# US 2004/0018708 A1 · Method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0018708 A1
- Document ID: US20040018708A1
- Status: Published application
- Kind: A1
- Application number: 10/395,724
- Filed: 2003-03-24
- Published: 2004-01-29
- Earliest claimed: 2002-03-25
- Assignees: Elpida Memory, Inc.
- Inventors: Kazuo Ogawa; Kiyonori Ohyu; Kensuke Okonogi; Toshihiro Imamura; Keiichi Watanabe; Hiroyuki Ohta
- Web page: https://patentgrep.com/patent/US20040018708A1

## CPC

- H10D 64/01354: {passivation or protection of the electrode, e.g. using re-oxidation}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

In a method for manufacturing a semiconductor device having a laminated gate electrode, a phosphorus-doped polysilicon is formed on a gate oxide film. A high-melting metal or a compound of a high-melting metal and silicon is formed on the polysilicon. Phosphorus is doped into the polysilicon so that a concentration of the phosphorus in the polysilicon at an interface between the polysilicon and the gate oxide film is 2×1020 (1/cm3) or less. Then, thermal oxidation is carried out in a wet-hydrogen atmosphere containing water vapor.

## Claims

### Claim 1

A method for manufacturing a semiconductor device having a laminated gate electrode, comprising:
forming a phosphorus-doped polysilicon on a gate oxide film;
forming a high-melting metal or a compound of a high-melting metal and silicon on the polysilicon:
doping phosphorus into the polysilicon so that a concentration of the phosphorus in the polysilicon at an interface between the polysilicon and the gate oxide film is 2×1020 (1/cm3) or less; and
carrying out thermal oxidation in a wet-hydrogen atmosphere containing water vapor.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein:
the wet-hydrogen atmosphere is a mixed atmosphere of H2O and H2.

### Claim 3 (depends on 1)

A method as claimed in claim 1, wherein;
the wet-hydrogen atmosphere contains 5 to 10% of water vapor, and
the thermal oxidation is carried out under conditions of a temperature of 800 to 900° C. and a film thickness of 3 to 5 nm.

### Claim 4 (depends on 1)

A method as claimed in claim 1; wherein:
a bird's beak is formed in a lower end of the polysilicon during the thermal oxidation in the wet-hydrogen atmosphere.

### Claim 5 (depends on 4)

A method as claimed in claim 4, wherein:
the bird's beak is formed so as to reduce a concentration of an electric field in the end of the polysilicon.

### Claim 6 (depends on 4)

A method as claimed in claim 4, wherein:
the phosphorus is doped so as to suppress a reduction in adhesion strength between the polysilicon and the gate oxide film caused by a stress of the bird's beak.

### Claim 7 (depends on 1)

A method as claimed in claim 1, wherein:
the concentration of the phosphorus in the polysilicon is substantially uniform toward an upper layer of the gate electrode.

### Claim 8 (depends on 7)

A method as claimed in claim 7, wherein;
the concentration of the phosphorus is equal to 1×1020 (1/cm3).

### Claim 9 (depends on 1)

A method as claimed in claim 1., wherein:
the concentration of the phosphorus in the polysilicon is continuously or discontinuously increased toward an upper layer of the gate electrode.

### Claim 10 (depends on 1)

A method as claimed in claim 1, wherein,
the high-melting metal contains tungsten.
