# US 2004/0024283 A1 · Lead projectile mineral coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0024283 A1
- Document ID: US20040024283A1
- Status: Published application
- Kind: A1
- Application number: 10/209,517
- Filed: 2002-07-30
- Published: 2004-02-05
- Earliest claimed: 2002-07-30
- Inventors: Keith E. Forrester
- Web page: https://patentgrep.com/patent/US20040024283A1

## CPC

- A62D 3/33: by chemical fixing the harmful substance, e.g. by chelation or complexation
- A62D 2101/43: containing heavy metals, in the bonded or free state
- A62D: CHEMICAL MEANS FOR EXTINGUISHING FIRES OR FOR COMBATING OR PROTECTING AGAINST HARMFUL CHEMICAL AGENTS; CHEMICAL MATERIALS FOR USE IN BREATHING APPARATUS

## Abstract

The invention pertains to a method for reducing the leaching of lead from lead projectile surface. The method includes contacting the lead projectile surface with a lead stabilizing agent or a lead stabilizing agent in the presence of a lead mineral complexing agent. The lead stabilizing agents provides a means to stabilize lead on the bullet/shot surface and thus reduce lead leaching and contact to the environment. This method eliminates the need to remove or re-treat range soils and greatly reduces the environmental and health risks associated with the use of lead as projectiles in the open environment as well as at control trap ranges.

## Claims

### Claim 1

A method of reducing the leaching of lead from the surface of a lead projectile, comprising contacting lead projectile surface with at least one lead stabilizing agent in an amount effective in reducing the leaching of lead from lead projectile surface to a level no more than 5.0 ppm lead as determined in an EPA TCLP test, said test performed on the projectile impact area lead contaminated soils or lead contaminated material receiving the projectile, as set forth in the Federal Register, vol. 55, no. 126, pp. 26985-26998 (Jun. 29, 1990).

### Claim 2 (depends on 1)

The method of claim 1, wherein the lead stabilizing agent is selected from the group consisting of water soluble phosphate, phosphate in the presence of lead mineral complexing agent, phosphoric acid, wet process amber phosphoric acid, wet process green phosphoric acid, coproduct phosphoric acid solution from aluminum polishing, technical grade phosphoric acid, merchant grade phosphoric acid, hypophosphoric acid, metaphosphoric acid, pyrophosphoric acid, hexametaphosphate, polyphosphate, tetrapotassium polyphosphate, calcium orthophosphate, superphosphate, triple superphosphate, phosphate fertilizer, phosphate rock, bone phosphate, fishbone apatite, monocalcium phosphate, monoammonia phosphate, diammonium phosphate, dicalcium phosphate, tricalcium phosphate, trisodium phosphate, salts of phosphoric acid, pulverized phosphate rock, dolomitic limestone, hydrated limestone, calcium oxide, calcium carbonate, magnesium oxide, sodium metasilicate, potassium silicate, phosphorite, herring meal, bone meal and combinations thereof.

### Claim 3 (depends on 2)

The method of claim 2, wherein the salts of phosphoric acid are alkali metal salts.

### Claim 4 (depends on 2)

The method of claim 2, wherein the phosphate is a trisodium phosphate, dicalcium phosphate, disodium hydrogen phosphate, sodium dihydrogen phosphate, tripotassium phosphate, dipotassium hydrogen phosphate, potassium dihydrogen phosphate, trilithium phosphate, dilithium hydrogen phosphate, lithium dihydrogen phosphate or mixtures thereof.

### Claim 5 (depends on 2)

The method of claim 2, wherein the phosphate and lead mineral complexing agent as iron, calcium, chloride, or aluminum are supplied as one product including triple superphosphate and combination fertilizer wet process mixtures.

### Claim 6 (depends on 2)

The method of claim 2, wherein the lead mineral complexing agent is selected from the group consisting of calcium, silicates, sodium silicate, lime, magnesium oxides, calcium chloride, sodium chloride, potassium chloride, vanadium, boron, iron, surfactant, aluminum, sulfates, ferric sulfate, and combinations thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the phosphate is dicalcium phosphate in the presence of calcium chloride.

### Claim 8 (depends on 1)

The method of claim 1, wherein the phosphate is amber phosphoric acid.

### Claim 9 (depends on 1)

The method of claim 1, wherein the phosphate is green phosphoric acid.

### Claim 10 (depends on 1)

The method of claim 1, wherein the phosphate is fishbone apatite.

### Claim 11 (depends on 1)

The method of claim 1, wherein the phosphate is a slurry of dicalcium phosphates.

### Claim 12 (depends on 1)

The method of claim 1, wherein the phosphate is tricalcium phosphate.

### Claim 13 (depends on 1)

The method of claim 1, wherein the phosphate is pulverized triple superphosphate.

### Claim 14

A method of reducing the leaching of lead from the surface of a lead projectile, comprising contacting lead projectile surface with at least one lead stabilizing agent and optionally a lead mineral complexing agent, in an amount effective in reducing the leaching of lead from lead projectile surface under natural or induced lead leaching conditions.

### Claim 15

A method of reducing the leaching of lead from the surface of a lead projectile, comprising contacting lead projectile surface with at least one lead stabilizing agent and optionally a lead mineral complexing agent, in an amount effective in reducing the leaching of lead from lead projectile surface, to a level of 50 ppb as determined by Simulated Precipitant Leaching Procedure method 1310 or water leach test.

### Claim 16

A method of reducing bioavailability of lead by reducing Pb solubility from the surface of a lead-containing projectile, comprising contacting lead projectile surface with at least one lead stabilizing agent and optionally a lead mineral complexing agent, in an amount effective in reducing the leaching of lead from lead projectile surface under natural or induced lead leaching conditions.

### Claim 17

A lead-containing projectile having coated thereon at least one lead stabilizing agent and optionally a lead mineral complexing agent, in an amount effective in reducing the leaching of lead from lead projectile surface under natural or induced lead leaching conditions, whereby the lead and stabilizing agent form a mineral coating on the projectile in which the lead is in a form that is less soluble than its uncoated counterpart.

### Claim 18 (depends on 17)

The lead-containing projectile of claim 17 wherein the projectile is in the form of pellets or shot and the stabilizing agent is dicalcium phosphate, tricalcium phosphate or combination thereof.

### Claim 19

A method of producing a lead-containing projectile having a mineral coating thereon, comprising:
coating lead-containing projectile with at least one lead stabilizing agent and optionally a lead mineral complexing agent, in an amount effective in reducing the leaching of lead from lead projectile surface under natural or induced lead leaching conditions; and
allowing the coating to cure,
wherein the lead and stabilizing agent form a mineral coating on the projectile in which the lead is in a form that is less soluble than its uncoated projectile counterpart.