# US 2004/0069831 A1 · Toughness-optimized weld joints and methods for producing said weld joints

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0069831 A1
- Document ID: US20040069831A1
- Status: Published application
- Kind: A1
- Application number: 10/633,134
- Filed: 2003-08-01
- Published: 2004-04-15
- Earliest claimed: 2002-10-11
- Assignees: ExxonMobil Upstream Research Company
- Inventors: Jeffrey R. O'Donnell; Ronald R. Bowen
- Web page: https://patentgrep.com/patent/US20040069831A1

## CPC

- G01N 29/069: {Defect imaging, localisation and sizing using, e.g. time of flight diffraction [TOFD], synthetic aperture focusing technique [SAFT], Amplituden-Laufzeit-Ortskurven [ALOK] technique}
- B23K 9/0026: {specially adapted for particular articles or work}
- B23K 9/0216: {Seam profiling, e.g. weaving, multilayer}
- B23K 9/0953: {using computing means}
- B23K 9/0956: {using sensing means, e.g. optical}
- B23K 31/125: {Weld quality monitoring}
- G01N 29/07: by measuring propagation velocity or propagation time of acoustic waves
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

Methods for producing toughness-optimized weld joints are provided. A welding procedure that will provide adequate toughness for the center-weld of the weld-joint is developed and used, and a welding procedure that will provide adequate toughness for the surface-weld of the weld-joint is developed and used.

## Claims

### Claim 1

A method of welding two pieces of metal to produce a weld joint comprised of a center-weld and a surface-weld, and having a specified thickness and optimized fracture toughness for an intended application, said method comprising the steps of:
(a) selecting a first non-destructive examination technique that is suitable for detecting surface-breaking discontinuities in a metal used in said intended application;
(b) determining a minimum surface-breaking discontinuity through-thickness dimension that is readily detectable by said first non-destructive examination technique;
(c) selecting a second non-destructive examination technique that is suitable for detecting embedded discontinuities in a metal used in said intended application;
(d) determining a minimum embedded discontinuity through-thickness dimension that is readily detectable by said second non-destructive examination technique;
(e) determining a first toughness value that is adequate to substantially prevent fracture initiation in said weld joint from surface-breaking discontinuities having a through-thickness dimension that is substantially equal to said minimum surface-breaking discontinuity through-thickness dimension and a second toughness value that is adequate to substantially prevent fracture initiation in said weld joint from embedded discontinuities having a through-thickness dimension that is substantially equal to said minimum embedded discontinuity through thickness dimension;
(f) designing a surface-weld welding procedure that will produce a surface-weld having a toughness value substantially equal to or greater than said first toughness value and a center-weld welding procedure that will produce a center-weld having a toughness value substantially equal to or greater than said second toughness value;
(g) creating said center-weld using said center-weld welding procedure; and
(h) creating said surface-weld using said surface-weld welding procedure.

### Claim 2

A weld joint having optimized fracture toughness for an intended application, said weld joint having been produced by a method of welding two pieces of metal to produce said weld joint, wherein said weld joint is comprised of a center-weld and a surface-weld and has a specified thickness, and said method comprises the steps of:
(a) selecting a first non-destructive examination technique that is suitable for detecting surface-breaking discontinuities in a metal used in said intended application;
(b) determining a minimum surface-breaking discontinuity through-thickness dimension that is readily detectable by said first non-destructive examination technique;
(c) selecting a second non-destructive examination technique that is suitable for detecting embedded discontinuities in a metal used in said intended application;
(d) determining a minimum embedded discontinuity through-thickness dimension that is readily detectable by said second non-destructive examination technique;
(e) determining a first toughness value that is adequate to substantially prevent fracture initiation in said weld joint from surface-breaking discontinuities having a through-thickness dimension that is substantially equal to said minimum surface-breaking discontinuity through-thickness dimension and a second toughness value that is adequate to substantially prevent fracture initiation in said weld joint from embedded discontinuities having a through-thickness dimension that is substantially equal to said minimum embedded discontinuity through thickness dimension;
(f) designing a surface-weld welding procedure that will produce a surface-weld having a toughness value substantially equal to or greater than said first toughness value and a center-weld welding procedure that will produce a center-weld having a toughness value substantially equal to or greater than said second toughness value;
(g) creating said center-weld using said center-weld welding procedure; and
(h) creating said surface-weld using said surface-weld welding procedure.