# US 2004/0069210 A1 · Method for forming aluminum oxide material used in optical data storage

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0069210 A1
- Document ID: US20040069210A1
- Status: Published application
- Kind: A1
- Application number: 10/309,179
- Filed: 2002-12-04
- Published: 2004-04-15
- Earliest claimed: 2002-10-10
- Assignees: Landauer, Inc.
- Inventors: Mark Akselrod
- Web page: https://patentgrep.com/patent/US20040069210A1

## CPC

- G11B 7/243: comprising inorganic materials only, e.g. ablative layers
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 29/20: Aluminium oxides
- G11B 2007/2431: {group 13 elements (B, Al, Ga, In)}
- G11B 2007/2432: {Oxygen}
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present invention provides aluminum oxide crystalline materials including dopants and oxygen vacancy defects and methods of making such crystalline materials. The crystalline materials of the present invention have particular utility in optical data storage applications.

## Claims

### Claim 1

A method for making a crystalline material comprising the steps of:
(a) doping a base material comprising Al2O3 with a first dopant comprising magnesium to form a doped material; and
(b) crystallizing said doped material in highly reducing atmosphere in order to form said crystalline material, wherein said crystalline material includes a plurality of at least one type of oxygen vacancy defect.

### Claim 2 (depends on 1)

The method of claim 1, wherein step (b) is conducted in highly reducing atmosphere under a partial pressure of oxygen of no greater than 10−3 atm.

### Claim 3 (depends on 1)

The method of claim 1, wherein step (b) is conducted in highly reducing atmosphere under a partial pressure of oxygen of no greater than 10−15 atm.

### Claim 4 (depends on 1)

The method of claim 1, wherein step (b) is conducted in highly reducing atmosphere under a partial pressure of oxygen of about 10−20 atm.

### Claim 5 (depends on 1)

The method of claim 1, wherein step (b) is conducted at a temperature of about 2010° C. to 2090° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein step (b) is conducted at a temperature of about 2050° C.

### Claim 7 (depends on 1)

The method of claim 1, wherein step (b) is conducted at a pulling rate of about 0.1 mm/hour to 600 mm/hour.

### Claim 8 (depends on 1)

The method of claim 1, wherein step (b) is conducted at a pulling rate of about 1 mm/hour to 10 mm/hour.

### Claim 9 (depends on 1)

The method of claim 1, wherein step (b) is conducted at a pulling rate of about 5 mm/hour.

### Claim 10 (depends on 1)

The method of claim 1, wherein step (b) is conducted with seed rotation of about 1 to 50 rpm.

### Claim 11 (depends on 1)

The method of claim 1, wherein step (b) is conducted with seed rotation of about 10 rpm.

### Claim 12 (depends on 1)

The method of claim 1, wherein step (b) is performed at a temperature of about 2050C with a pulling rate of about 5 mm/min and seed rotation of about 10 rpm.

### Claim 13 (depends on 1)

The method of claim 1 said first dopant comprises a Mg compound.

### Claim 14 (depends on 13)

The method of claim 13, wherein said Mg compound comprises MgO.

### Claim 15 (depends on 14)

The method of claim 14, wherein said Mg compound comprises MgO powder.

### Claim 16 (depends on 14)

The method of claim 14, wherein said Mg compound comprises MgO single crystal.

### Claim 17 (depends on 14)

The method of claim 14, wherein MgO comprises of 2 ppm to 5000 ppm of the amount of said base material by weight.

### Claim 18 (depends on 14)

The method of claim 14, wherein MgO comprises 550 ppm of the amount of said base material by weight.

### Claim 19 (depends on 13)

The method of claim 13, wherein said Mg compound comprises MgAl2O4.

### Claim 20 (depends on 19)

The method of claim 19, wherein said Mg compound comprises MgAl2O4 spinel polycrystalline powder.

### Claim 21 (depends on 19)

The method of claim 19, wherein said Mg compound comprises MgAl2O4 crystal.

### Claim 22 (depends on 19)

The method of claim 19, wherein MgAl2O4 comprises of 4 ppm to 10,000 ppm of the amount of said base material by weight.

### Claim 23 (depends on 1)

The method of claim 1, wherein step (a) further comprises doping said base material with a second dopant comprising carbon to form said doped material.

### Claim 24 (depends on 23)

The method of claim 23, wherein said crystalline material comprises Al2O3:C,Mg

### Claim 25 (depends on 23)

The method of claim 23, wherein said step (a) comprises the following sub-steps:
(c) adding a Mg doping material to said Al2O3 base material to form a Mg—Al2O3 material;
(d) forming a Mg—Al2O3 melt from said Mg—Al2O3 material; and
(e) dissolving CO gas in said melt to form said doped material.

### Claim 26 (depends on 25)

The method of claim 25, wherein sub-step (e) is carried out in a gas atmosphere comprising argon and said carbon monoxide comprises of 2 ppm to 50,000 ppm of the amount of argon in the gas atmosphere by volume.

### Claim 27 (depends on 25)

The method of claim 25, wherein said carbon monoxide comprises 8800 ppm of the amount of argon in the gas atmpsphere by volume.

### Claim 28 (depends on 23)

The method of claim 23, wherein step (b) is carried out in an induction heating furnace and step (b) further comprises using a hot graphite succeptor coupled to an inductor of said induction-heating furnace to melt said Al2O3:C,Mg mixture and to solidify said MgAl2O3:C,Mg mixture.

### Claim 29 (depends on 23)

The method of claim 23, wherein said second dopant comprises CO.

### Claim 30 (depends on 23)

The method of claim 23, wherein said base material is doped with said first dopant to form a Mg-doped mixture and said Mg-doped mixture is doped with said second dopant to form said doped material.

### Claim 31 (depends on 23)

The method of claim 23, wherein step (a) further comprises doping said base material with a third dopant comprising hydrogen to form said doped material.

### Claim 32 (depends on 31)

The method of claim 31, wherein said crystalline material comprises Al2O3:C,Mg,H.

### Claim 33 (depends on 31)

The method of claim 31, wherein said base material is doped with said first dopant to form a Mg-doped mixture and said Mg-doped mixture is simultaneously doped with said second dopant and said third dopant to form said doped material.

### Claim at position 34 (depends on 33)

34 The method of claim 33, wherein said Mg-doped mixture is doped with said second dopant and said third dopant while said Mg-doped mixture is heated in a furnace and wherein said first dopant is present in said doped material in a quantity of between 2 and 5000 ppm of base material by weight; said second dopant is present in the gas atmosphere of the furnace during crystallization in a quantity of between 2 and 50,000 ppm by volume; and said third dopant is present in the gas atmosphere of the furnace during crystallization in a quantity of between 100 and 10,000 ppm by volume.

### Claim 35 (depends on 31)

The method of claim 31, wherein said first dopant comprises MgAl2O4 and the amount of MgAl2O4 mixed with said base material is about 4 to 10,000 ppm of the amount of said base material by weight.

### Claim 36 (depends on 31)

The method of claim 31, wherein said first dopant comprises MgAl2O4 and the amount of MgAl2O4 is about 800 ppm of the amount of said base material by weight.

### Claim 37 (depends on 31)

The method of claim 31, wherein said second dopant comprises CO.

### Claim 38 (depends on 31)

The method of claim 31, wherein said third dopant comprises hydrogen gas.

### Claim 39 (depends on 31)

The method of claim 31, wherein step (a) further comprises the sub-steps of:
(c) adding MgAl2O4 material to said base material to form a Mg—Al2O3 material;
(d) forming a Mg—Al2O3 melt from said Mg—Al2O3 material; and
(e) dissolving CO gas and hydrogen gas in said melt to form said doped material.

### Claim 40 (depends on 39)

The method of claim 39, wherein sub-step (e) is carried out in a gas atmosphere comprising argon and wherein CO gas comprises 2 to 50,000 ppm of the amount of argon in the gas atmosphere by volume.

### Claim 41 (depends on 40)

The method of claim 40, wherein CO gas comprises about 8800 ppm of the amount of argon in the gas atmosphere by volume.

### Claim at position 42 (depends on 39)

41 The method of claim 39, wherein sub-step (e) is carried out in a gas atmosphere comprising argon and hydrogen, and hydrogen comprises about 100 to 10,000 ppm of the amount of argon in the gas atmosphere by volume.

### Claim 42 (depends on 39)

The method of claim 39, wherein sub-step (e) is carried out in a gas atmosphere comprising argon and hydrogen, and hydrogen comprises of 1200 ppm of the amount of argon in the gas atmosphere by volume.

### Claim 43 (depends on 1)

The method of claim 1 were said base material is made in the form of a thin film and step (a) comprises producing a first layer comprising a Al2O3 film and depositing at least one second layer comprising a MgO film on said second layer to form said doped material.

### Claim 44 (depends on 43)

The method of claim 43, wherein said method further comprises the steps of:
(c) heating said doped material in a furnace
(c) adding carbon monoxide and hydrogen gas to highly reducing atmosphere of the furnace;
(d) crystallizing said doped material by thermal annealing at temperature above 1200° C., but below 2100° C. for period of time between 1 s and 1800 s.

### Claim 45 (depends on 44)

The method of claim 44, wherein step (d) is performed at about 2000° C. for about 120 S.

### Claim 46 (depends on 1)

The method of claim 1, wherein said crystalline material absorbs light in the range of 205±5 nm and emits luminescent light in the wide emission band around 420±5 nm and with luminescent lifetime about 35±5 ms.

### Claim 47 (depends on 1)

The method of claim 1, wherein said crystalline material absorbs light in the range of 255±5 nm emits luminescent light in the wide emission band around 330±5 nm and with luminescent lifetime shorter than 5 ns.

### Claim 48 (depends on 1)

The method of claim 1, wherein said crystalline material absorbs light in the range of 335±5 nm emits luminescent light in the wide emission band around 750±15 nm and with luminescent lifetime about 80±10 ns.

### Claim 49 (depends on 1)

The method of claim 1, wherein said crystalline material absorbs light in the range of 435±5 nm emits luminescent light in the wide emission band around 520±5 nm and with luminescent lifetime about 9±3 ns.

### Claim 50 (depends on 1)

A crystalline material made according to the method of claim 1.

### Claim 51 (depends on 23)

A crystalline material made according to the method of claim 23.

### Claim 52 (depends on 31)

A crystalline material made according to the method of claim 31.