# US 2004/0069213 A1 · Method and device for producing an electronic gaas detector for x-ray detection for imaging

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0069213 A1
- Document ID: US20040069213A1
- Status: Published application
- Kind: A1
- Application number: 10/466,761
- Filed: 2003-12-08
- Published: 2004-04-15
- Earliest claimed: 2001-01-31
- Assignees: Universite Pierre et Marie Curie
- Inventors: Jacques Bourgoin
- Web page: https://patentgrep.com/patent/US20040069213A1

## CPC

- H10F 30/29: the devices being sensitive to radiation having very short wavelengths, e.g. X-rays, gamma-rays or corpuscular radiation
- C30B 25/02: Epitaxial-layer growth
- C30B 29/42: Gallium arsenide
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The invention relates to a method for producing an X-ray detector for imaging. By increasing the epitaxial layers, a GaAs material (1) is placed on a substrate n<+> (or p<+>) (2). p<+> (or n<+>)< >ions are then implanted on the external face (11) of the material (1) in order to form a p<+>/i/n<+> structure after annealing. Ohmic contacts (12) are subsequently disposed on the two faces and individual detectors (pixels) (13) are produced over the entire surface using means of dry or chemical masking and pickling. The epitaxial material (1) has a thickness d′ that is sufficient to absorb effectively the X photons and means can be used to reduce the residual doping of said material (1). The material obtained in this way is suitable for medical (mammography, dental, etc.) and industrial imaging.

## Claims

### Claim 1

A method for producing an electronic GaAs detector for X-ray detection for imaging wherein:
a method for growing epitaxial layer on a substrate n+(or p+) 2 is used in order to form a semiconductor material (1) which material contains a certain residual doping,
the thickness of the substrate (2) is reduced by mechanical-chemical polishing,
a p+/i/n+structure is formed:
ions p+(or n+) (11) are then implanted on the external face of the material,
said structure is annealed at a temperature θ1 for a duration t1,
ohmic contacts (12) are disposed on both faces
individual detectors (13) are produced by masking, passivation and chemical pickling,
characterised in that
said method for growing layers of material comprises the following steps:
a source material (7), which is a wafer cut into an ingot of semi-insulating GaAs, non-intentionally doped, is heated to a temperature T1>600° C.,
a reactive gas (6) interacts chemically with the source material (7) of temperature T1 in order to create volatile products,
said substrate n+(or p+) (2) is heated to a temperature T2<T1,
parallelism and thermal insulation of the substrate n+(or p+) (2) and of the source material (7) are provided,
the thickness d′ of the epitaxial layer (1) is sufficient in order to absorb the X photons efficiently.

### Claim 2 (depends on 1)

A method according to claim 1, characterised in that the ohmic contacts (12) are produced by evaporation of a gold-based alloy, followed by annealing,

### Claim 3 (depends on 1, 2)

A method according to claims 1 and 2, characterised in that the residual doping is reduced by uniform irradiation with approx. 1 MeV electrons and at a dose adjusted as follows: the capacity of an individual detector is measures according to the dose and the irradiation is stopped when the capacity is equal to that of the thickness of the layer d′.

### Claim 4 (depends on 1, 2, 3)

A method according to any of the claims 1 to 3, characterised in that the thickness d′ of the layer depends on the energy of the X photons to be absorbed, but it ranges between 100 μm and 1 mm,

### Claim 5 (depends on 1, 2, 3, 4)

A method according to any of the claims 1 to 4, characterised in that the reactive gas (6) is H2O under partial pressure of several hundred ppm.

### Claim 6 (depends on 1, 2, 3, 4, 5)

A method according to any of the claims 1 to 5, characterised in that the growth is performed under purified hydrogen atmosphere, of the order of the atmospheric pressure.

### Claim 7

A device for producing an electronic GaAS detector for X-ray detection for imaging comprising:
a chamber (14),
k feet (with k≧3) forming a tripod (15) and insulating the chamber (14) thermally from the remainder of the device,
a first plate (16) mounted on the tripod (15) and serving as a base for the remainder of the device,
a first inert plate (17) serving for thermal insulation of the base (16) of the heating means,
a first wafer (18) comprising a duct (19) in order to accommodate therein temperature measuring means (20),
heating means comprising a first power (21) supplied heater (8) and heating a substrate n+(or p+) (2) to a temperature T2>600° C.,
an inert ring (10) of thickness d of the order of a few millimetres, separating and insulating the substrate n+(or p+) (2) and a source material (7) thermally,
a second power (22) supplied heater (9) heating the source material (7) to a temperature T1>T2,
a second wafer (23) comprising a duct (24) in order to accommodate therein temperature measuring means (25),
a second inert plate (26) serving for thermal insulation of a second plate (27) from the remainder of the device.

### Claim 8 (depends on 7)

A device according to claim 7, characterised in that the parallelism of the source material (7) and of the substrate n+(or p+) (2) is ensured in excess of within 0.1 mm by the inert ring of thickness d of the order of a few millimetres,

### Claim 9 (depends on 7, 8)

A device according to claims 7 and 8, characterised in that the inert ring (10) enables gaseous permeability between the space where the reactions take place and the internal atmosphere of the device, H2 purified, containing H2O (6) at controlled pressure.

### Claim 10 (depends on 7, 8, 9)

A device according to any of the claims 7 to 9, characterised in that the chamber (14) is evacuated by a pump (28) before introduction of purified H2 and after deposition of the epitaxial layer in order to filter the products derived from the reaction (6).