# US 2004/0018930 A1 · Sealing glass composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0018930 A1
- Document ID: US20040018930A1
- Status: Published application
- Kind: A1
- Application number: 10/205,657
- Filed: 2002-07-25
- Published: 2004-01-29
- Earliest claimed: 2002-07-25
- Assignees: Nortel Networks Limited
- Inventors: Kenneth Snowdon; Christopher Tanner; Timothy Durrant; Christopher Woodend
- Web page: https://patentgrep.com/patent/US20040018930A1

## CPC

- C03C 8/14: Glass frit mixtures having non-frit additions, e.g. opacifiers, colorants, mill-additions
- C03C 8/245: {containing more than 50% lead oxide, by weight}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A glass composition for a seal consists essentially of 70-75 wt % of PbO, 3-7 wt % of PbF2, 5-8 wt % of Bi2O3, 5-7 wt % of B203, 2-5 wt % of ZnO, 1-3 wt % of Fe2O3, 0-2 wt % of CuO, 0-2% of TeO2, and a trace <0.2% of MnO2, the composition having a flow temperature of <350° C. Such seals can be flowed at low temperatures, using different and less environmentally damaging constituents to those used before. Damage to temperature sensitive materials near the seals, can be reduced. Low flow temperatures can be achieved without excessive degradation of properties such as low viscosity, low expansion coefficient, good adhesion to glass and metals, low permeability of air, good long term hydrolytic stability. A filler such as a ceramic powder, is added to match the temperature expansion coefficient to the materials being sealed. It can be used to fix silica fiber into electro-optic devices to achieve hermetic joints with high mechanical stability.

## Claims

### Claim 1

A glass composition suitable for use as a component of a sealing composition, the glass composition consisting essentially of:
70-75 wt % of PbO,
3-7 wt % of PbF2,
5-8 Wt % of Bi2O3,
5-7 wt % of B203,
2-7 wt %of ZnO,
1-3 wt % of Fe2O3,
0-2 wt % of CuO,
0-3 wt % of TeO2, and
a trace <0.2 wt % of MnO2, the composition having a flow temperature of <350° C.

### Claim 2 (depends on 1)

The glass composition of claim 1, having a temperature coefficient of expansion of between 4 and 16 ppm/° C.

### Claim 3 (depends on 1)

The glass composition of claim 1, having one or more of V2O5, P2O5, TeO2, SnO2, Co3O4, Li2O, As2O3, Sb2O3.

### Claim 4 (depends on 1)

The glass composition of claim 1, having 7 wt % B2O3, 8 wt % Bi2O3, 7 wt % ZnO, 5 wt % PbF2, and 3 wt % TeO2.

### Claim 5 (depends on 1)

The glass composition of claim 1, having 6 to 7 wt % B2O3, 6 to 7 wt % Bi2O3, 3 to 4 wt % ZnO, 5 to 6 wt % F, 1 to 2 wt % TeO2, 0.1 to 0.15 wt % MnO2 2 to 3 wt % Fe2O3 and 1 to 2 wt % CuO.

### Claim 6 (depends on 1)

A sealing composition comprising 70-99 wt % of the glass composition of claim 1, and 1-30 wt % of a ceramic filler, the resulting combination of glass/tiller compositions having a TCE of 1 to 5 ppm/° C. and a flow temperature of less than 400° C.

### Claim 7 (depends on 6)

The sealing composition of claim 6, having sufficient adhesion to glass and to metal to enable a glass fiber sealed to metal, to withstand a bend test of 3 mm deflection of the fiber, 2 mm away from the seal.

### Claim 8 (depends on 6)

The sealing composition of claim 6 having a durability sufficient to maintain seal hermeticity <1×10−9 Atmos cc/s without optical power losses of packaged devices tested for 2000 hrs at 85° C. and 85% relative humidity.

### Claim 9

A glass composition consisting essentially of:
70-75 wt % of PbO,
3-7 wt % of PbF2,
5-8 wt % of Bi2O3
5-7 wt % of B203
2-5 wt % of ZnO
1-3 wt % of Fe2O3
0-2 wt % of CuO
0-2% of TeO2
and a trace <0.2% of MnO2.

### Claim 10 (depends on 6)

A method of manufacturing the sealing composition of claim 6, comprising the steps of: mixing the PbO, and metal oxide components, and reacting the mixture with ammonium bifluoride to create PbF21 and adding the low TCE ceramic filler.

### Claim 11 (depends on 6)

A method of manufacturing a seal using the sealing composition of claim 6, comprising the steps of placing a preform of the sealing composition of claim 6 over a gap to be sealed, and applying localized heating to cause the preform to flow into the gap.

### Claim 12 (depends on 12)

The method of claim 12, the localized heating being one of induction heating or laser heating.

### Claim 13 (depends on 6)

An optical component having a fiber and a package, the fiber being sealed to the package using the sealing composition of claim 6.

### Claim 14 (depends on 6)

A method of offering a data transmission service over an optical network along an optical fiber sealed using the composition of claim 6.