# US 2004/0025558 A1 · Hot rolling thin strip

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0025558 A1
- Document ID: US20040025558A1
- Status: Published application
- Kind: A1
- Application number: 10/296,354
- Filed: 2002-12-31
- Published: 2004-02-12
- Earliest claimed: 2000-05-26
- Assignees: Castrip, LLC
- Inventors: John Albert Ziegelaar; Michael Angel Lopez; Andrew Edward Dixon
- Web page: https://patentgrep.com/patent/US20040025558A1

## CPC

- B21B 37/28: Control of flatness or profile during rolling of strip, sheets or plates
- B21B 1/26: by hot-rolling {, e.g. Steckel hot mill}
- B21B 1/463: {in a continuous process, i.e. the cast not being cut before rolling}
- B21B 37/48: Tension control; Compression control
- B21B 37/56: Elongation control
- B21B 39/006: {Pinch roll sets}
- B21B 39/08: Braking or tensioning arrangements
- B21B 45/008: {Heat shields}
- B21B 2001/225: {by hot-rolling}
- B21B 2265/04: Front or inlet tension
- B21B 2265/08: Back or outlet tension
- Y02P 70/10: Greenhouse gas [GHG] capture, material saving, heat recovery or other energy efficient measures, e.g. motor control, characterised by manufacturing processes, e.g. for rolling metal or metal working
- Y10T 29/49991: Combined with rolling
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Thin steel strip is passed through a pinch roll stand comprising pinch rolls to a rolling mill comprising a pair of work rolls and upper and lower backing rolls. Strip passes through the bite between the work rolls and strip squeezing forces are applied between the work rolls to reduce the thickness of the strip. The pinch rolls apply tension to the strip passing to the work rolls. In order to minimize generation of crimping defects in the strip, the tension applied by the pinch rolls is high enough to ensure no part of the strip entering the work rolls is in longitudinal compression such as to exceed the buckling stress of the strip. The applied tension is sufficiently low as to produce no more than 1% strip elongation through creep. The strip may be hot rolled by the work rolls at a temperature in the range of 700° C.-1200° C.

## Claims

### Claim 1

A method of hot rolling thin steel strip comprising:
feeding the strip through a roll bite between a pair of work rolls,
applying strip squeezing forces between the work rolls to reduce the thickness of the strip,
and applying tension to the strip passing to the work rolls sufficiently high to avoid buckling stress in the strip entering the work rolls, and sufficiently low as to produce no more than 1% strip elongation through creep.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein the strip is no more than 3 mm thick prior to feeding to the work rolls.

### Claim 3 (depends on 2)

A method as claimed in claim 2, wherein the strip thickness is in the range of 0.5 mm to 2 mm prior to feeding to the work rolls.

### Claim 4 (depends on 1)

A method as claimed in claim 1, wherein the strip is hot rolled at a temperature in the range of 700° C. to 1200° C.

### Claim 5 (depends on 2)

A method as claimed in claim 2, wherein the strip is hot rolled at a temperature in the range of 700° C. to 1200° C.

### Claim 6 (depends on 3)

A method as claimed in claim 3, wherein the strip is hot rolled at a temperature in the range of 700° C. to 1200° C.

### Claim 7 (depends on 4)

A method as claimed in claim 4, wherein the strip is hot rolled at a temperature in the range 900° C. to 1200° C.

### Claim 8 (depends on 5)

A method as claimed in claim 5, wherein the strip is hot rolled at a temperature in the range 900° C. to 1200° C.

### Claim 9 (depends on 6)

A method as claimed in claim 6, wherein the strip is hot rolled at a temperature in the range 900° C. to 1200° C.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the applied tension is such as to limit the strip elongation through creep to no more than 0.5%.

### Claim 11 (depends on 1)

A method according to claim 1, wherein the variation in strip thickness reduction across the strip as imposed by the work rolls is such that the strip shape defects downstream of the work rolls are no more than 400 I-units.

### Claim 12 (depends on 11)

A method according to claim 11, wherein said variation in strip thickness reduction is such that the strip shape defects downstream of the work rolls is no more than 200 I-units.

### Claim 13 (depends on 1)

A method according to claim 1, wherein tension is applied to the strip by passing said strip through a pair of pinch rolls in advance of the work rolls.

### Claim 14 (depends on 1)

A method according to claim 1, wherein the strip is a manganese/silicon killed steel strip of thickness in the range 0.5 mm to 3 mm,
the strip is hot rolled in the temperature range 900° C. to 1200° C.,
and the applied tension is within an operating range between maximum and minimum values defined by:
tension max=maximum allowable elongation at the rolling temperature, and
tension min=maximum strip buckle stress allowable at the rolling temperature.

### Claim 15

A method of hot rolling thin steel strip produced by direct casting by a twin roll caster comprising:
feeding the strip through a roll bite between a pair of work rolls,
applying strip squeezing forces between the work rolls to reduce the thickness of the strip,
and applying tension to the strip passing to the work rolls sufficiently high to avoid buckling stress in the strip entering the work rolls, and sufficiently low as to produce no more than 1% strip longation through cre p.

### Claim 16 (depends on 15)

A method as claimed in claim 15, wherein the strip is no more than 3 mm thick prior to feeding to the work rolls.

### Claim 17 (depends on 16)

A method as claimed in claim 16, wherein the strip thickness is in the range of 0.5 mm to 2 mm prior to feeding to the work rolls.

### Claim 18 (depends on 15)

A method as claimed in claim 15, wherein the strip is hot rolled at a temperature in the range of 700° C. to 1200° C.

### Claim 19 (depends on 16)

A method as claimed in claim 16, wherein the strip is hot rolled at a temperature in the range of 700° C. to 1200° C.

### Claim 20 (depends on 17)

A method as claimed in claim 17, wherein the strip is hot rolled at a temperature in the range of 700° C. to 1200° C.

### Claim 21 (depends on 18)

A method as claimed in claim 18, wherein the strip is hot rolled at a temperature in the range 900° C. to 1200° C.

### Claim 22 (depends on 19)

A method as claimed in claim 19, wherein the strip is hot rolled at a temperature in the range 900° C. to 1200° C.

### Claim 23 (depends on 20)

A method as claimed in claim 20, wherein the strip is hot rolled at a temperature in the range 900° C. to 1200° C.

### Claim 24 (depends on 15)

A method according to claim 15, wherein the applied tension is such as to limit the strip elongation through creep to no more than 0.5%.

### Claim 25 (depends on 15)

A method according to claim 15, wherein the variation in strip thickness reduction across the strip as imposed by the work rolls is such that the strip shape defects downstream of the work rolls are no more than 400 I-units.

### Claim 26 (depends on 25)

A method according to claim 25, wherein said variation in strip thickness reduction is such that the strip shape defects downstream of the work rolls is no more than 200 I-units.

### Claim 27 (depends on 15)

A method according to claim 15, wherein tension is applied to the strip by passing said strip through a pair of pinch rolls in advance of the work rolls.

### Claim 28 (depends on 15)

A method according to claim 15, wherein the strip is a manganese/silicon killed steel strip of thickness in the range 0.5 mm to 3 mm,
the strip is hot rolled in the temperature range 900° C. to 1200° C.,
and the applied tension is within an operating range between maximum and minimum values defined by:
tension max=maximum allowable elongation at the rolling temperature, and
tension min=maximum strip buckle stress allowable at the rolling temperature.