# US 2004/0056376 A1 · Method for preparing precursors for producing monolithic metal oxide aerogels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0056376 A1
- Document ID: US20040056376A1
- Status: Published application
- Kind: A1
- Application number: 10/253,141
- Filed: 2002-09-23
- Published: 2004-03-25
- Earliest claimed: 2002-09-23
- Assignees: The Regents of the University of California
- Inventors: Paul R. Coronado
- Web page: https://patentgrep.com/patent/US20040056376A1

## CPC

- C03C 1/006: {to produce glass through wet route}
- C01B 33/163: {by hydrolysis of organosilicon compounds, e.g. ethyl orthosilicate}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A method for preparing precursors for producing high density monolithic aerogels. The method enables fabrication of transparent porous glass monoliths, with the porosity or density controlled by adjusting the ratio of water to monomer. By this adjustment, syneresis is increased or minimized. The method involves either a single step precursor or a two step precursor where a base is added to the single step precursor after hydrolysis has occurred. Monolithic metal oxide aerogels with densities between 0.3 g/cc to 1.5 g/cc have been produced using this method.

## Claims

### Claim 1

A method for preparing precursors for producing monolithic metal oxide aerogels, comprising: forming a precursor solution from a monomer and water.

### Claim 2 (depends on 1)

The method of claim 1, additionally including adding an acid to the thus formed solution to stimulate hydrolysis.

### Claim 3 (depends on 2)

The method of claim 2, additionally including forming the precursors solution from 0.5 to about 1.5 mole monomer, about 0.5 to about 30 mole water, and 1.0×10−5 to about 0.5 mole acid.

### Claim 4 (depends on 1)

The method of claim 1, additionally including adding a base after hydrolysis has occurred to expedite condensation of the monomer.

### Claim 5 (depends on 4)

The method of claim 4, additionally including forming the base from at least water and a base material.

### Claim 6 (depends on 5)

The method of claim 5, additionally including adding alcohol to the base.

### Claim 7 (depends on 6)

The method of claim 6, wherein the base comprising of a mixture of about 0.05 mole to about 0.15 mole water, about 0.05 to about 0.15 mole alcohol, and about 1×10−5 to about 5×10−5 mole base material.

### Claim 8 (depends on 7)

The method of claim 7, wherein the base material is selected from the group consisting of NH4OH, NaOH and Acidic Acid.

### Claim 9 (depends on 1)

The method of claim 1, additionally including selecting the monomer from the group consisting of tetraethylorthosilicate, tetramethoxy-silane (TMOS), purified TMOS, and condensed silica (LH, JP, ETHANDTT).

### Claim 10 (depends on 1)

The method of claim 1, additionally including controlling the density or porosity of the aerogel by adjusting the ration of water to monomer in the precursor solution.

### Claim 11

In a method for producing transparent porous glass, the improvement comprising: providing specific refractive indexes by adjusting the ratio of water to monomer in the precursor solution.

### Claim 12 (depends on 11)

The improvement of claim 11, additionally including forming the precursor solution from a single step or a two step operation.

### Claim 13 (depends on 12)

The improvement of claim 12, wherein the single step operation is carried out by adding a quantity of water to a quantity of monomer having a ratio of 0.2-0.6 part water to 1.0 part monomer.

### Claim 14 (depends on 13)

The improvement of claim 13, additionally including adding acid to the water/monomer solution in the ratio of 1.0×10−6 to >0.2 part acid to 1.0 part monomer.

### Claim 15 (depends on 13)

The improvement of claim 13, additionally including controlling the porosity or density of the transparent porous glass by adjusting the ratio of water to monomer.

### Claim 16 (depends on 12)

The improvement of claim 12, additionally including selecting the monomer from the group consisting of TEOS, TMOS, purified TMOS, and condensed silica (LH, JP, ETANDTT).

### Claim 17 (depends on 12)

The method of claim 12, wherein the two step operation is carried out using the single step operation and adding to the water/monomer solution a quantity of base.

### Claim 18 (depends on 17)

The method of claim 17, wherein adding the quantity of base is carried out after hydrolysis of the water/monomer solution to expedite condensation of the solution.

### Claim 19 (depends on 18)

The method of claim 18, additionally including forming the base from a mixture of at least water and a base material in the ratio of 0.10 part water to 3.0×10−5 part base material.

### Claim 20 (depends on 19)

The method of claim 19, additionally including adding to the mixture of water and a base material a quantity of alcohol is the ratio 0.10 part alcohol to 1.0 part water.

### Claim 21 (depends on 20)

The method of claim 20, additionally including selecting the base material from the group consisting of NH4OH, NaOH and Acidic Acid.

### Claim 22

In a method for producing monolithic metal oxide aerogels, the improvement comprising: forming the aerogels with densities in the range of 0.3 g/cc to 1.5 g/cc, and wherein the forming operation includes adjusting a ratio of water to monomer in the formation of a precursor solution.

### Claim 23 (depends on 22)

The improvement of claim 22, additionally including injecting the precursor solution into a sealed mold, and allowing the solution to gel, thereby forming a net-shape aerogel monolith.