# US 2004/0055748 A1 · Elastomeric admixtures for improving cement elasticity

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0055748 A1
- Document ID: US20040055748A1
- Status: Published application
- Kind: A1
- Application number: 10/246,943
- Filed: 2002-09-19
- Published: 2004-03-25
- Earliest claimed: 2002-09-19
- Inventors: B. Raghava Reddy; Krishna M. Ravi
- Web page: https://patentgrep.com/patent/US20040055748A1

## CPC

- C04B 24/2652: {Nitrogen containing polymers, e.g. polyacrylamides, polyacrylonitriles}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C09K 8/46: containing inorganic binders, e.g. Portland cement
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A method and cementing composition is provided for sealing a subterranean zone penetrated by a well bore, wherein the cementing composition comprises a mixture of cementitious material, acrylonitrile butadiene styrene (ABS), and sufficient water to form a slurry.

## Claims

### Claim 1

A method of sealing a subterranean zone penetrated by a well bore comprising:
preparing a cementing composition comprising cement, acrylonitrile butadiene styrene polymer, and water;
placing the cementing composition into the subterranean zone; and
allowing the cementing composition to set therein.

### Claim 2 (depends on 1)

The method of claim 1 wherein the cementing composition further comprises silica flour.

### Claim 3 (depends on 1)

The method of claim 1 wherein the cement is Portland cement, pozzolan cement, gypsum cement, aluminous cement, silica cement, or alkaline cement.

### Claim 4 (depends on 1)

The method of claim 1 wherein the acrylonitrile butadiene styrene polymer is made with a 70% polybutadiene substrate.

### Claim 5 (depends on 1)

The method of claim 1 wherein the acrylonitrile butadiene styrene polymer is made with a 65% styrene-butadiene rubber substrate.

### Claim 6 (depends on 1)

The method of claim 1 wherein the acrylonitrile butadiene styrene polymer is made with a 35% styrene-butadiene rubber substrate.

### Claim 7 (depends on 1)

The method of claim 1 wherein the acrylonitrile butadiene styrene polymer is present in a range of 5% to 30% by weight of the cement.

### Claim 8 (depends on 1)

The method of claim 1 wherein the water is present in a range of 38% to 70% by weight of the cement.

### Claim 9

A cementing composition for sealing a subterranean zone penetrated by a well bore comprising:
cement, acrylonitrile butadiene styrene polymer, and water.

### Claim 10 (depends on 9)

The composition of claim 9 further comprising silica flour.

### Claim 11 (depends on 9)

The composition of claim 9 wherein the cement is Portland cement, pozzolan cement, gypsum cement, aluminous cement, silica cement, or alkaline cement.

### Claim 12 (depends on 9)

The composition of claim 9 wherein the acrylonitrile butadiene styrene polymer is made with a 70% polybutadiene substrate.

### Claim 13 (depends on 9)

The composition of claim 9 wherein the acrylonitrile butadiene styrene polymer is made with a 65% styrene-butadiene rubber substrate.

### Claim 14 (depends on 9)

The composition of claim 9 wherein the acrylonitrile butadiene styrene polymer is made with a 35% styrene-butadiene rubber substrate.

### Claim 15 (depends on 9)

The composition of claim 9 wherein the acrylonitrile butadiene styrene polymer is present in a range of 5% to 30% by weight of the cement.

### Claim 16 (depends on 9)

The composition of claim 9 wherein the water is present in a range of 38% to 70% by weight of the cement.

### Claim 17

A method of sealing a subterranean zone penetrated by a well bore comprising:
preparing a cementing composition comprising cement, acrylonitrile butadiene styrene polymer, and water, wherein the acrylonitrile butadiene styrene polymer is present in a range of 5% to 30% by weight of the cement;
placing the cementing composition into the subterranean zone; and
allowing the cementing composition to set therein.

### Claim 18 (depends on 17)

The method of claim 17 wherein the cement is Portland cement, pozzolan cement, gypsum cement, aluminous cement, silica cement, or alkaline cement.

### Claim 19 (depends on 17)

The method of claim 17 wherein the acrylonitrile butadiene styrene polymer is made with a 70% polybutadiene substrate.

### Claim 20 (depends on 17)

The method of claim 17 wherein the acrylonitrile butadiene styrene polymer is made with a 65% styrene-butadiene rubber substrate.

### Claim 21 (depends on 17)

The method of claim 17 wherein the acrylonitrile butadiene styrene polymer is made with a 35% styrene-butadiene rubber substrate.

### Claim 22 (depends on 17)

The method of claim 17 wherein the water is present in a range of 38% to 70% by weight of the cement.

### Claim 23 (depends on 17)

The method of claim 17 wherein the cementing composition further comprises silica flour.