# US 2004/0023577 A1 · Method and device for manufacturing electret processed product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0023577 A1
- Document ID: US20040023577A1
- Status: Published application
- Kind: A1
- Application number: 10/399,681
- Filed: 2003-04-21
- Published: 2004-02-05
- Earliest claimed: 2001-06-18
- Assignees: Toray Industries, Inc.
- Inventors: Hiroyoshi Horiguchi; Masaaki Takeda
- Web page: https://patentgrep.com/patent/US20040023577A1

## CPC

- D06M 13/535: Suction; Vacuum treatment; Degassing; Blowing
- B01D 39/1623: {of synthetic origin}
- D06M 11/05: with water, e.g. steam; with heavy water
- Y10T 442/20: Coated or impregnated woven, knit, or nonwoven fabric which is not [a] associated with another preformed layer or fiber layer or, [b] with respect to woven and knit, characterized, respectively, by a particular or differential weave or knit, wherein the coating or impregnation is neither a foamed material nor a free metal or alloy layer
- D06M: TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS, FABRICS, FEATHERS OR FIBROUS GOODS MADE FROM SUCH MATERIALS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A manufacturing method of an electret processed product, comprising the steps of allowing a section nozzle (22) to come into contact with a nonconductive fiber sheet (S) so as to cross in the lateral direction of the sheet while running the sheet, allowing the surface of the sheet on the opposite side of the contact portion to come into contact with or to immerse into a water surface, sucking water from the suction nozzle (22) so that the water can be passed through the sheet in the thickness direction of the sheet to penetrate the water into the nonconductive fiber sheet (S), and drying the nonconductive fiber sheet (S), whereby a high quality and high performance electret processed product can be manufactured at a low cost.

## Claims

### Claim 1

The manufacturing method of an electret processed product, comprising the steps of:
allowing a suction nozzle to come into contact with a nonconductive fiber sheet so as to cross in the lateral direction of the sheet while running the sheet;
allowing the surface of the sheet on the opposite side of the contact portion to come into contact with or to immerse into a water surface;
sucking water from the suction nozzle so that the water can be passed through the sheet in the thickness direction of the sheet to penetrate the water into the nonconductive fiber sheet; and
drying the nonconductive fiber sheet.

### Claim 2 (depends on 1)

The manufacturing method of an electret processed product as claimed in claim 1, wherein a dewatering process is interposed between said penetration process and drying process.

### Claim 3 (depends on 2)

The manufacturing method of an electret processed product as claimed in claim 2, wherein said penetration process and dewatering process are repeated at least twice.

### Claim 4 (depends on 1, 2, 3)

The manufacturing method of an electret processed product as claimed in claim 1, 2 or 3, wherein the permeability of water to said nonconductive fiber sheet by said penetration process is 500% or more.

### Claim 5 (depends on 1, 2)

The manufacturing method of an electret processed product as claimed in claim 1, 2, or 3, wherein a suction port of said suction nozzle is in a slit-shape.

### Claim 6 (depends on 1, 2, 3)

The manufacturing method of an electret processed product as claimed in claim 1, 2 or 3, wherein said nonconductive fiber sheet contains a hindered amine-based additive or triazine additive by 0.5 to 5% by weight.

### Claim 7 (depends on 1, 2, 3)

The manufacturing method of an electret processed product as claimed in claim 1, 2 or 3, wherein said nonconductive fiber sheet is made of synthetic fibers.

### Claim 8 (depends on 7)

The manufacturing method of an electret processed product as claimed in claim 7, wherein said sheet made of synthetic fibers is melt blown nonwoven fabric.

### Claim 9 (depends on 7)

The manufacturing method of an electret processed product as claimed in claim 7, wherein said sheet made of synthetic fibers is spunbonded nonwoven fabric.

### Claim 10 (depends on 7)

The manufacturing method of an electret processed product as claimed in claim 7, wherein said nonconductive fiber sheet is composed mainly of polyolefin.

### Claim 11 (depends on 7)

The manufacturing method of an electret processed product as claimed in claim 7, wherein said polyolefin is composed mainly of polypropylene.

### Claim 12 (depends on 7)

The manufacturing method of an electret processed product as claimed in claim 7, wherein said nonconductive fiber sheet is composed mainly of polylactic acid.

### Claim 13 (depends on 1, 2, 3)

The manufacturing method of an electret processed product as claimed in claim 1, 2 or 3, wherein said water is demineralized water, distilled water or filtered water by a reverse osmosis membrane.

### Claim 14 (depends on 1, 2, 3)

The manufacturing method of an electret processed product as claimed in claim 1, 2 or 3, wherein said water contains a water soluble organic solvent.

### Claim 15 (depends on 14)

The manufacturing method of an electret processed product as claimed in claim 14, wherein said water soluble organic solvent has a boiling point lower than that of water.

### Claim 16 (depends on 14)

The manufacturing method of an electret processed product as claimed in claim 14, wherein said water soluble organic solvent contains mainly alcohols or ketones.

### Claim 17 (depends on 16)

The manufacturing method of an electret processed product as claimed in claim 16, wherein said water soluble organic solvent is at least one kind of isopropyl alcohol, ethyl alcohol and acetone.

### Claim 18

A device for manufacturing an electret processed product, comprising in a continuous arrangement:
papermaking means for manufacturing a nonconductive fiber sheet;
a water penetrating means, corresponding to the nonconductive fiber sheet, for allowing a suction nozzle to come into contact with a nonconductive fiber sheet so as to cross in the lateral direction of the sheet, allowing the surface of the sheet on the opposite side of the contact portion to come into contact with or to immerse into a water surface, and sucking water from the suction nozzle; and
drying means for drying the nonconductive fiber sheet.

### Claim 19 (depends on 18)

The device for manufacturing an electret processed product as claimed in claim 18, wherein a suction port of said suction nozzle is in a slit-shape.