# US 2004/0018696 A1 · Method of filling an opening in a material layer with an insulating material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0018696 A1
- Document ID: US20040018696A1
- Status: Published application
- Kind: A1
- Application number: 10/403,584
- Filed: 2003-03-31
- Published: 2004-01-29
- Earliest claimed: 2002-07-26
- Assignees: Advanced Micro Devices, Inc.
- Inventors: Karsten Wieczorek; Stephan Kruegel; Michael Raab
- Web page: https://patentgrep.com/patent/US20040018696A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- Y10S 438/933: Germanium or silicon or Ge-Si on III-V
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The filling of sub-0.25 μm trenches with dielectric material may lead to the formation of a void. Typically, the void may be closed by oxidation. When the trench includes non-oxidizable sidewall portions, insufficient closure may result. Therefore, an oxidizable spacer layer is conformally deposited prior to depositing the bulk dielectric, so that the sidewalls of the trench may be oxidized along the entire depth of the trench, thereby allowing the complete closure of the void.

## Claims

### Claim 1

A method of filling a trench formed in a substrate, the method comprising:
conformally depositing a spacer layer comprised of oxidizible material on said substrate and in said trench;
depositing a dielectric material over said spacer layer to fill said trench; and
performing an oxidation process in an oxidizing ambient to convert at least a portion of said spacer layer into an insulating layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein said spacer layer is substantially completely oxidized.

### Claim 3 (depends on 1)

The method of claim 1, further comprising anisotropically etching said spacer layer prior to depositing said dielectric material.

### Claim 4 (depends on 3)

The method of claim 3, further comprising forming an etch stop layer prior to depositing said spacer layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein performing said oxidation process converts at least a portion of said spacer layer to silicon dioxide.

### Claim 6 (depends on 4)

The method of claim 4, wherein said spacer layer is anisotropically etched to form sidewall spacers in said trench.

### Claim 7 (depends on 1)

The method of claim 1, wherein said substrate comprises at least one non-oxidizable insulating layer formed thereon, whereby said trench is formed in said at least one insulating layer and partially in said substrate.

### Claim 8 (depends on 1)

The method of claim 1, wherein said trench has at least one lateral dimension of 0.25 μm or less.

### Claim 9 (depends on 1)

The method of claim 1, wherein a depth of said trench is in the range of approximately 200-700 nm.

### Claim 10 (depends on 1)

The method of claim 1, wherein said substrate comprises a semiconductor layer and a non-oxidizable insulating layer formed on said semiconductor layer, whereby said trench is formed in said insulating layer and at least partially in said semiconductor layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein said semiconductor layer comprises at least one of silicon and germanium.

### Claim 12 (depends on 10)

The method of claim 10, wherein said insulating material comprises silicon nitride.

### Claim 13 (depends on 1)

The method of claim 1, wherein said dielectric material is an oxide of a semiconductive material.

### Claim 14

A method of filling a trench formed in a substrate with a dielectric material, the method comprising:
forming spacer elements on sidewalls of said trench, said spacer elements being comprised of an oxidizable material;
depositing a dielectric material over said substrate to substantially fill said trench; and
exposing said substrate to an oxidizing ambient to convert at least a portion of said spacer elements into an insulating layer.

### Claim 15 (depends on 14)

The method of claim 14, wherein forming said spacer elements comprises depositing a spacer layer on said substrate and in said trench and anisotropically etching said spacer layer to remove said spacer layer at the bottom of said trench.

### Claim 16 (depends on 15)

The method of claim 15, further comprising forming an etch stop layer prior to depositing said spacer layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein said etch stop layer is formed by oxidizing said substrate to form an oxide layer within said trench.

### Claim 18 (depends on 14)

The method of claim 14, wherein said substrate comprises an insulating layer stack formed on a semiconductive layer, wherein said trench is formed in said insulating layer stack and at least partially in said semiconductive layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein said insulating layer stack comprises a silicon nitride layer and a silicon oxide layer.

### Claim 20 (depends on 15)

The method of claim 15, wherein a thickness of said spacer layer is in the range of approximately 5-100 nm.

### Claim 21

A method of filling a trench in a substrate, said substrate comprising a layer of a semiconductive material and a layer of a dielectric material formed thereon, said method comprising:
forming sidewall spacers of a semiconductive material in said trench, the sidewall spacers covering non-oxidizable sidewall portions of said trench;
filling said trench with a dielectric material; and
exposing said substrate to an oxidizing ambient to at least partially oxidize said sidewall spacers.

### Claim 22 (depends on 21)

The method of claim 21, wherein forming said sidewall spacers in the trench comprises conformally depositing a second layer of a semiconductive material on said substrate.

### Claim 23 (depends on 22)

The method of claim 22, further comprising anisotropically etching said second layer of semiconductive material so as to remove said second semiconductive material from areas of said substrate outside said trench and from a bottom of said trench.

### Claim 24 (depends on 23)

The method of claim 23, wherein filling said trench with a dielectric material comprises depositing a second layer of a dielectric material on said substrate.

### Claim 25 (depends on 24)

The method of claim 24, further comprising forming an oxide layer inside said trench prior to conformally depositing said second layer of a semiconductive material.

### Claim 26 (depends on 25)

The method of claim 25, wherein oxidizing said spacers comprises subjecting said substrate to a thermal oxidation process at a temperature in the range of approximately 600-1100° C.

### Claim 27 (depends on 22)

The method of claim 22, wherein said second layer of a semiconductive material is deposited by one of a sub-atmospheric chemical vapor deposition process and a high density plasma-enhanced chemical vapor deposition process.

### Claim 28 (depends on 24)

The method of claim 24, wherein said second layer of a dielectric material is deposited by one of a sub-atmospheric chemical vapor deposition process and a high density plasma-enhanced chemical vapor deposition process.

### Claim 29 (depends on 23)

The method of claim 23, wherein said layer of semiconductive material and said second layer of semiconductive material comprise silicon.

### Claim 30 (depends on 24)

The method of claim 24, wherein said layer of dielectric material and said second layer of dielectric material comprise silicon dioxide.

### Claim 31

A method of forming an isolation structure in a substrate comprising a semiconductive layer and a dielectric layer stack formed on said semiconductive layer, the method comprising:
forming a trench in said substrate, said trench extending in a depth dimension through said dielectric layer stack;
conformally depositing a spacer layer on said substrate, said spacer layer being comprised of an oxidizable material;
depositing a dielectric material for filling said trench; and
exposing said substrate to an oxidizing ambient to at least partially oxidize said spacer layer to fill any void that may have formed during the deposition of said dielectric material.

### Claim 32 (depends on 31)

The method of claim 31, further comprising anisotropically etching said spacer layer prior to depositing said dielectric material to form sidewall spacers on sidewalls of said trench.

### Claim 33 (depends on 32)

The method of claim 32, further comprising forming an etch stop layer prior to depositing said spacer layer.

### Claim 34 (depends on 31)

The method of claim 31, wherein one lateral dimension of said trench is 0.25 μm or less.

### Claim 35 (depends on 31)

The method of claim 31, wherein said dielectric material is a semiconductor oxide.

### Claim 36 (depends on 31)

The method of claim 31, wherein said spacer layer comprises one of silicon and germanium.

### Claim 37 (depends on 31)

The method of claim 31, wherein a thickness of said spacer layer is in the range of approximately 5-100 nm.

### Claim 38

A method of forming shallow trench isolation structures in a substrate of a semiconductive material during a manufacturing process for manufacturing integrated circuits, said method comprising:
forming a first layer of dielectric material on said substrate of semiconductive material;
selectively etching said first layer of dielectric material and said substrate of semiconductor material so as to form trenches deeper than the thickness of said layer of dielectric material, said trenches having sidewalls;
forming sidewall spacers comprised of a semiconductive material in said trenches, said spacers covering the inside sidewalls of said trenches;
filling said trenches with a dielectric material; and
oxidizing said sidewall spacers along the entire depth of said trench sidewalls.

### Claim 39 (depends on 38)

The method of claim 38, wherein forming said sidewall spacers in said trenches comprises conformally depositing a second layer of a semiconductive material on said first layer of dielectric material to a thickness allowing complete sidewall coverage inside said trenches.

### Claim 40 (depends on 39)

The method of claim 39, further comprising anisotropically etching said second layer of a semiconductive material so as to remove said semiconductive material from the areas of said first layer of dielectric material outside said trenches and from the bottom of said trenches.

### Claim 41 (depends on 40)

The method of claim 40, wherein filling said trenches with a dielectric material comprises depositing a third layer of a dielectric material on said first layer of dielectric material.

### Claim 42 (depends on 38)

The method of claim 38, further comprising thermal growing of a liner layer of dielectric material inside said trenches prior to conformally depositing said second layer of a semiconductive material.

### Claim 43 (depends on 38)

The method of claim 38, wherein oxidizing said spacers is performed at a temperature in the range of about 600-1100° C.

### Claim 44 (depends on 38)

The method of claim 38, wherein said second layer of a semiconductive material is deposited by a sub-atmospheric chemical vapor deposition process.

### Claim 45 (depends on 44)

The method of claim 44, wherein said third layer of a dielectric material is deposited according to one of a sub-atmospheric chemical vapor deposition process and a high density plasma-enhanced chemical vapor deposition process.

### Claim 46 (depends on 39)

The method of claim 39, wherein said semiconductive material of said substrate and said second layer comprises silicon.

### Claim 47 (depends on 39)

The method of claim 39, wherein said dielectric material of said third layer comprises silicon dioxide.