: Solid density
- C01P 2006/12: Surface area
- C01P 2006/32: Thermal properties
- C01P 2006/33: Phase transition temperatures
- C01P 2006/42: Magnetic properties
- C04B 2235/3201: Alkali metal oxides or oxide-forming salts thereof
- C04B 2235/3203: Lithium oxide or oxide-forming salts thereof
- C04B 2235/3206: Magnesium oxides or oxide-forming salts thereof
- C04B 2235/3215: Barium oxides or oxide-forming salts thereof
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3262: Manganese oxides, manganates, rhenium oxides or oxide-forming salts thereof, e.g. MnO
- C04B 2235/3274: Ferrites
- C04B 2235/3275: Cobalt oxides, cobaltates or cobaltites or oxide forming salts thereof, e.g. bismuth cobaltate, zinc cobaltite
- C04B 2235/3277: Co3O4
- C04B 2235/3279: Nickel oxides, nickalates, or oxide-forming salts thereof
- C04B 2235/3281: Copper oxides, cuprates or oxide-forming salts thereof, e.g. CuO or Cu2O
- C04B 2235/3284: Zinc oxides, zincates, cadmium oxides, cadmiates, mercury oxides, mercurates or oxide forming salts thereof
- C04B 2235/3298: Bismuth oxides, bismuthates or oxide forming salts thereof, e.g. zinc bismuthate
- C04B 2235/3409: Boron oxide, borates, boric acids, or oxide forming salts thereof, e.g. borax
- C04B 2235/36: Glass starting materials for making ceramics, e.g. silica glass
- C04B 2235/365: Borosilicate glass
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5445: submicron sized, i.e. from 0,1 to 1 micron
- C04B 2235/6025: Tape casting, e.g. with a doctor blade
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/767: Hexagonal symmetry, e.g. beta-Si3N4, beta-Sialon, alpha-SiC or hexa-ferrites
- C04B 2235/77: Density
- C04B 2235/784: Monomodal
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/85: Intergranular or grain boundary phases
- C04B 2235/9615: Linear firing shrinkage
- Y10T 428/12465: having magnetic properties, or preformed fiber orientation coordinate with shape
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Provided is magnetic ferrite powder in which a peak intensity ratio of Z phase (M3Me2Fe24O41: M=one or more kinds of alkaline-earth metal, Me=one or more kinds from Co, Ni, Mn, Zn, Mg and Cu) of hexagonal ferrite is 30% or higher in X-ray diffraction and a peak value of a grain size distribution is in a range from 0.1 μm to 3 μm.

## Claims

### Claim 1

Magnetic ferrite powder,
wherein a peak intensity ratio of Z phase (M3Me2Fe24O41: M=one or more kinds of alkaline-earth metal, Me=one or more kinds selected from Co, Ni, Mn, Zn, Mg and Cu) of hexagonal ferrite is 30% or higher in X-ray diffraction, and
a peak value of grain size distribution is within a range from 0.1 μm to 3 μm.

### Claim 2 (depends on 1)

The magnetic ferrite powder according to claim 1,
wherein one or more kinds selected from borosilicate glass, zinc borosilicate glass, Bi2O3 based glass, CuO and Bi2O3 are added by 0.5 wt % to 20 wt %.

### Claim 3 (depends on 1)

The magnetic ferrite powder according to claim 1,
wherein CuO and Bi2O3 are added by 0.5 wt % to 20 wt % in total.

### Claim 4 (depends on 1)

The magnetic ferrite powder according to claim 1,
wherein Bi2O3 based glass and CuO are added by 3 wt % to 15 wt % in total.

### Claim 5 (depends on 1)

The magnetic ferrite powder according to claim 1,
wherein Bi2O3 based glass is added by 3 wt % to 7 wt %, and CuO is added by 3 wt % to 7 wt %.

### Claim 6

Magnetic ferrite powder,
wherein Z phase (where M=Ba, Me=one or more kinds selected from Co, Ni, Mn, Zn, Mg and Cu) indicated as M3Me2Fe24O41 forms a main phase, and
a powder specific surface area is from 5 m2/g to 30 m2/g.

### Claim 7 (depends on 6)

The magnetic ferrite powder according to claim 6,
wherein a portion of Ba is substituted with Sr.

### Claim 8

A sintered body of magnetic ferrite,
wherein a Z phase (M=Ba, Me=one or more kinds selected from Co, Ni, Mn, Zn, Mg and Cu) indicated as M3Me2Fe24O41 forms a main phase,
CuO and Bi2O3 are included by 0.5 wt % to 20 wt % in total,
CuO mainly exists within grains, and
Bi2O3 mainly exists at grain boundaries.

### Claim 9 (depends on 8)

The sintered body of magnetic ferrite according to claim 8,
wherein a portion of Ba is substituted with Sr.

### Claim 10

Sintered body of magnetic ferrite,
wherein Z phase (where M=Ba, Me=one or more kinds selected from Co, Ni, Mn, Zn, Mg and Cu) indicated as M3Me2Fe24O41 forms a main phase, and
Bi2O3 based glass and CuO are added by 1 wt % to 20 wt % in total.

### Claim 11

A multilayer ferrite chip component in which a magnetic ferrite layer and an internal electrode are stacked alternately, the multilayer ferrite chip component comprising an external electrode electrically connected with said internal electrode,
wherein said magnetic ferrite layer has Z phase (M3Me2Fe24O41: M=one or more kinds of alkaline-earth metal, Me=one or more kinds selected from Co, Ni, Mn, Zn, Mg and Cu) of hexagonal ferrite as a main phase in X-ray diffraction, the magnetic ferrite layer being constituted of sintered body of magnetic ferrite having a mean grain size of 1 to 5 μm, and
said internal electrode is constituted of any one of Ag and an Ag alloy.

### Claim 12 (depends on 11)

The multilayer ferrite chip component according to claim 11,
wherein said multilayer ferrite chip component is formed by co-firing said magnetic ferrite layer and said internal electrode layer, and
density of said magnetic ferrite layer is 5 g/cm3 or higher.

### Claim 13 (depends on 11)

The multilayer ferrite chip component according to claim 11,
wherein said magnetic ferrite layer includes CuO and Bi2O3 by 0.5 wt % to 20 wt % in total,
CuO mainly exists within grains, and
Bi2O3 mainly exists at grain boundaries.

### Claim 14 (depends on 11)

The multilayer ferrite chip component according to claim 11,
wherein said magnetic ferrite layer includes Bi2O3 based glass and CuO by 1 wt % to 20 wt % in total.

### Claim 15

A manufacturing method of a multilayer ferrite chip component in which a magnetic ferrite layer and an internal electrode are stacked, comprising the steps of:
mixing raw material powder of magnetic ferrite;
calcining the mixed raw material powder in a temperature range of 1200° C. or higher;
milling the obtained calcined body so as to make a peak value of grain size distribution fall into a range from 0.1 to 3 μm;
obtaining a sheet or paste for forming a magnetic layer by using the obtained milled powder;
obtaining a laminated green body by alternately stacking material for the internal electrode and any one of said sheet and said paste; and
sintering said laminated green body at a temperature lower than 960° C.,
wherein said magnetic ferrite layer consists of sintered body of magnetic ferrite having a peak intensity ratio of Z phase (M3Me2Fe24O41: M=one or more kinds of alkaline-earth metal, Me=one or more kinds selected from Co, Ni, Mn, Zn, Mg and Cu) of hexagonal ferrite at 30% or greater in X-ray diffraction.

### Claim 16 (depends on 15)

The manufacturing method of the multilayer ferrite chip component according to claim 15,
wherein a powder specific surface area of each of said raw material powder is 4.5 m2/g or more.

### Claim 17 (depends on 15)

The manufacturing method of the multilayer ferrite chip component according to claim 15,
wherein a powder specific surface area of said milled powder is in a range from 8 m2/g to 20 m2/g.